Compositions for removal of processing byproducts and method for using same
    51.
    发明授权
    Compositions for removal of processing byproducts and method for using same 失效
    用于除去加工副产物的组合物及其使用方法

    公开(公告)号:US07582570B2

    公开(公告)日:2009-09-01

    申请号:US11312110

    申请日:2005-12-20

    Inventor: Donald L. Yates

    Abstract: A composition and methods for using the composition in removing processing byproducts is provided. The composition can be non-aqueous or semi-aqueous. The non-aqueous composition includes a non-aqueous solvent and one or more components including a fluoride compound and a pyridine compound. The semi-aqueous composition includes glacial acetic acid and one or more components including a fluoride compound and a pyridine compound. The composition can be used in removing processing byproducts from substrate assembly, including MRAM devices, that include at least a metal containing region and processing byproducts, where removing the processing byproducts includes exposing the substrate assembly to the composition for a time effective to remove at least a portion of the processing byproducts.

    Abstract translation: 提供了组合物和使用该组合物去除加工副产物的方法。 组合物可以是非水或半水性的。 非水性组合物包括非水溶剂和一种或多种包含氟化物和吡啶化合物的组分。 半水性组合物包括冰醋酸和一种或多种组分,包括氟化物和吡啶化合物。 该组合物可用于从包括至少含金属区域和加工副产物的基片组装(包括MRAM器件)中除去加工副产物,其中除去加工副产物包括将基片组件暴露于组合物上一段时间以有效地除去至少 一部分加工副产品。

    Compositions for Dissolution of Low-K Dielectric Films, and Methods of Use
    52.
    发明申请
    Compositions for Dissolution of Low-K Dielectric Films, and Methods of Use 有权
    低K电介质膜溶出的组合物及其使用方法

    公开(公告)号:US20090001314A1

    公开(公告)日:2009-01-01

    申请号:US12146113

    申请日:2008-06-25

    Inventor: Donald L. Yates

    Abstract: An improved composition and method for cleaning the surface of a semiconductor wafer are provided. The composition can be used to selectively remove a low-k dielectric material such as silicon dioxide, a photoresist layer overlying a low-k dielectric layer, or both layers from the surface of a wafer. The composition is formulated according to the invention to provide a desired removal rate of the low-k dielectric and/or photoresist from the surface of the wafer. By varying the fluorine ion component, and the amounts of the fluorine ion component and acid, component, and controlling the pH, a composition can be formulated in order to achieve a desired low-k dielectric removal rate that ranges from slow and controlled at about 50 to about 1000 angstroms per minute, to a relatively rapid removal of low-k dielectric material at greater than about 1000 angstroms per minute. The composition can also be formulated to selectively remove a photoresist layer, leaving the underlying low-k dielectric layer essentially intact.

    Abstract translation: 提供了用于清洁半导体晶片的表面的改进的组合物和方法。 该组合物可用于选择性地除去低k介电材料,例如二氧化硅,覆盖低k电介质层的光致抗蚀剂层,或从晶片表面两层。 根据本发明配制组合物以从晶片的表面提供低k电介质和/或光致抗蚀剂的期望的去除速率。 通过改变氟离子成分以及氟离子成分和酸,成分和控制pH的量,可以配制组合物以实现期望的低k电介质去除速率,其范围从慢和约在约 每分钟50至约1000埃,以每分钟大约1000埃的速度相对快速地除去低k电介质材料。 组合物也可以配制成选择性地除去光致抗蚀剂层,使底层的低k电介质层基本上完整无缺。

    Methods of fabricating integrated circuitry
    53.
    发明授权
    Methods of fabricating integrated circuitry 失效
    集成电路的制造方法

    公开(公告)号:US07419768B2

    公开(公告)日:2008-09-02

    申请号:US10299165

    申请日:2002-11-18

    Inventor: Donald L. Yates

    Abstract: The invention includes methods of fabricating integrated circuitry and semiconductor processing polymer residue removing solutions. In one implementation, a method of fabricating integrated circuitry includes forming a conductive metal line over a semiconductor substrate. The conductive line is exposed to a solution comprising an inorganic acid, hydrogen peroxide and a carboxylic acid buffering agent. In one implementation, a method of fabricating integrated circuitry includes forming an insulating layer over a semiconductor substrate. A contact opening is at least partially formed into the insulating layer. The contact opening is exposed to a solution comprising an inorganic acid, hydrogen peroxide and a carboxylic acid buffering agent. In one implementation, a semiconductor processing polymer residue removing solution comprises an inorganic acid, hydrogen peroxide and a carboxylic acid buffering agent. Other aspects and implementations are contemplated.

