摘要:
A polarizer comprising a polyvinyl alcohol based film being dyed by iodine and treated with potassium iodide, wherein an element content ratio (K/I) of iodine (I) and potassium (K) is 0.05 through 0.24, show an effect controlling coloring and satisfying high durability under conditions of high temperature.
摘要:
In a method of producing an optical film including: a rubbing treatment step of rubbing a surface of a long plastic film F by a rubbing roll 4 on which a raised fabric is wound; an applying step of applying liquid crystalline molecules on the surface of the film after the rubbing treatment step; and a fixing step of fixing the applied liquid crystalline molecules, in which in the rubbing treatment step, the film is conveyed while being supported by a conveyance belt 3 having a metal surface, and a backup roll mechanism 5 that supports a bottom face of the conveyance belt is provided. The backup roll mechanism has a plurality of backup rolls 51 each rotating along the conveyance direction of the conveyance belt, and each backup roll is disposed directly below the rubbing roll, along a straight line that is approximately parallel with a rotation axis of the rubbing roll.
摘要:
A method for producing a multilayer laminated film comprising: laminating a resin film having a moisture percentage of 10% by weight to 60% by weight with a first transparent film and a second transparent film each having a moisture percentage of 0.5% by weight to 5% by weight to be bonded to both sides of the resin film through an adhesive or pressure-sensitive adhesive layer interposed therebetween; wherein the laminating comprising steps of: passing the resin film and the first transparent film between a pair of a first metal roll and a first elastic roll in such a manner that the first transparent film is placed on the first metal roll side so that they are bonded to each other under pressure to form a laminated film; and then, using the laminated film without winding up it and passing the laminated film and the second transparent film between a pair of a second metal roll and a second elastic roll in such a manner that the second transparent film is placed on the second metal roll side so that they are bonded to each other under pressure to form a multilayer laminated film. The method can prevent bubbles from being formed between the resin film and the transparent film.
摘要:
An oriented film with a high degree of orientation may be manufactured even a width of master roll film is wider width, by a manufacturing method for an oriented film, comprising steps of stretching an un-oriented polyvinyl alcohol derived film in dry and in longitudinal uniaxial direction by applying tension produced by peripheral velocity difference between rolls, wherein a value of L/W is not more than 0.6 when a distance between rolls defined as L and a width of the un-oriented polyvinyl alcohol derived film is defined as W; and further heating at 60 to 160° C. after the stretching step.
摘要:
A method for manufacturing a coated sheet that may form a coated layer having a uniform film thickness by a coating liquid even when a substrate has a large area. A method for manufacturing a coated sheet to form a coated layer by a process including a process (1) for coating a coating liquid including a resin material and a solvent on a substrate, and a drying process (2) for drying a coated liquid, wherein a value L obtained in drying process (2) satisfies a following relationship; L = ∫ 0 T σ [ mN / m ] × ( h [ m ] ) 3 η [ mPa · sec ] ⅆ t > 1.9 × 10 - 13 [ m 4 / sec ] (where: T: total period of drying process [sec]; σ: surface tension of coated liquid [mN/m]; h: thickness of coated liquid [m]; and η: viscosity of coated liquid [mPa·sec]).
摘要:
The present invention pertains to a method of fabricating a polarizing film by uniaxially stretching a resin film such as a polyvinyl alcohol-based film in a fabrication process including a swelling step and a dyeing step following the swelling step, comprising the steps of immersing a resin film in bath liquids in at least two or more swelling baths in sequence in the above-mentioned swelling step, wherein at least a bath temperature of a swelling bath located at a Nth position from the front-stage side is set at a temperature which is higher than a bath temperature of a swelling bath located at a (N+M)th position by 3° C. or more (both N and M are specified positive integers).
摘要:
The present invention relates to a method of drying a coating film, and its object is to produce a coating film with small variations in thickness with stability. Thus, in the method of drying a coating film 11 formed by application of a coating solution to a long-length substrate 10 which is traveling, the coating film 11 is dried immediately after the application of a coating solution to the long-length substrate 10, with an evaporation rate of a solvent kept at 0.1 g/m2 s or less. Preferably, on a travel path of the coating film 11 immediately after coating, a plate 20 should be provided with a predetermined air gap between itself and the coating film 11 thereby to control the evaporation rate of the coating solution.
摘要翻译:本发明涉及一种干燥涂膜的方法,其目的是制备具有稳定性的厚度变化小的涂膜。 因此,在将涂布液涂布在长行进的长度基板10上形成的涂膜11的干燥方法中,在将涂布液涂布在长长基板10上之后立即干燥涂膜11 ,溶剂的蒸发速率保持在0.1g / m 2以下。 优选地,在涂布后的涂膜11的行进路径上,板20应在其与涂膜11之间设置预定的气隙,从而控制涂布溶液的蒸发速率。
摘要:
A birefringent film with excellent uniformity in in-plane retardation, retardation in the thickness direction, and alignment axis is provided. The birefringent film is produced in such a manner that, in the step of stretching a polymer film, the polymer film is stretched in a width direction while being shrunk in a longitudinal direction, and assuming that lengths in the width direction and the longitudinal direction of the polymer film before being stretched are 1, a change ratio (STD) of the length in the width direction of the polymer film resulting from the stretching and a change ratio (SMD) of the length in the longitudinal direction of the polymer film resulting from the shrinking satisfy the following formula (1). (1/STD)1/2≦SMD
摘要:
The method of cleaning a coated sheet according to the present invention is characterized in that dry wind is brown along the traveling direction of a film onto the surface of a coating layer wherein the solid content and the viscosity of the coating solution are within specified ranges. By this method, the thickness precision of the coating film can be improved in its large area, and the evenness of its in-plane optically functional property can be made even therein. The speed of the dry wind, the temperature of the wind, and the thickness of the dried coating film are preferably within specified ranges. In particular, the coated sheet is very useful as an optical material having good properties in an optically functional layer which is frequently used as a large-area coated sheet, an optical device having such an optically functional layer, an optically compensating layer, or an optically compensating plate. The coated sheet is particularly effective for an image display on which they are mounted.
摘要:
A multi-layer phase retarder is a laminated member of a phase retarder satisfying 1.05≦&agr; 1 with following proviso. The retardation in the normal direction by a light beam of a 400 nm wavelength is R1, the retardation in the normal direction by a light beam of a 550 nm is R2, the retardation in the perpendicular direction in the state tilted by 40 degrees with respect to the normal direction with the slow axis as the rotation axis is R3, and R1/R2 is &agr; and R3/R2 is &bgr;. An elliptical polarizer is alaminated member of the multi-layer phase retarder, and a polarizer. A liquid crystal display device includes the multi-layer phase retarder, or the same and a polarizer at least on one side of a liquid crystal cell.