BIORIENTED POLYETHYLENE FILM
    31.
    发明申请

    公开(公告)号:US20190299517A1

    公开(公告)日:2019-10-03

    申请号:US16435935

    申请日:2019-06-10

    Abstract: The present invention discloses a process for forming a biaxially oriented film. The process includes first selecting a polyolefin resin wherein said polyolefin resin comprises a linear low density polyethylene resin characterized by having from 9 to 35 weight percent of the total weight of linear low density polyethylene resin eluting from a CEF at a temperature greater than 97.0° C.; and further characterized by having a CDR of from 33 to 80 and a Mw Ratio of from 0.15 to 0.45. Next a film is formed from the polyolefin resin selected in the first step. Finally the film formed in the second step is oriented in a sequential manner. The films produced by this process are characterized by having an ultimate elongation at least 1.5 times greater in the MD as compared to the CD and the 2% secant modulus is a least 1.25 times greater in the CD as compared to the MD. The films are further characterized by having free residual shrinkage of less than 10% in the MD and less than 10% in the CD when exposed to a temperature of 90° C. for 10 minutes.

    MULTILAYER FILMS AND LAMINATES AND ARTICLES COMPRISING THE SAME

    公开(公告)号:US20190210333A1

    公开(公告)日:2019-07-11

    申请号:US16325888

    申请日:2017-08-14

    Abstract: Embodiments of the present invention relate to biaxially oriented, multilayer polyethylene films and to laminates and articles formed therefrom. In one aspect, a biaxially oriented, multilayer polyethylene film comprises Layer A which is a sealant layer p having a top facial surface and a bottom facial surface and comprising a first polyethylene, wherein the first polyethylene has a density of at least 0.900 g/cm3, an IHDF>95 of 20-60 kg/mol, and a MWHDF>95 of greater than 130 kg/mol, wherein Layer A comprises at least 50 weight percent of the first polyethylene based on the weight of Layer A, and Layer B having a top facial surface and a bottom facial surface, wherein Layer B comprises one or more additional polyethylenes, and wherein the top facial surface of Layer B is in adhering contact with a bottom facial surface of Layer A, wherein the density of the first polyethylene is at least 0.002 g/cm3 less than the density of Layer B.

    LAMINATE MATERIAL WITH SUPERIOR BARRIER PERFORMANCE AND PREPARATION METHOD THEREOF

    公开(公告)号:US20240416630A1

    公开(公告)日:2024-12-19

    申请号:US18698564

    申请日:2021-11-08

    Abstract: Provided are a laminate material, an article comprising the laminate material and a method for preparing the laminate material. The laminate material, comprises a first substrate comprising at least one metalized PE-based film, a second substrate comprising at least one PE-based film, and an adhesive layer adhering the first substrate to the second substrate, wherein the adhesive layer is derived from a two-component solvent-based polyurethane adhesive composition, and wherein the concentration of fatty acids or fatty acid derivatives in the metalized PE-based film is less than 300 ppm, based on the total weight of the metalized PE-based film. The two-component solvent-based polyurethane adhesive composition comprises a polyester polyol component and a polyisocyanate component, wherein the polyol component has 40 wt %-60 wt % of aromatic rings in the backbone, based on the total weight of the polyester polyol and a Mw between 5.000 and 50.000, and wherein the weight ratio of the polyester polyol component to polyisocyanate component is from 100:5 to 100:30.