摘要:
Provided is a wavelength conversion member that is less decreased in luminescence intensity with time by irradiation with light of an LED or LD and a light emitting device using the wavelength conversion member. A wavelength conversion member is formed of an inorganic phosphor dispersed in a glass matrix, wherein the glass matrix contains, in % by mole, 30 to 85% SiO2, 0 to 20% B2O3, 0 to 25% Al2O3, 0 to 3% Li2O, 0 to 3% Na2O, 0 to 3% K2O, 0 to 3% Li2O+Na2O+K2O, 0 to 35% MgO, 0 to 35% CaO, 0 to 35% SrO, 0 to 35% BaO, 0.1 to 45% MgO+CaO+SrO+BaO, and 0 to 4% ZnO, and the inorganic phosphor is at least one selected from the group consisting of an oxide phosphor, a nitride phosphor, an oxynitride phosphor, a chloride phosphor, an oxychloride phosphor, a halide phosphor, an aluminate phosphor, and a halophosphate phosphor.
摘要:
The invention relates to InP-based nanoclusters that include indium and phosphorus and further include zinc, chlorine, or a combination thereof, and to a method of preparing the InP-based nanoparticles including heating the InP-based nanoclusters in the presence of zinc, chlorine, or a combination thereof.
摘要:
An electroluminescent lamp having a high color rendering index (CRI) can be made using a phosphor blend comprising a mixture of an electroluminescent phosphor and an europium-activated alkaline earth silicon nitride phosphor, wherein the electroluminescent phosphor is selected from a blue-emitting electroluminescent phosphor, a blue-green-emitting electroluminescent phosphor, or a combination thereof. Preferably, the lamp exhibits a CRI of at least about 75, and, more preferably, at least about 80. A preferred blend contains from about 10% to about 20% by weight of the europium-activated alkaline earth silicon nitride phosphor.
摘要:
An LED lamp includes a light source configured to emit radiation with a peak intensity at a wavelength between about 250 nm and about 550 nm; and a phosphor composition configured to be radiationally coupled to the light source. The phosphor composition includes particles of a phosphor of formula I, said particles having a coating composition disposed on surfaces thereof; ((Sr1−zMz)1−(x+w)AwCex)3(Al1−ySiy)O4+y+3(x−w)F1−y−3(x−w) I wherein the coating composition comprises a material selected from aluminum oxide, magnesium oxide, calcium oxide, barium oxide, strontium oxide, zinc oxide, aluminum hydroxide, magnesium hydroxide, calcium hydroxide, barium hydroxide, strontium hydroxide, zinc hydroxide, aluminum phosphate, magnesium phosphate, calcium phosphate, barium phosphate, strontium phosphate, and combinations thereof; and A is Li, Na, K, or Rb, or a combination thereof; M is Ca, Ba, Mg, Zn, or a combination thereof; and 0
摘要:
A sputtering target for fluorescent thin-film formation comprising a matrix material and a luminescent center material,wherein said matrix material has a chemical composition represented by the following formula (1), and simultaneously satisfies conditions represented by the following inequalities (2) to (5). MIIvAxByOzSw (1) 0.05≦v/x≦5 (2) 1≦y/x≦6 (3) 0.01≦z/(z+w)≦0.85 (4) 0.6≦(v+x+3y/2)/(z+w)≦1.5 (5) wherein MII represents one or more elements selected from the group consisting of Zn, Cd and Hg, A represents one or more elements selected from the group consisting of Mg, Ca, Sr, Ba and rare earth elements, B represents one or more elements selected from the group consisting of Al, Ga and In, and v, x, y, z and w each represent numerical values satisfying the conditions specified in the inequalities (2) to (5).
摘要:
In the manufacture of an alkaline earth halophosphate phosphor, a tray is filled from an automatic loader with a predetermined weight of powder comprising a blend of raw ingredients for forming said phosphor. The filled tray is then vibrated with a pattern inserted therein to settle the powder into a powder mass having a shape that promotes uniformity of reaction when the powder is fired at a temperature that causes the raw ingredients to react and form said phosphor.
摘要:
A nanocrystal particle including at least one semiconductor material and at least one halogen element, the nanocrystal particle including: a core comprising a first semiconductor nanocrystal; and a shell surrounding the core and comprising a crystalline or amorphous material, wherein the halogen element is present as being doped therein or as a metal halide