Abstract:
A packaging material for a power storage device includes a base material layer as an outer layer, a heat fusible resin layer as an inner layer, and a metal foil layer arranged between both the layers. The base material layer and the metal foil layer are adhered via an outer adhesive layer. The outer adhesive layer is formed of a cured film of a two-part curing type urethane adhesive agent including a main agent containing a polyol and a multifunctional isocyanate mixture, wherein a content rate of the polyol is 50 mass % to 95 mass %. The multifunctional isocyanate mixture is composed of a mixture containing an aromatic multifunctional isocyanate and an aliphatic multifunctional isocyanate having an aromatic ring.
Abstract:
A sealant film has a structure made of a laminated body of two or more layers. The laminated body includes a first resin layer 7 containing 50 mass % or more of a random copolymer containing propylene and a copolymer component other than propylene as copolymer components, and a second resin layer 8 formed by a mixed resin containing a first elastomer-modified olefin based resin having a melting point of 155° C. or higher and a crystal melting energy of 50 J/g or more, and a second elastomer-modified olefin based resin having a melting point is 135° C. or higher and a crystal melting energy of 30 J/g or less. With this structure, when the inner pressure of a power storage device is excessively increased, breakage (separation) occurs inside the sealant layer, causing gas-releasing, which in turn can prevent bursting of the packaging material due to the inner pressure increase.
Abstract:
A power storage device includes a positive electrode part including a first metallic foil layer and a positive electrode active material layer partially laminated on one surface of the first metallic foil layer, a negative electrode part including a second metallic foil layer and a negative electrode active material layer partially laminated on one surface of the second metallic foil layer, and a separator arranged between the positive electrode part and the negative electrode part. The positive electrode active material layer is arranged between the first metallic foil layer and the separator, and the negative electrode active material layer is arranged between the second metallic foil layer and the separator. The peripheral regions of the one surfaces of the first and second metallic foil layers in which the positive and negative electrode active material layers are not formed are joined via a peripheral sealing layer containing a thermoplastic resin.
Abstract:
In laminating resin layers on both surfaces of a metal foil layer by adhering a heat-resistant resin layer to a first surface of the metal foil layer and adhering a heat-sealable resin layer to a second surface thereof, as an adhering method, by employing an adhesive agent unapplied portion forming and adhering process in which the resin layer and the metal foil layer are adhered together by applying an adhesive agent to a region of a joining face of both the layers excluding a part of the region so that an adhesive agent unapplied section is formed, a laminated body having the adhesive agent unapplied section is manufactured. A resin layer removal process for removing a resin layer corresponding to the adhesive agent unapplied section of the laminated body to expose the metal foil layer is performed.
Abstract:
An outer packaging material for a battery includes a heat resistant stretched resin film layer as an outer layer integrally laminated on one of surfaces of an aluminum foil layer via a first adhesive layer. A thermoplastic unstretched resin film layer as an inner layer is integrally laminated on the other surface of the aluminum foil layer via a second adhesive layer. An adhesive strength between the inner layer and the aluminum foil layer is 4N/15 mm-width to 30N/15 mm-width, and an adhesive strength between the outer layer and the aluminum foil layer is 2N/15 mm-width to 14N/15 mm-width. As a thermoplastic unstretched resin film constituting the inner layer, a thermoplastic unstretched resin film having a sealing strength of two sheets of the thermoplastic unstretched resin films arranged one on the other and heat sealed exceeding 30N/15 mm-width but not exceeding 110N/15 mm-width is used.
Abstract:
A package for a power storage device includes at least one laminated packaging material having first and second sections. The packaging material includes a metallic foil layer, a heat-resistant resin layer, and a heat-fusible resin layer. In a state in which the heat-fusible resin layers of the first and second sections are faced, peripheral edges thereof are heat-sealed to form a storage chamber for accommodating a device main body. One of the sections is extended outside the storage chamber to form a conductive flange having an exposed heat-fusible resin layer. The conductive flange is provided with an external conductive section in which the heat-fusible resin layer is partially removed to expose the metallic foil layer. The packaging material having the external conductive section is provided with an internal conductive section in the storage chamber in which the heat-fusible resin layer is partially removed to expose the metallic foil layer.
Abstract:
A molding packaging material includes an outer substrate layer made of a heat-resistant resin, an inner sealant layer made of a thermoplastic resin, a metallic foil layer provided between the outer substrate layer and the inner sealant layer, and a protection coat layer formed on a side opposite to the metallic foil layer side of the outer substrate layer. The protection coat layer is made of a resin composition including a main resin containing a phenoxy resin and a urethane resin, and a curing agent, and has a thickness of 0.1 μm to 10 μm.
Abstract:
The present invention provides a molding material for package including a matte-coating layer having excellent formability, chemical resistance, solvent resistance, electrolytic solution resistance and printing property. The molding material for package (1) includes an outer base material layer (13) comprising a heat-resistant resin; an inner sealant layer (16) comprising a thermoplastic resin; a metal foil layer (11) disposed between the outer base material layer (13) and the inner sealant layer (16); and a matte-coating layer (14) formed on a side opposite to the metal foil layer (11) of the outer base material layer (13), wherein the matte-coating layer (14) is a multilayer including a bottom layer (14a) comprising a resin composition including a main agent resin including a phenoxy resin and a urethane resin, a curing agent, and solid fine particles; and an upper layer (14b) comprising a resin composition including a fluorine-containing resin.
Abstract:
A tab lead including a first insulating film made of resin is adhered to one of surfaces of a part of a region of a metal plate in a length direction of the metal plate and a second insulating film made of resin is adhered to the other surface of the part of the region. Both end portions of the first insulating film and both end portions of the second insulating film are integrally welded to each other. First protruding portions protruding outward in a thickness direction of the first insulating film are formed at regions of the first insulating film corresponding to both widthwise side edges of the metal plate and vicinities thereof. Second protruding portions protruding outward in a thickness direction of the second insulating film are formed at regions of the second insulating film corresponding to both widthwise side edges of the metal plate and vicinities thereof.
Abstract:
An outer casing material for a battery 4 is provided, wherein an outer layer 11, a metal foil layer 10 and an inner layer 8 are laminated via an adhesive layer 5; the inner layer 8 comprises a sealant layer 8b and a base material layer 8a; the sealant layer 8b is made from a propylene-ethylene random copolymer wherein a melt flow rate at 230° C. thereof is in a range of 3 to 30 g/10 minutes; the base material layer 8a is made of a resin composition wherein a melt flow rate at 230° C. thereof is in a range of 0.1 to 15 g/10 minutes, xylene-soluble component Xs thereof satisfies the predetermined conditions, and the resin composition comprises 50 to 80% by mass of a propylene component (A) and 50 to 20% by mass of a copolymer component (B) which is an elastomer of a copolymer of propylene and ethylene and/or α-olefin having 4 to 12 carbons and includes 50 to 85% by mass of a polymerization unit originated from propylene.