Abstract:
Thermoplastic molding compositions essentially comprise (A) from 20 to 99% by weight of at least one graft copolymer, (B) from 1 to 80% by weight of a copolymer obtainable from at least one alpha-olefin and from at least one polar comonomer, with the proviso that the monomers used are not vinyl acetate or any vinylaromatic monomer, and (C) from 0 to 80% by weight of a thermoplastic polymer, obtainable by polymerizing a monomer mixture, essentially consisting of (c1) from 50 to 100% by weight of at least one vinylaromatic monomer and/or of a C1-C8-alkyl (meth)acrylate, and (c2) from 0 to 50% by weight of at least one monofunctional comonomer, and (D) from 0.1 to 15% by weight of a three-block polymer made from (d1) from 5 to 90% by weight of polyethylene oxide and (d2) from 95 to 10% by weight of polypropylene oxide nulland having a central polypropylene oxide block with a molar mass of from 800 to 5 000 g/mol and terminal blocks made from polyethylene oxide, nullwhere components A to D give 100% by weight in total. A process for preparing the thermoplastic molding compositions is also described, as is their use.
Abstract:
The present invention provides block copolymers containing at least one block of a poly(heteroaromatic)polymer and at least two blocks of a non-conjugated polymer. The chemically different blocks of the copolymer are covalently bonded to each other in an alternating fashion through an appropriate linkage group. The poly(heteroaromatic) block may exist in its neutral or oxidized form, and when in the oxidized form, it associates with organic or inorganic counter-anions to balance the charge. The poly(heteroaromatic)polymer is an intrinsically conducting polymer (ICP), and when in the oxidized form it is electrically conducting. When the ICP block or blocks of the block copolymer are in the doped form, the block copolymer is electrically conducting. Preferably the conducting block copolymers have conductivities in the range 10null6-103 S/cm. Block copolymers of this invention are soluble or dispersible in water, one or more organic solvents, or in a mixture thereof at a level of at least about 0.1 g/liter.
Abstract:
The present invention provides a novel amino-group-containing polymer (salt) and a production process therefor wherein the amino-group-containing polymer (salt) is a product by a process including the step of introducing amino groups into a grafted polymer having a polyether skeleton, and can make good use of the reactivity or cationic property of at least primary amino groups and further, according to circumstances, secondary amino groups, and further can display various performances, such as curability useful for various uses and adsorbency onto films or fibers. The novel amino-group-containing polymer (salt) is a product by a process including the steps of: carrying out a graft polymerization of a monoethylenically unsaturated monomer component onto a polyether compound, wherein the monoethylenically unsaturated monomer component includes an unsaturated carboxylic monomer as an essential component, and wherein the polyether compound has a specific repeating unit in a ratio of not less than 30 mol % and has a number-average molecular weight of not less than 150; and introducing amino groups by carrying out a ring-opening addition of an alkylenimine to at least a part of carboxyl group portions of the monoethylenically unsaturated monomer component which has been graft-polymerized onto the polyether compound, wherein at least a part of the amino groups might be neutralized with an acid.
Abstract:
The invention relates to polyamide compositions having improved antistatic behaviour and/or improved hydrophilicity. These compositions are particularly suitable for the manufacture of polyamide-based yarns, fibres and filaments. The compositions comprise polyamide and a modifier containing polyether units, which modifies the antistatic and/or hydrophilic properties.
Abstract:
The present invention relates to polyethyleneglycol/polylactide (or polyglycolide or polycaprolactone)/polyethyleneglycol triblock copolymers with an enhanced reactivity, and process for their preparation. More specifically, the present invention is directed to triblock copolymers that are obtained by the process comprising the step of synthesizing a polylactide (or polyglycolide or polycaprolactone) having hydroxy groups at both ends and the step of coupling said polylactide with polyethyleneglycol having an acylhalide group of a high reactivity at one of its ends, and the process for preparing the same. Since the triblock copolymer according to the present invention has an ester structure with good biocompatibility, it can be applied extensively for biomaterials used in tissue engineering, in a matrix that slowly releases drugs, etc.
Abstract:
The present invention provides rubber mixtures with improved processing behavior containing special polyethers and use of the rubber mixtures for preparing vulcanizates, in particular for the production of highly reinforced, abrasion-resistant molded items, particularly preferably for producing tires which have a low rolling resistance and a high abrasion resistance.
Abstract:
A syndiotactic polystyrene copolymer resin composition with high impact strength, which comprises: (A) about 1-99 weight % of a syndiotactic polystyrene copolymer which is polymerized from at least one macromonomer having an active polymerization group at its end and at least one styrene monomer; and (B) about 99-1 weight % of at least one rubber phase resin and/or at least one thermoplastic resin.
Abstract:
The present invention relates to a thermoplastic resin composition comprising a thermoplastic resin and hollow carbon fibrils dispersed in the thermoplastic resin, the hollow carbon fibrils being present in an amount of 0.1 to 20% by weight based on the total weight of the composition, comprising independent fibrils and agglomerated fibrils, and having such a dispersing condition, when represented by indices based on the measurement of transmission electron microphotograph, that the ratio of the independent fibrils to the agglomerated fibrils lies within the range of 8/92 to 40/60 and the independent fibrils have an average length of 20 to 200 nm.
Abstract:
A thermoplastic molding composition comprising a transparent resinous component suitable for tinting by dip-dye method is disclosed. The resinous component is selected from the group consisting of (i) a blend of (co)polycarbonate resin and (co)polycaprolacone, and (ii) a copolymer containing carbonate and caprolactone structural units. The composition, characterized in that it is free of photochromic colorants, may be molded by thermoplastic means, and the molded article is then dipped-dyed by immersion in a tinting solution. The tinted articles are suitable for making, among others, optical lenses.
Abstract:
Molecular weight-enlarged, homogeneously soluble ligands are provided that are especially useful for hydrogenation catalysts, wherein the ligands contain homochiral active centers of bis(3,4-diarylphosphinyl)pyrrolidines, and their use in producing cataylsts for enantioselective reactions, as well as the catalysts thus produced.