摘要:
Provided are resin-based and metal-based anti-thermally-expansive members each having small thermal expansion. More specifically, provided are an anti-thermally-expansive resin and an anti-thermally-expansive metal, each including a resin or a metal having a positive linear expansion coefficient at 20° C. and a solid particle dispersed in the resin or metal, in which the solid particle includes at least an oxide represented by the following general formula (1): (Bi1-xMx)NiO3 (1), where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.
摘要翻译:提供了具有小的热膨胀的树脂基和金属基的抗热膨胀性构件。 更具体地说,提供了一种抗热膨胀树脂和抗热膨胀性金属,其各自包括在20℃具有正线性膨胀系数的树脂或金属和分散在树脂或金属中的固体颗粒, 其中固体颗粒至少包含由以下通式(1)表示的氧化物:(Bi1-xMx)NiO3(1),其中M表示选自La,Pr,Nd,Sm中的至少一种金属 ,Eu,Gd,Tb,Dy,Ho,Er,Tm,Yb,Lu,Y和In; x表示0.02 @ x @ 0.15的数值。
摘要:
Provided are resin-based and metal-based anti-thermally-expansive members each having small thermal expansion. More specifically, provided are an anti-thermally-expansive resin and an anti-thermally-expansive metal, each including a resin or a metal having a positive linear expansion coefficient at 20° C. and a solid particle dispersed in the resin or metal, in which the solid particle includes at least an oxide represented by the following general formula (1): (Bi1-xMx)NiO3 (1), where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.
摘要:
Provided are a thermal expansion suppressing member having negative thermal expansion properties and a metal-based anti-thermally-expansive member having small thermal expansion. More specifically, provided are a thermal expansion suppressing member, including at least an oxide represented by the following general formula (1), and an anti-thermally-expansive member, including a metal having a positive linear expansion coefficient at 20° C., and a solid body including at least an oxide represented by the following general formula (1), the metal and solid being joined to each other: (Bi1-xMx)NiO3 (1) where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.
摘要:
Provided are a thermal expansion suppressing member having negative thermal expansion properties and a metal-based anti-thermally-expansive member having small thermal expansion. More specifically, provided are a thermal expansion suppressing member, including at least an oxide represented by the following general formula (1), and an anti-thermally-expansive member, including a metal having a positive linear expansion coefficient at 20° C., and a solid body including at least an oxide represented by the following general formula (1), the metal and solid being joined to each other: (Bi1-xMx)NiO3 (1) where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.
摘要:
Provided is a Bi-based piezoelectric material having good piezoelectric properties. The piezoelectric material includes a perovskite-type metal oxide represented by the following general formula (1): Ax(ZnjTi(1-j))l(MgkTi(1-k))mMnO3 General formula (1) where: A represents a Bi element, or one or more kinds of elements selected from the group consisting of trivalent metal elements and containing at least a Bi element; M represents at least one kind of an element selected from the group consisting of Fe, Al, Sc, Mn, Y, Ga, and Yb; and 0.9≦x≦1.25, 0.4≦j≦0.6, 0.4≦k≦0.6, 0.09≦l≦0.49, 0.19≦m≦0.64, 0.13≦n≦0.48, and l+m+n=1 are satisfied.
摘要:
Provided is a Bi-based piezoelectric material having good piezoelectric properties. The piezoelectric material includes a perovskite-type metal oxide represented by the following general formula (1): Ax(ZnjTi(1-j))l(MgkTi(1-k))mMnO3 General formula (1) where: A represents a Bi element, or one or more kinds of elements selected from the group consisting of trivalent metal elements and containing at least a Bi element; M represents at least one kind of an element selected from the group consisting of Fe, Al, Sc, Mn, Y, Ga, and Yb; and 0.9≦x≦1.25, 0.4≦j≦0.6, 0.4≦k≦0.6, 0.09≦l≦0.49, 0.19≦m≦0.64, 0.13≦n≦0.48, and l+m+n=1 are satisfied.