    Abstract translation: 本发明包括制造集成电路和半导体处理聚合物残渣除去溶液的方法。 在一个实现中,制造集成电路的方法包括在半导体衬底上形成导电金属线。 导电线暴露于包含无机酸,过氧化氢和羧酸缓冲剂的溶液中。 在一个实施方案中,制造集成电路的方法包括在半导体衬底上形成绝缘层。 接触开口至少部分地形成在绝缘层中。 将接触开口暴露于包含无机酸,过氧化氢和羧酸缓冲剂的溶液中。 在一个实施方案中,半导体加工聚合物残渣除去溶液包含无机酸,过氧化氢和羧酸缓冲剂。 考虑了其他方面和实现。

    Method of reducing water spotting and oxide growth on a semiconductor structure
    54.
    发明授权
    Method of reducing water spotting and oxide growth on a semiconductor structure 失效
    减少半导体结构上的水斑和氧化物生长的方法

    公开(公告)号:US07163019B2

    公开(公告)日:2007-01-16

    申请号:US10633069

    申请日:2003-08-01

    Inventor: Donald L. Yates

    Abstract: The present invention relates to a method of cleaning and drying a semiconductor structure in a modified conventional gas etch/rinse or dryer vessel. In an embodiment of the present invention, a semiconductor structure is placed into a first treatment vessel and chemically treated. Following the chemical treatment, the semiconductor structure is transferred directly to a second treatment vessel where it is rinsed with DI water and then dried. The second treatment vessel is flooded with both DI water and a gas that is inert to the ambient, such as nitrogen, to form a DI water bath upon which an inert atmosphere is maintained during rinsing. Next, an inert gas carrier laden with IPA vapor is fed into the second treatment vessel. After sufficient time, a layer of IPA has formed upon the surface of the DI water bath to form an IPA-DI water interface. The semiconductor structure is drawn out of the DI water bath at a rate that allows substantially all DI water, and contaminants therein, to be entrained beneath the IPA-DI water interface. In a second embodiment of the present invention, chemical treatment, rinsing, and drying are carried out in a single vessel. In a third embodiment of the present invention, a retrofitted spray/dump rinser with a lid is used for rinsing and drying according to the method of the present invention.

    Abstract translation: 本发明涉及一种在改进的常规气体蚀刻/漂洗或干燥容器中清洗和干燥半导体结构的方法。 在本发明的一个实施例中,将半导体结构放置在第一处理容器中并进行化学处理。 化学处理后,将半导体结构直接转移到第二处理容器,在其中用DI水冲洗然后干燥。 第二处理容器充满了DI水和对环境如氮气是惰性的气体,以形成在洗涤期间保持惰性气氛的去离子水浴。 接下来,将载有IPA蒸气的惰性气体载体进料到第二处理容器中。 在足够的时间之后,在去离子水浴表面上形成一层IPA以形成IPA-DI水界面。 将半导体结构从DI水浴中抽出,其速率允许基本上所有的去离子水和其中的污染物被夹带在IPA-DI水界面下面。 在本发明的第二个实施方案中,化学处理,漂洗和干燥在单个容器中进行。 在本发明的第三实施例中,根据本发明的方法,使用具有盖的改装的喷淋/倾卸式冲洗机进行漂洗和干燥。

    Cleaning composition useful in semiconductor integrated circuit fabrication

    公开(公告)号:US07087561B2

    公开(公告)日:2006-08-08

    申请号:US10187163

    申请日:2002-07-01

    CPC classification number: C11D7/08 C11D7/265 C11D11/0047

    Abstract: A composition for use in semiconductor processing wherein the composition comprises water, phosphoric acid, and an organic acid; wherein the organic acid is ascorbic acid or is an organic acid having two or more carboxylic acid groups (e.g., citric acid). The water can be present in about 40 wt. % to about 85 wt. % of the composition, the phosphoric acid can be present in about 0.01 wt. % to about 10 wt. % of the composition, and the organic acid can be present in about 10 wt. % to about 60 wt. % of the composition. The composition can be used for cleaning various surfaces, such as, for example, patterned metal layers and vias by exposing the surfaces to the composition.

