Abstract:
A polyethylene composition suitable for use in a living hinge component, the composition comprising a first ethylene-based polymer component, wherein the first ethylene-based polymer component has a density of from 0.940 g/cc to less than 0.960 g/cc, a melt index, I2.16, of less than 0.5 g/10 min, and a weight average molecular weight, Mw,cc, as measured by gel permeation chromatography using conventional calibration, of greater than or equal to 200,000 g/mol, and a second ethylene-based polymer component, wherein the composition has an overall density of from 0.945 g/cc to 0.960 g/cc and an overall melt index, I2.16, of from 10 g/10 min to 70 g/10 min.
Abstract:
A polyethylene composition suitable for use in a living hinge component, the composition comprising a first ethylene-based polymer component, the first ethylene-based polymer component has a density of from 0.91.5 g/cc to less than 0.940 g/cc. and a melt index, I2.16, of less than 5 g/10 min. and a second ethylene-based polymer component, wherein the composition has an overall density of from 0.945 g/cc to 0.960 g/cc and an overall melt index, I2.16, of from 5 g/10 min to 20 g/10 min.
Abstract:
A multilayer ethylene-based shrink films comprising a core layer comprising a polyethylene resin,and two skin layers, wherein the core layer is positioned between the two skin layers,wherein the polyethylene resin comprises greater than 50 mol. % of the units derived from ethylene and less than 30 mol. % of the units derived from one or more alpha-olefin comonomers, has greater than 50% of the copolymer fraction eluting between 75.0° C. and 95.0° C. as determined by Crystallization Elution Fractionation (CEF), and has a density ranging from 0.915 to 0.940 g/cc, and wherein the film is biaxially-oriented.
Abstract:
Provided are bicomponent fibers with improved curvature. The bicomponent fibers comprise a first polymer region or first region and a second polymer region or second region. The first region according to embodiments of the present disclosure comprises an ethylene/alpha-olefin interpolymer and has a light scattering cumulative detector fraction (CDFLS) of greater than 0.1200, wherein the CDFLS is computed by measuring the area fraction of a low angle laser light scattering (LALLS) detector chromatogram greater than, or equal to, 1,000,000 g/mol molecular weight using Gel Permeation Chromatography (GPC). The second region comprises a polyester. The bicomponent fibers can be used for forming nonwovens.
Abstract:
In various embodiments, a polyethylene formulation has a density of greater than 0.940 g/cm3 when measured according to ASTM D792, and a high load melt index (I21) of 1.0 g/10 min to 10.0 g/10 min when measured according to ASTM D1238 at 190° C. and a 21.6 kg load. Moreover, the polyethylene formulation has a peak molecular weight (Mp(GPC)) of less than 50,000 g/mol, a number average molecular weight (Mn(GPC)) of less than 30,000 g/mol, and a weight fraction (w1) of molecular weight (MW) less than 10,000 g/mol of less than or equal to 10.5 wt %, as determined by Gel Permeation Chromatography (GPC). Articles made from the polyethylene formulation, such as articles made by blow molding processes are also provided.
Abstract:
Polyethylene formulations and articles produced therefrom, comprise a multimodal high density polyethylene (HDPE) composition, and 0.1 ppm to 300 ppm of a nucleating agent, wherein the multimodal HDPE composition comprises a density of 0.940 g/cm3 to 0.970 g/cm3 when measured according to ASTM D792, and a melt index (I2) of 0.1 g/10 min. to 10.0 g/10 min. when measured according to ASTM D1238 at 190° C. and a 2.16 kg load, and wherein the multimodal HDPE composition comprises an infrared cumulative detector fraction (CDFIR) of greater than 0.27 and an infrared cumulative detector fraction to light scattering cumulative detector fraction ratio (CDFIR/CDFLS) from 0.7 to 2.0.
Abstract:
A process comprising forming fibers having at least a first region and a second region wherein the first region comprises an ethylene/alpha olefin interpolymer composition characterized by: density in the range of 0.930 to 0.965 g/cm3; melt index (I2) in the range of from 10 to 60 g/10 minutes; molecular weight distribution in the range of from 1.5 to 2.6; tan delta at 1 radian/second of at least 45; a low temperature peak and a high temperature peak on an elution profile via improved comonomer composition distribution (ICCD) procedure; and full width at half maximum of the high temperature peak is less than 6.0° C. and stretching the fibers to an elongation of at least 20% thereby increasing curl of the fiber. The process may further include forming a non-woven from the fibers and the stretching of the fibers may occur before or after forming of the non-woven.
Abstract:
In accordance with one embodiment of the present disclosure, a nonwoven web may be manufactured by a process that includes forming a bicomponent fiber and forming the bicomponent fiber into the nonwoven web. The bicomponent fiber may comprise one or more primary polymer regions and two or more secondary polymer regions. The primary polymer regions may comprise polyethylene. The secondary polymer regions may comprise polypropylene, polyester, or polyamide. The primary polymer regions may comprise at least 2.5 wt. % of polypropylene, polyester, or polyamide, or the secondary polymer regions may comprise at least 2.5 wt. % of polyethylene, or both.
Abstract:
The present disclosure provides a plastic living hinge. The plastic living hinge includes a blend containing (A) an ethylene-based polymer; and (B) a composite component selected from the group consisting of a block composite, a crystalline block composite, and a combination thereof.