摘要翻译:提供具有良好的压电性能的Bi基压电材料。 压电材料包括由以下通式(1)表示的钙钛矿型金属氧化物:Ax(ZnjTi(1-j))l(MgkTi(1-k))mMnO3通式(1)其中:A表示Bi元素 ,或选自三价金属元素并且至少含有Bi元素的一种或多种元素; M表示选自Fe,Al,Sc,Mn,Y,Ga和Yb中的至少一种元素; 和0.9 @ x @ 1.25,0.4 @ j @ 0.6,0.4 @ k @ 0.6,0.09 @ l @ 0.49,0.19 @ m @ 0.64,0.13 @ n @ 0.48和l + m + n = 1。
摘要:
Provided is a piezoelectric ceramics that can achieve both high piezoelectric performance and a high Curie temperature. Also provided are a piezoelectric element, a liquid discharge head, an ultrasonic motor, and a dust removing device, which use the piezoelectric ceramics. The piezoelectric ceramics include a perovskite-type metal oxide expressed by a general formula (1): xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3, where M represents at least one type of element selected from the group consisting of Mg and Ni, x satisfies 0.40≦x≦0.80, y satisfies 0≦y≦0.30, z satisfies 0.05≦z≦0.60, and x+y+z=1 is satisfied, and are oriented in a (111) plane in a pseudocubic expression.
摘要翻译:提供能够实现高压电性能和高居里温度的压电陶瓷。 还提供了使用压电陶瓷的压电元件,排液头,超声波马达和除尘装置。 压电陶瓷包括由通式(1)表示的钙钛矿型金属氧化物:xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3,其中M表示选自Mg和 Ni,x满足0.40≦̸ x≦̸ 0.80,y满足0≦̸ y≦̸ 0.30,z满足0.05≦̸ z≦̸ 0.60,并且x + y + z = 1,并且在(111) 假性表达。
摘要:
Provided is a piezoelectric material that achieves both high piezoelectric performance and high Curie temperature. In addition, provided are a piezoelectric element, a liquid discharge head, an ultrasonic motor, and a dust removing device, which use the piezoelectric material. The piezoelectric material includes a perovskite-type metal oxide that is expressed by the following general formula (1): xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3 (1), where M represents at least one type of element selected from the group consisting of Mg and Ni, x satisfies 0.25≦x≦0.75, y satisfies 0.15≦y≦0.70, z satisfies 0.05≦z≦0.60, and x+y+z=1 is satisfied.
摘要翻译:提供一种能够实现高压电性能和高居里温度的压电材料。 此外,提供了使用压电材料的压电元件,排液头,超声波马达和除尘装置。 压电材料包括由以下通式(1)表示的钙钛矿型金属氧化物:xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3(1),其中M表示至少一种选自 由Mg和Ni组成的组x满足0.25≦̸ x≦̸ 0.75,y满足0.15≦̸ y≦̸ 0.70,z满足0.05≦̸ z≦̸ 0.60,x + y + z = 1。
摘要:
Provided is a lead-free dielectric ceramics having a low leakage current value, and a bismuth iron oxide powder as a raw material thereof. The bismuth iron oxide powder includes at least: (A) grains including a bismuth iron oxide having a perovskite-type crystal structure; (B) grains including a bismuth iron oxide having a crystal structure classified to a space group Pbam; and (C) grains including a bismuth iron oxide or a bismuth oxide having a crystal structure that is classified to a space group I23. The dielectric ceramics are made of bismuth iron oxide in which the bismuth iron oxide crystals having the crystal structure classified to the space group Pbam are distributed at a grain boundary of crystal grains of the bismuth iron oxide crystals having the perovskite-type crystal structure.
摘要:
Provided is a piezoelectric material that achieves both high piezoelectric performance and high Curie temperature. In addition, provided are a piezoelectric element, a liquid discharge head, an ultrasonic motor, and a dust removing device, which use the piezoelectric material. The piezoelectric material includes a perovskite-type metal oxide that is expressed by the following general formula (1): xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3 (1), where M represents at least one type of element selected from the group consisting of Mg and Ni, x satisfies 0.25≦x≦0.75, y satisfies 0.15≦y≦0.70, z satisfies 0.05≦z≦0.60, and x+y+z=1 is satisfied.
摘要翻译:提供一种能够实现高压电性能和高居里温度的压电材料。 此外,提供了使用压电材料的压电元件,排液头,超声波马达和除尘装置。 压电材料包括由以下通式(1)表示的钙钛矿型金属氧化物:xBaTiO3-yBiFeO3-zBi(M0.5Ti0.5)O3(1),其中M表示至少一种选自 由Mg和Ni组成的组x满足0.25 @ x @ 0.75,y满足0.15 @ y @ 0.70,z满足0.05 @ z @ 0.60,x + y + z = 1。