摘要:
The present invention is a multimodal polyethylene composition having (1) a density of at least about 0.940 g/cm3; (2) a melt flow index (I5) of from about 0.2 to about 1.5 g/10 mm; (3) a melt flow index ratio (I21/I5) of from about 20 to about 50; (4) a molecular weight distribution, Mw/Mn, of from about 20 to about 40; and (5) a bubble stability measured on an HS50S stationary extrusion system with an BF 10-25 die, HK 300 air ring, A8 take off, and WS8 surface winder, with a 100 mm die diameter having a 50 mm 21:1 L/D grooved feed extruder used for a film of about 6×10−6 m thickness of at least about 1.22 m/s line speed, at least about 45 kg/hr (0.013 kg/sec) output rate, or at least about 0.5 lb/hr/rpm (0.0000011 kg/s/rps) specific output rate or a combination thereof.
摘要:
The invention is related to compositions suitable for the fabrication of pipes, and other articles, with excellent performance properties. The invention provides a composition, comprising a blend, wherein said blend comprises a high molecular weight ethylene-based interpolymer and a low molecular weight ethylene-based interpolymer, and the high molecular weight ethylene-based interpolymer is a heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.922 g/cc to 0.929 g/cc, and a high load melt index (I21) from 0.2 g/10 min to 1.0 g/10 min, and the low molecular weight ethylene-based interpolymer is heterogeneously branched linear or a homogeneously branched linear ethylene-based interpolymer, and has a density from 0.940 g/cc to 0.955 g/cc, and a melt index (I2) from 6 g/10 min to 50 g/10 min. The blend has a single peak in an ATREF profile eluting above 30° C., and has a coefficient of viscosity average molecular weight (CM?) less than −0.0032 in the log(calculated Mv) versus elution temperature, said CMv calculated in the range of elution temperatures from 70° C. to 90° C. The Mv is the viscosity average molecular weight.
摘要:
This invention relates to coupling of polyethylene resins, more specifically coupling of polyethylene resins for use in extruded profiles, especially extruded profiles for sheet extrusion and cut sheet thermoforming applications and geomembranes. The process involves conveying a HDPE resin through an extruder, wherein the extruder comprises a feed zone, a first melt zone downstream of the feed zone, a second melt zone downstream of the first melt zone, and a third melt zone downstream of the second melt zone. The resin is melted in the first zone, contacted with oxygen in the second melt zone, and contacted antioxidant in the third melt zone.
摘要:
A polymer composition comprises a low-molecular-weight (LMW) ethylene polymer component and a high-molecular-weight (HMW) ethylene polymer component coupled with a polysulfonyl azide. Preferably, the LMW polyethylene component and the HMW polyethylene component co-crystallize in the composition such that it exhibits a single or substantially single peak in a lamella thickness distribution (LTD) curve. The ethylene polymer for the LMW and the HMW polyethylene components can be either homopolymer or ethylene copolymer. Preferably, both components are an ethylene copolymer of the same, or different, composition (that is, with the same or different comonomers). A method of making a pipe that includes selecting a polymer composition having a substantially single peak in the LTD curve is described. Compositions comprising a chromium-catalyzed ethylene polymer, coupled with a polysulfonyl azide are also described herein.
摘要:
A polyethylene composition comprising a granular polyethylene resin characterized by a resin solid density of from 0.91 to 0.97 g/cm3, a ratio of intraparticle void volume to interparticle void volume of from 0.33 to 0.67, and a total resin porosity, Φtotal, of equal to or greater than 0.45 is provided. Further provided are articles made from the polyethylene composition.
摘要:
The invention relates to formulated compositions which can be easily formed into bottle caps, without the need for a liner, while still maintaining pressure requirements, such as for carbonated beverages. The compositions may include an ethylene polymer having a density in the range of from about 0.947 to 0.962 g/cm3, a melt index of from about 1 to about 10 g/10 min., and another ethylene polymer having a density in the range of from about 0.912 to 0.932 g/cm3, a melt index of from about 0.25 to about 6 g/10 min., wherein the two ethylene polymers have a density difference of equal to or greater than 0.03 g/cm3. In other cases, the composition may include a single component resin with a density in the 0.935-0.955 g/cm3 range with a melt index in the range of 0.3-1.2 g/10 minutes, and wherein the resin comprises a polyethylene polymer.
