Abstract:
High impact polystyrene may be formed with increased swell index and reduced or eliminated discoloration. A process of forming high impact polystyrene may include providing a polymerization system including a polymerization reactor and a devolatilizer. High impact polystyrene may be formed in the polymerization reactor, and sent to the devolatilizer. A polar antioxidant having a hindered phenol structure and an aliphatic amine group, and with a phosphite antioxidant may be added to the polymerization system. In another process, a chemical retarder and a fluorescent whitening agent may be added to the polymerization system. In another process, a chemical retarder that inhibits free radical rubber crosslinking may be added to the polymerization system.
Abstract:
A composition is provided for making a polyurethane that may be incorporated in various products, such as a sealant, a coating, a caulk, an electric potting compound, a membrane, a sponge, a foam, an adhesives, and a propellant binder. The composition includes one or more polyols, one or more isocyanate-group containing compounds having an isocyanate group functionality of at least two, and optionally one or more chain extenders. At least one of the polyols is a farnesene-based polyol having a number average molecular weight less than or equal to 100,000 g/mol and a viscosity at 25° C. less than 10,000 cP. The farnesene-based polyol may be a homopolymer or a copolymer of farnesene. The composition may also comprise additional polyols, such as a polyol of a homopolymer or copolymer of a polydiene. Methods of preparing a polyurethane are also provided.
Abstract:
A process for producing rubber modified polymers having an increased rubber phase volume, including feeding a vinyl aromatic monomer and an elastomer to a polymerization reactor to form a reaction mixture, polymerizing the reaction mixture, combining a copolymer to the polymerized reaction mixture to form a combined mixture, subjecting the combined mixture to further polymerization, and obtaining a rubber modified polymer product from the further polymerization.
Abstract:
A polymer composition of polypropylene copolymer and 1 to 50% by weight of hard resin. The polypropylene copolymer is either an impact copolymer or a random copolymer. The polymer composition can be used to make injection stretch blow molded articles having improved top load strength.
Abstract:
Polymer articles and processes of forming polymer articles are described herein. The processes generally include providing a propylene based polymer formed from a metallocene catalyst and melt processing the propylene based polymer to form a polymer article.
Abstract:
Injection stretch blow molded (ISBM) articles containing a bio-based polymers and methods of forming the same are described herein. The method generally includes providing a propylene-based polymer; contacting the propylene-based polymer with polylactic acid to form a polymeric blend; injection molding the blend into a preform; and stretch-blowing the preform into an article.
Abstract:
The method includes providing a high impact polystyrene (HIPS) reaction system, wherein the HIPS reaction system has a devolitalizer downstream of a reactor and injecting a retarding agent into the HIPS reaction system prior to the devolitalizer.
Abstract:
A process for producing rubber modified polymers having an increased rubber phase volume, including feeding a vinyl aromatic monomer and an elastomer to a polymerization reactor to form a reaction mixture, polymerizing the reaction mixture, combining a copolymer to the polymerized reaction mixture to form a combined mixture, subjecting the combined mixture to further polymerization, and obtaining a rubber modified polymer product from the further polymerization.