    Method of improving surface planarity prior to MRAM bit material deposition
    57.
    发明授权
    Method of improving surface planarity prior to MRAM bit material deposition 有权
    在MRAM钻头材料沉积之前提高表面平面度的方法

    公开(公告)号:US06743641B2

    公开(公告)日:2004-06-01

    申请号:US10022721

    申请日:2001-12-20

    CPC classification number: H01L27/222 G11C11/15 H01L21/7684

    Abstract: The present invention provides a method of fabricating a portion of a memory cell, the method comprising providing a first conductor in a trench which is provided in an insulating layer and flattening an upper surface of the insulating layer and the first conductor, forming a material layer over the flattened upper surface of the insulating layer and the first conductor and flattening an upper portion of the material layer while leaving intact a lower portion of the material layer over the insulating layer and the first conductor.

    Abstract translation: 本发明提供了一种制造存储单元的一部分的方法,该方法包括提供一沟槽中的第一导体,其设置在绝缘层中并使绝缘层和第一导体的上表面平坦化,形成材料层 在绝缘层和第一导体的平坦的上表面上方,并且使材料层的上部平坦化,同时在绝缘层和第一导体上完整地保留材料层的下部。

    Methods of making magnetoresistive memory devices
    59.
    发明授权
    Methods of making magnetoresistive memory devices 有权
    制造磁阻存储器件的方法

    公开(公告)号:US06656372B2

    公开(公告)日:2003-12-02

    申请号:US09971758

    申请日:2001-10-04

    Inventor: Donald L. Yates

    CPC classification number: H01L43/12 H01L27/222

    Abstract: The invention includes methods of forming magnetoresistive devices. In one method, a construction is formed which includes a first magnetic layer, a non-magnetic layer over the first magnetic layer, and a second magnetic layer over the non-magnetic layer. A first pattern is extended through the second magnetic layer and to the non-magnetic layer with an etch selective for the material of the second magnetic layer relative to the material of the non-magnetic layer. A dielectric material is formed over the patterned second magnetic layer, and subsequently a second etch is utilized to extend a second pattern through the non-magnetic layer and at least partway into the first magnetic layer.

    Abstract translation: 本发明包括形成磁阻器件的方法。 在一种方法中,形成包括第一磁性层,第一磁性层上的非磁性层和非磁性层上的第二磁性层的结构。 相对于非磁性层的材料,第一图案通过第二磁性层和与非磁性层相对于第二磁性层的材料的选择性蚀刻而延伸。 介电材料形成在图案化的第二磁性层之上,随后利用第二蚀刻来延伸通过非磁性层的第二图案,并且至少部分地进入第一磁性层。

    Cleaning composition useful in semiconductor integrated circuit fabrication
    60.
    发明授权
    Cleaning composition useful in semiconductor integrated circuit fabrication 有权
    用于半导体集成电路制造的清洁组合物

    公开(公告)号:US06486108B1

    公开(公告)日:2002-11-26

    申请号:US09584552

    申请日:2000-05-31

    CPC classification number: C11D7/08 C11D7/265 C11D11/0047

    Abstract: A composition for use in semiconductor processing wherein the composition comprises water, phosphoric acid, and an organic acid; wherein the organic acid is ascorbic acid or is an organic acid having two or more carboxylic acid groups (e.g., citric acid). The water can be present in about 40 wt. % to about 85 wt. % of the composition, the phosphoric acid can be present in about 0.01 wt. % to about 10 wt. % of the composition, and the organic acid can be present in about 10 wt. % to about 60 wt. % of the composition. The composition can be used for cleaning various surfaces, such as, for example, patterned metal layers and vias by exposing the surfaces to the composition.

    Abstract translation: 一种用于半导体加工的组合物,其中组合物包含水,磷酸和有机酸; 其中有机酸是抗坏血酸,或者是具有两个以上羧酸基团的有机酸(例如柠檬酸)。 水可以约40wt。 %至约85重量% 组合物的%,磷酸可以以约0.01重量%存在。 %至约10wt。 %的组成,并且有机酸可以以约10重量% %至约60wt。 %的组成。 组合物可以用于通过将表面暴露于组合物来清洁各种表面,例如图案化的金属层和通孔。