Air Curable Ethylene/Alpha-Olefin/Diene Interpolymer Composition

    公开(公告)号:US20200255639A1

    公开(公告)日:2020-08-13

    申请号:US16651855

    申请日:2017-09-30

    Abstract: A composition is composed of (A) an ethylene/alpha-olefin/diene TEMPO compound having the Structure (I) and (D) a peroxide. The molar ratio of isocyanate groups of Component (B) to the functional groups of Component (C) is from 0.80 to 1.10. A composition is composed of (A) an ethylene/alpha-olefin/diene interpolymer; a second composition comprising a reaction mixture comprising (B) an isocyanate comprising at least two isocyanate groups and (C) a TEMPO compound having the Structure (I) and (D) a peroxide, wherein the molar ratio of isocyanate groups of Component (B) to the functional groups of Component (C) is from 0.80 to 1.10. In Structure I, R1, R2, R3 and R4 are each independently selected from H and C1-C6 alkyl groups and X is a functional group selected from OH and NH2.

    Polyolefin blend composition and articles made therefrom

    公开(公告)号:US09982122B2

    公开(公告)日:2018-05-29

    申请号:US14391318

    申请日:2013-04-02

    Abstract: The instant invention provides a polyolefin blend composition, process for producing the same, and articles made therefrom. The polyolefin blend composition according to the present invention comprises: (a) from 75 to 97 percent by weight of one or more random propylene copolymers having a DSC melting point in the range of from 120° C. to 160° C., and a melt flow rate (MFR) in the range of from 1 to 120 g/10 minutes; (b) from 3 to 25 percent by weight of one or more ethylene ?-olefin copolymers having a melt index (I2) in the range of from 100 to 1500 g/10 minutes, a density in the range of 0.860 to 0.910 g/cm3, and a molecular weight (Mw) in the range of from 10,000 to 50,000 g/mole, wherein said ethylene ?-olefin copolymer is homogenously branched copolymer, and wherein said ethylene ?-olefin copolymer is linear or substantially linear; (c) optionally from 5 to 15 percent by weight of one or more propylene ?-olefin interpolymers having a DSC melting point in the range of less than 110° C., a heat of fusion in the range of less than 50 Joules/gram, and a crystallinity in the range of from at least 1 percent by to 40 percent by weight, and a melt flow rate in the range of less than 80 g/10 minutes.

Patent Agency Ranking