摘要:
Biodegradable compositions containing an aliphatic-aromatic copolyester derived from aromatic polyesters. Methods of making the compositions and articles made from the compositions.
摘要:
Biodegradable compositions containing an aliphatic-aromatic copolyester derived from aromatic polyesters. Methods of making the compositions and articles made from the compositions.
摘要:
The invention relates to a process for making modified polybutylene terephthalate random copolymers from a polyethylene terephthalate component. In one embodiment, the invention relates to a two step process in which a 1,4-butane diol component reacts with a polyethylene terephthalate component under conditions that depolymerize the polyethylene terephthalate component into a molten mixture and the molten mixture is placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. In another embodiment, the invention relates to a three step process in which a diol component selected from the group consisting of ethylene glycol, propylene glycol, and combinations thereof reacts with a polyethylene terephthalate component under conditions sufficient to depolymerize the polyethylene terephthalate component into a first molten mixture; and where the first molten mixture is combined with 1,4-butane diol under conditions that create a second molten mixture that is subsequently placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. The invention also relates to compositions made from processes of the invention.
摘要:
In one embodiment, the invention relates to a two step process in which a 1,4-butane diol component reacts with a polyethylene terephthalate component under conditions that depolymerize the polyethylene terephthalate component into a molten mixture and the molten mixture is placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. In another embodiment, the invention relates to a three step process in which a diol component selected from the group consisting of ethylene glycol, propylene glycol, and combinations thereof reacts with a polyethylene terephthalate component under conditions sufficient to depolymerize the polyethylene terephthalate component into a first molten mixture; and where the first molten mixture is combined with 1,4-butane diol under conditions that create a second molten mixture that is subsequently placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. The invention also relates to compositions made from processes of the invention.
摘要:
In one embodiment, the invention relates to a two step process in which a 1,4-butane diol component reacts with a polyethylene terephthalate component under conditions that depolymerize the polyethylene terephthalate component into a molten mixture and the molten mixture is placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. In another embodiment, the invention relates to a three step process in which a diol component selected from the group consisting of ethylene glycol, propylene glycol, and combinations thereof reacts with a polyethylene terephthalate component under conditions sufficient to depolymerize the polyethylene terephthalate component into a first molten mixture; and where the first molten mixture is combined with 1,4-butane diol under conditions that create a second molten mixture that is subsequently placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. The invention also relates to compositions made from processes of the invention.
摘要:
The invention relates to a process for making modified polybutylene terephththalate random copolymers from a polyethylene terephthalate component. The invention relates to a three step process in which a diol component selected from the group consisting of ethylene glycol, propylene glycol, and combinations thereof reacts with a polyethylene terephthalate component under conditions sufficient to depolymerize the polyethylene terephthalate component into a first molten mixture; and where the first molten mixture is combined with 1,4-butanediol under conditions that create a second molten mixture that is subsequently placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. The invention also relates to compositions made from the process.
摘要:
The invention relates to a process for making modified polybutylene terephthalate random copolymers from a polyethylene terephthalate component. The invention relates to a three step process in which a diol component selected from the group consisting of ethylene glycol, propylene glycol, and combinations thereof reacts with a polyethylene terephthalate component under conditions sufficient to depolymerize the polyethylene terephthalate component into a first molten mixture; and where the first molten mixture is combined with 1,4-butanediol under conditions that create a second molten mixture that is subsequently placed under subatmospheric conditions that produce the modified polybutylene terephthalate random copolymers. The invention also relates to compositions made from the process.
摘要:
A thermoplastic composition comprises, based on the total weight of the composition: 51-90 wt % of a polyester, 10-49 wt % of an ABS impact modifier; 0 to 20 wt % of a multifunctional epoxy compound; 0-40 wt % of a filler; 0-2 wt % of a fibrillated fluoropolymer; and from more than 0 to 5 wt % of a stabilizer composition. An article blow molded or injection molded from the composition has a multi-axial impact total energy from 40-100 Joules at −30° C.; a ductility of more than 90%, a permeability of more than 0 to less than or equal to 1.5 g/m2-day, measured after exposure Fuel C vapor for 20 weeks at 40° C.; an MVR of 1-20 cc/10 min; a flexural modulus of greater than 1300 MPa; and retains at least 75% of its initial tensile elongation at break after exposure to Fuel E85 for 28 days at 70° C.
摘要:
A thermoplastic composition comprises, based on the total weight of the composition: 51-90 wt % polyester, 10-49 wt % ABS impact modifier; 0-20 wt % of multifunctional epoxy compound; 0-40 wt % filler; 0-2 wt % fibrillated fluoropolymer; and more than 0 to 5 wt % of a stabilizer composition. An article blow molded or injection molded from the composition has a multi-axial impact total energy from 30-100 Joules at −30° C. and a ductility of more than 90%; a permeability of more than 0 and less than or equal to 1.5 g/m2-day to ASTM D 471-98 Fuel C, measured after exposure to ASTM D 471-98 Fuel C vapor for 20 weeks at 40° C.; an MVR of 1-20 cc/10 min., measured at 265° C.; a flexural modulus of greater than 1300 MPa; and retains at least 75% of its initial tensile elongation at break, after exposure to Fuel E85 for 28 days at 70° C.
摘要翻译:基于组合物的总重量,热塑性组合物包含:5-1-90wt%聚酯,10-49wt%ABS抗冲改性剂; 0-20重量%多官能环氧化合物; 0-40重量%填料; 0-2重量%原纤化含氟聚合物; 和大于0至5重量%的稳定剂组合物。 由该组合物吹塑或注射成型的制品在-30℃下具有30-100焦耳的多轴冲击总能量和大于90%的延展性; 根据ASTM D 471-98燃料C,在40℃下暴露于ASTM D 471-98燃料C蒸气20周后测量的渗透率大于0且小于或等于1.5g / m 2·天。 在265℃下测量的,为1-20cc / 10分钟的MVR。 弯曲模量大于1300MPa; 并且在70℃下暴露于Fuel E85 28天后,保持其初始拉伸伸长率的至少75%
摘要:
Phase separated blends of polyaryl ether ketones, polyaryl ketones, polyether ketones, polyether ether ketones and mixtures thereof with at least one polysulfone etherimide, wherein the polysulfone etherimide has greater than or equal to 50 mole % of the polymer linkages contain at least one aryl sulfone group are described. Such blends have improved load bearing capability at high temperature. In another aspect a high crystallization temperature, especially at fast cooling rates, is achieved.