Fluorescent lamp.luminaire and method for manufacturing fluorescent lamp
    8.
    发明申请
    Fluorescent lamp.luminaire and method for manufacturing fluorescent lamp 有权
    荧光灯及荧光灯制造方法

    公开(公告)号:US20070188073A1

    公开(公告)日:2007-08-16

    申请号:US10597658

    申请日:2005-06-22

    IPC分类号: H01J1/62

    摘要: A fluorescent lamp is configured so that a glass bulb has a phosphor film formed on its internal face, and a rare gas and an amalgam pellet are enclosed therein. The amalgam pellet contains zinc, tin, and mercury as principal components, one amalgam pellet is enclosed in the glass bulb, and the amalgam pellet has a weight of not more than 20 mg. The fluorescent lamp satisfies the relationship expressed as: 45×(1−A)≦x≦55x(1−A), 75A≦y≦85A, 45−30A≦z≦55−30A, and x+y+z≦100, where x represents a content of zinc contained in the amalgam pellet in percent by weight, y represents a content of tin therein in percent by weight, and z represents a content of mercury therein in percent by weight. This configuration allows the fluorescent lamp to be characterized in that an amount of released mercury that is necessary for the first lighting of the fluorescent lamp is secured, and that the phosphor film is less prone to being peeled due to the amalgam.

    摘要翻译: 荧光灯被配置为使得玻璃灯泡在其内表面上形成有荧光膜,并且在其中封入稀有气体和汞齐颗粒。 汞齐颗粒含有锌,锡和汞作为主要成分,一个汞齐颗粒被封闭在玻璃泡中,汞齐颗粒的重量不超过20毫克。 荧光灯满足表示为:45x(1-A)<= x <= 55x(1-A),75A <= y <= 85A,45-30A <= z <= 55-30A,x + y + z <= 100,其中x表示汞齐颗粒中含有的锌含量,重量百分比,y表示锡的含量,重量百分比,z表示其中的汞含量。 这种结构允许荧光灯的特征在于,确保荧光灯的第一次点亮所需的释放汞量,并且荧光膜不太可能由于汞齐而被剥离。