摘要翻译:本发明涉及配制的组合物,其可以容易地形成瓶盖,而不需要衬垫,同时仍然保持压力要求,例如用于碳酸饮料。 组合物可以包括密度在约0.947至0.962g / cm 3范围内的乙烯聚合物,熔体指数为约1至约10g / 10分钟,而另一种乙烯聚合物的密度范围为 约0.912至0.932g / cm 3,熔体指数为约0.25至约6g / 10min,其中两种乙烯聚合物具有等于或大于0.03g / cm 3的密度差。 在其它情况下,组合物可以包括密度在0.935-0.955g / cm 3范围内的单组分树脂,熔体指数在0.3-1.2g / 10分钟的范围内,并且其中树脂包含聚乙烯聚合物。
摘要:
A polymer composition comprises a low-molecular-weight (LMW) ethylene polymer component and a high-molecular-weight (HMW) ethylene polymer component. Preferably, the LMW polyethylene component and the HMW polyethylene component co-crystallize in the composition such that it exhibits a single or substantially single peak in a lamella thickness distribution (“LTD”) curve. The ethylene polymer for the LMW and the HMW polyethylene components can be either homopolyethylene or ethylene copolymer. Preferably, both components are an ethylene copolymer of the same or different composition (i.e., with the same or different comonomers). A method of making a pipe that includes selecting a polymer composition having a substantially single peak in the LTD curve is described.
摘要:
The instant invention discloses fibers. The fibers according to the instant invention comprise a polyethylene composition comprising: (a) less than or equal to 100 percent by weight of the units derived from ethylene; and (b) less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein the polyethylene composition has a density in the range of 0.920 to 0.970 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 0.2 to 1000 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of the composition.
摘要:
The instant invention is a high-density polyethylene composition, method of producing the same, closure devices made therefrom, and method of making such closure devices. The high-density polyethylene composition according to the present invention comprises (a) a first component comprising a high molecular weight ethylene alpha-olefin copolymer having a density in the range of 0.927 to 0.938 g/cm3, and a melt flow rate (I21) in the range of 4 to 10 g/10 minutes, and (b) a second component comprising a low molecular weight ethylene polymer having a density in the range of 0.960 to 0.975 g/cm3, and a melt index (I2) in the range of 100 to 1200 g/10 minutes; and wherein the high-density polyethylene composition has a melt index (I2) in the range of from 2 to 10 g/10 minutes, a density in the range of from 0.950 to 0.960 g/cm3, and a flow direction shrinkage to cross flow direction shrinkage ratio in the range of from 2 to 3.2, and an environmental stress crack resistance (ESCR) (F50) according to ASTM D-1693, condition B at 50° C., and using 10 percent Branched Octylphenoxy Poly(Ethyleneoxy) Ethanol, in the range of equal to or greater than 50 hours.
摘要翻译:本发明是高密度聚乙烯组合物,其制造方法,由其制成的封闭装置,以及制造这种闭合装置的方法。 根据本发明的高密度聚乙烯组合物包含(a)包含密度在0.927至0.938g / cm 3范围内的高分子量乙烯α-烯烃共聚物和熔体流动速率(I21)的第一组分, 在4至10g / 10分钟的范围内,和(b)包含密度在0.960至0.975g / cm 3范围内的低分子量乙烯聚合物的第二组分和在该范围内的熔体指数(I 2) 为100〜1200g / 10分钟; 并且其中所述高密度聚乙烯组合物具有在2至10g / 10分钟范围内的熔体指数(I 2),在0.950至0.960g / cm 3范围内的密度和横向流动方向收缩 方向收缩率在2至3.2范围内,以及根据ASTM D-1693,条件B在50℃下的环境应力开裂抗力(ESCR)(F50),并使用10%支链辛基苯氧基聚(乙烯氧基)乙醇 在等于或大于50小时的范围内。
摘要:
The invention provides an ethylene-based interpolymer comprising the following features: a) density from 0.910 to 0.930 g/cc; b) melt index (I2) from 0.1 to 0.5 g/10 min; and c) a high density fraction in an ATREF short chain branch distribution (SCBD) curve, eluting above 92° C., of greater than 10 percent to less than 28 percent of the total ATREF SCBD curve area. The invention also provides a composition comprising an ethylene-based interpolymer that comprises the following features: a) a density from 0.919 to 0.928 g/cc; b) a melt index (I2) from 0.1 to 0.8 g/10 min; and c) a high density fraction in an ATREF short chain branch distribution (SCBD) curve, eluting above 92° C., of greater than 10 percent to less than 28 percent of the total ATREF SCBD curve area. The invention also provides a hollow tube comprising at least one component formed from a composition comprising an ethylene-based interpolymer that comprises the following features: a) a density from 0.919 to 0.928 g/cc; b) a melt index (I2) from 0.1 to 0.8 g/10 min; and c) a high density fraction in an ATREF short chain branch distribution (SCBD) curve, eluting above 92° C., of greater than 10 percent to less than 28 percent of the total ATREF SCBD curve area; and wherein the tube has a hydrostatic design basis (HDB) of at least 1000-psi at 23° C. per ASTM D-2837 regression method.