摘要:
Light-weight, fire-resistant “mineral foam” includes an inorganic cementitious matrix and at least one metal hydrate that is a “super hydrate” substance, in which water is present with the substance in an amount of at least about ten moieties of water of hydration per formula unit of the substance. As a cured solid, that “mineral foam,” or another mineral foam composition including an inorganic cementitious matrix, can be provided as a structural member in part of an assembly that has at least one open web, thermally insulating support member at least partially embedded in the cured solid. Also, the cured “mineral foam” may be a solid foam in a form of a panel, panel block or tile, which may have a tongue provision and/or a groove provision.
摘要:
A cementitious composition may include polyvinyl alcohol, high alumina cement, water, a metallic coagent, a peroxide crosslinking initiator, and an organic acid retardant. A molded article may be manufactured from the cementitious composition by preparing a hydrogel pre-polymer blend of saponified polyvinyl alcohol acetate (PVAA) with greater than or equal to approximately 85% saponified PVAA, and water, mixing the hydrogel pre-polymer blend with high alumina cement (HAC) using a high shear mixing process, mixing in a metallic coagent and a peroxide crosslinking initiator, mixing in an organic acid retardant, and hot press molding the mixture.
摘要:
A description is given of a two-component mortar composition having a curable resin component having a content of at least one free-radically polymerizable resin, fillers, accelerators, stabilizers and optionally further conventional mortar constituents and a hardener component which is arranged separately therefrom to inhibit reaction and has a content of at least one peroxide for chemical fastening of anchoring means in boreholes, which is characterized in that the resin component contains from 0.1 to 0.5% by weight of at least one accelerator and from 0.003 to 0.03% by weight of at least one stabilizer and the hardener component contains from 0.1 to 0.35% by weight of organic peroxide, in each case based on the total weight of resin component and hardener component, and also the use of this two-component mortar composition for chemical fastening of anchoring means in boreholes.
摘要:
The present invention relates to methods and compositions useful for isolating a portion of a wellbore. In one embodiment, a method includes preparing a sealant composition containing two phases. The sealant composition is placed into the wellbore where one phase sets upon subjecting the sealant composition to a thermal source followed by the setting of the other phase.
摘要:
A cementitious composition may include polyvinyl alcohol, high alumina cement, water, a metallic coagent, a peroxide crosslinking initiator, and an organic acid retardant. A molded article may be manufactured from the cementitious composition by preparing a hydrogel pre-polymer blend of saponified polyvinyl alcohol acetate (PVAA) with greater than or equal to approximately 85% saponified PVAA, and water, mixing the hydrogel pre-polymer blend with high alumina cement (HAC) using a high shear mixing process, mixing in a metallic coagent and a peroxide crosslinking initiator, mixing in an organic acid retardant, and hot press molding the mixture.
摘要:
Building materials include a dampening layer which contains a plaster and a viscoelastic polymer, such as polyvinyl butyral. The dampening layer may also include a barium salt. Methods of making a sound dampening material include providing a plaster mixture. The mixture may include a viscoelastic polymer and/or a barium salt. The plaster mixture is combined with water and/or a viscoelastic polymer dispersion, to form a slurry. The slurry is applied to a surface and set to form a sound dampening layer.
摘要:
Method of reducing the odour of sulphur-bound products, in particular modified sulphur or sulphur concrete, comprising contacting the sulphur-bound products with a bleaching agent, like e.g. sodium hydrochloride or hydrogen peroxide. The resulting sulphur-bound products emit reduced levels of sulphur-containing gases such as H2S and SO2 and have a reduced odour.
摘要:
A grouting system for anchoring a reinforcement in a mine includes a package that is a tubular member formed of polymer film and has discrete first and second compartments. Hardenable cementitious material that is a hydratable substance and water is disposed in the first compartment. A method of forming a resin grouting capsule includes: injecting a hardenable material into a first compartment of the capsule having resin mastic; wherein the hardenable material does not substantially react with the resin mastic when injected into the first compartment. Another method of forming a resin grouting capsule includes: injecting a hardenable material into a first compartment of the capsule having catalyst mastic; wherein the hardenable material does not substantially react with the catalyst mastic when injected into the first compartment.
摘要:
A process for making a pervious concrete comprising a geopolymerized pozzolanic ash. Generally, the process includes mixing a solid aggregate and a geopolymerized pozzolanic ash binder together to form a pervious concrete mixture. Some examples of suitable aggregates comprise recycled carpet, recycled cement, and aggregates of coal-combustion byproducts. The geopolymerized pozzolanic ash binder is made by combining a pozzolanic ash, such as fly ash, with a sufficient amount of an alkaline activator and water to initiate a geopolymerization reaction. The activator solution may contain an alkali metal hydroxide, carbonate, silicate, aluminate, or mixtures thereof. In some aspects, the final concrete forms a solid mass in the form of pavement or a pre-cast concrete shape. The solid mass of concrete may have a void content of between about 5% and about 35%.
摘要:
A resin mortar composition suitable for construction purposes is disclosed. The composition includes a resin component (A) curable with an aliphatic amine and a peroxide and a hardener component (H) with at least one peroxide (B) and at least one amine (C). At least one of the resin component (A) and the hardener component (H) contains at least one inorganic filler and the resin component (A) and the hardener component (H) or the resin composition (A) and the at least one peroxide (B) and the at least one amine (C) of the hardener component (H) are spatially separated from one another. The resin component (A) includes a compound (a) capable of undergoing a radical polymerization, a compound (b) capable of reacting with an amine, a transition metal compound (c), at least one inhibitor (d) to adjust the gel time and a bridging compound (e) having at least two reactive functionalities.