摘要:
Molding materials are composed ofA) from 5 to 95% by weight of polyaryl ethers,B) from 5 to 95% by weight of a mixture (B) ofB.sub.I) from 75 to 97% by weight of partly aromatic polyamides andB.sub.II) from 3 to 25% by weight of a rubber impact modifierand furthermoreC) from 0 to 40% by weight of additives and/or processing assistants.
摘要:
Silicon single crystals are pulled from a melt in a crucible, the single crystal surrounded by a heat shield, the lower end of which is a distance h from the melt surface, wherein gas flows downward between the single crystal and the heat shield, outward between the lower end of the heat shield and the melt, and then upward in the region outside the heat shield. The internal diameter of the heat shield at its lower end is 55 mm or more than the diameter of the single crystal, and the radial width of the heat shield at its lower end is not more than 20% of the diameter of the single crystal. Highly doped single crystals pulled accordingly have a void concentration ≤50 m−3.
摘要:
Thermoplastic molding compositions comprising: a) 3 to 91.8 wt % of at least one polyamide, as component A, b) 3 to 91.8 wt % of one or more styrene copolymers B without any maleic anhydride-derived units, c) 3 to 91.8 wt % of one or more impact-modifying grafted rubbers C, d) 0.2 to 1.5 wt % of a compound of formula (I), as component D: e) 0 to 0.9 wt % of a mixture of formula (II), as component E: f) 0 to 0.9 wt % of a further stabilizer component F, g) 1 to 25 wt % of one or more styrene copolymers G, h) 1 to 30 wt % of one or more further rubbers, exhibit improved weathering resistance.
摘要:
Molding compositions comprising: a composition (I) present in an amount of 10 to 100% by weight, based on the molding composition, wherein the composition (I) comprises: (A) 40 to 95% by weight, based on the composition (I), of a copolymer comprising: α-methylstyrene in an amount of 55 to 90% by weight, acrylonitrile in an amount of 10 to 50% by weight, and one or more other monomers in an amount of 0 to 5% by weight, wherein the percentages by weight of the α-methylstyrene, the acrylonitrile and the one or more other monomers are based on the weight of component (A); (B) 2.5 to 75% by weight, based on the composition (I), of a polymer comprising: a vinylaromatic monomer in an amount of 60 to 90% by weight, acrylonitrile in an amount of 8.01 to 39.8% by weight, and maleic anhydride in an amount of 0.2 to 1.99% by weight, wherein the percentages by weight of the vinylaromatic monomer, the acrylonitrile and the maleic anhydride are based on the weight of component (B); and (C) 2.5 to 60% by weight, based on the composition (I), of glass fibers.
摘要:
The present invention relates to a process for the production of polyarylene ether block copolymers comprising, in a first stage, the reaction of at least one aromatic dihydroxy compound comprising 4,4′-dihydroxybiphenyl in a molar excess and of at least one aromatic dihalogen compound, to form a polybiphenyl sulfone polymer, and then, in a second stage, the reaction of the polybiphenyl sulfone polymer with at least one aromatic dihydroxy compound and of at least one aromatic dihalogen compound.The invention further relates to the resultant polyarylene sulfone block copolymers and to the use of the polyarylene sulfone block copolymers for the production of moldings, fibers, films, or foams.
摘要:
A process for producing an expandable pelletized polymeric material which comprises: a) providing a polymer component, consisting of a styrene polymer component having a glass transition temperature of ≧130° C., formed from and one or more thermoplastic polymers selected from the group consisting of aromatic polyethers; polyolefins; polyacrylates; polycarbonates; polyesters; polyamides; polyether sulfones; polyether ketones and polyether sulfides, (b) heating the polymer component to form a polymer melt, (c) introducing a blowing agent component into the polymer melt to form a foamable melt, (d) homogenizing the mixture, (f) extruding the blowing agent-containing polymer melt through a die plate, (g) pelletizing the blowing agent-containing melt in a liquid-filled chamber to form a pelletized material. The expandable pelletized material is suitable for production of molded foam bodies, the applications as insulation material and as structural foam elements for lightweight construction and composite applications.
摘要:
Silicon wafers having a density of BMDs with sizes between 20 to 40 nm at positions ≧20 μm below the wafer surface in the range of 5×1011/cm3, and a density of BMDs with sizes of ≧300 nm≦1×107/cm3, exhibit reduced slip dislocation and warpage. The wafers are sliced from a crystal grown under specific conditions and then subjected to both low temperature heat-treatment and high temperature anneal.
摘要翻译:在晶片表面的≥20μm的位置处,在5×10 11 / cm 3范围内具有尺寸在20至40nm之间的BMD的密度的硅晶片,以及尺寸为≥300nm< 1×107 / cm3的BMD的密度 ,表现出减滑脱位和翘曲。 将晶片从在特定条件下生长的晶体切片,然后进行低温热处理和高温退火。
摘要:
The present invention relates to a method for producing fiber-reinforced composite materials, in which a multiplicity of continuous filaments or woven fabric is impregnated optionally together with reinforcing materials, comprising caprolactam and other starting materials for polyamide 6 or other starting materials for copolymers of caprolactam, passed through at temperatures of 70 to 100° C., and anionically polymerized at temperatures of 100 to 190° C., and optionally repolymerized at temperatures of 90 to 170° C.
摘要:
The present invention relates to a process for the production of polyarylene ether block copolymers comprising, in a first stage, the reaction of at least one aromatic dihydroxy compound comprising 4,4′-dihydroxybiphenyl in a molar excess and of at least one aromatic dihalogen compound, to form a polybiphenyl sulfone polymer, and then, in a second stage, the reaction of the polybiphenyl sulfone polymer with at least one aromatic dihydroxy compound and of at least one aromatic dihalogen compound.The invention further relates to the resultant polyarylene sulfone block copolymers and to the use of the polyarylene sulfone block copolymers for the production of moldings, fibers, films, or foams.
摘要:
An aromatic polyether sulfone block copolymer comprises hydrophilic segments which have sulfonic acid groups and hydrophobic segments which have no sulfonic acid groups, wherein the proportion by weight of hydrophilic segments is from 0.02 to 0.35.