LAMINATED STEEL SHEET FOR BOTH-SIDED RESIN-COATED CONTAINER

    公开(公告)号:US20200262183A1

    公开(公告)日:2020-08-20

    申请号:US15781605

    申请日:2016-10-21

    Abstract: A laminated steel sheet for a both-sided resin-coated container includes a steel sheet, a first polyester resin layer formed on a surface of the steel sheet serving as an inner side of a container after the container is formed, and a second polyester resin layer formed on a surface of the steel sheet serving as an outer side of the container after the container is formed. The first polyester resin layer includes a polyethylene terephthalate content of 95% by weight or more and has a degree of crystallinity in a range of 3% to 25%. The second polyester resin layer includes polyethylene terephthalate and polybutylene terephthalate and has a proportion of polybutylene terephthalate in a range of 40% by weight to 80% by weight.

    Steel sheet for three-piece can and method for manufacturing the same

    公开(公告)号:US10392682B2

    公开(公告)日:2019-08-27

    申请号:US14440779

    申请日:2013-11-06

    Abstract: Provided are a steel sheet for a can having high buckling strength for a can body against an external force and excellent formability when being formed into a shape having a design effect by additionally giving elongation strain in the circumferential direction after the steel sheet having been formed into a cylindrical shape and a method for manufacturing the steel sheet. The chemical composition is controlled to contain, by mass %, C: 0.0005% or more and 0.0035% or less, Si: 0.050% or less, Mn: more than 0.60% and 1.00% or less, P: 0.030% or less, S: 0.020% or less, Al: 0.010% or more and 0.100% or less, N: 0.0030% or less, B: 0.0005% or more, and the balance being Fe and inevitable impurities, in which the relationship B/N≥0.50 is satisfied where B/N represents (B(mass %)/10.81)/(N(mass %)/14.01), and a Young's modulus in a direction at an angle of 90° to the rolling direction is 220 GPa or more.

    Laminated metal sheet for container

    公开(公告)号:US10427381B2

    公开(公告)日:2019-10-01

    申请号:US15553027

    申请日:2016-03-31

    Abstract: A laminated metal sheet 1 includes a film 3 including a laminated resin layer including at least two layers with polyester as a main component formed on one face or both faces of a metal sheet 2. A polyester resin layer serving as a lower layer 3a in contact with the metal sheet 2 of the laminated resin layer contains 90 mol % or more of terephthalic acid as a polycarboxylic acid component and contains a polyol component containing ethylene glycol and 1,4-butanediol, in which the polyol component contains 30 to 50 mol % of ethylene glycol, 50 to 70 mol % of 1,4-butanediol, and 10 mol % or less of other polyol components. A polyester resin layer serving as an upper layer 3b of the laminated resin layer contains polyester containing terephthalic acid as a polycarboxylic acid component and 1,4-butanediol as a polyol component both of which are 90 mol % or more of the respective components, has a total thickness of 3 to 25 μm, and has a ratio (I011/I100) of peak intensity (I011) observed in the range of 2θ=15.5 degrees to 17.0 degrees to peak intensity (I100) observed in the range of 2θ=22.5 degrees to 24.0 degrees in X-ray diffraction in the range of 0.2 to 5.0.

    RESIN-COATED METAL SHEET FOR CONTAINERS AND METHOD FOR MANUFACTURING THE SAME
    18.
    发明申请
    RESIN-COATED METAL SHEET FOR CONTAINERS AND METHOD FOR MANUFACTURING THE SAME 有权
    用于容器的树脂涂层金属片及其制造方法

    公开(公告)号:US20170008256A1

    公开(公告)日:2017-01-12

    申请号:US15117877

    申请日:2015-02-17

    Abstract: Provided is a resin-coated metal sheet for containers having a resin layer (A) on a side of the metal sheet, the side being a side that will serve as a container inner surface when the metal sheet is formed into a container. The resin layer (A) has a polyester-based multilayer structure. The resin layer (A) contains 85 mol % or more of terephthalic acid. The resin layer (A) includes at least two layers, and an uppermost resin layer (a1), which is to be in contact with contends, contains 0.10 to 2.0 mass % of a wax compound with respect to the uppermost resin layer (a1). The maximum value of the Raman band intensity ratio (I1720/I1615) when measured for the cross section of the uppermost resin layer (a1) by using a laser polarization plane parallel to the surface of the resin layer (a1) is in the range of 0.45 or more and 0.80 or less. The uppermost resin layer (a1) has a thickness of 0.5 μm or more and 10 μm or less. The resin layer (A) excluding the uppermost resin layer (a1) has a thickness of 5 μm or more and 20 μm or less.

    Abstract translation: 本发明提供一种用于在金属板侧具有树脂层(A)的容器树脂涂覆金属片,该侧面是当金属片形成容器时将用作容器内表面的一侧。 树脂层(A)具有聚酯类多层结构。 树脂层(A)含有85摩尔%以上的对苯二甲酸。 树脂层(A)至少包含两层,与上述接触的最上层树脂层(a1)相对于最上层树脂层(a1)含有0.10〜2.0质量%的蜡化合物, 。 通过使用与树脂层(a1)的表面平行的激光偏振面测量最上层树脂层(a1)的截面时的拉曼带强度比(I1720 / I1615)的最大值在 0.45以上且0.80以下。 最上层的树脂层(a1)的厚度为0.5μm以上且10μm以下。 除了最上层树脂层(a1)以外的树脂层(A)的厚度为5μm以上且20μm以下。