摘要:
The present invention provides a solventless, continuous process, which includes: in at least one extruder, intensive compounder, intensive mixer or static mixer, mixing and heating a reaction mixture including the following (A), (B), and one or both of (C) and (D): (A) at least one aliphatic, (cyclo)aliphatic and/or cycloaliphatic C3-C50 diisocyanate compound; (B) at least one aliphatic, (cyclo)aliphatic and/or cycloaliphatic C3-C50 polyisocyanate compound containing one or more isocyanurate groups; (C) 1,2,4-triazole; (D) one or more pyrazole having the formula: where R1, R2 and R3 simultaneously or independently of one another are hydrogen or alkyl, alkenyl, aralkyl, aryl or N-substituted carbamoyl groups, halogen or —C(═O)—O—R4, where R4 is a C1-C12 alkyl group; to obtain a product mixture including at least one (semi)crystalline, blocked C3-C50 isocyanate compound and at least one amorphous, blocked C3-C50 isocyanate compound. The present invention also provides a composition prepared by the process and methods of using the composition.
摘要:
The invention relates to a continuous process for producing a reactive polymer based on compounds according to the structures (A1) and/or (A2) and phenolic resin in an extruder and to the reactive polymer produced according to said process and the use thereof for producing composite materials.
摘要:
Process for the continuous preparation of prepolymers based on phenolic resin, an oxazoline component and an epoxide in the presence of a catalyst, including supplying the phenolic resin and the oxazoline component to an extruder in a stream A; a Lewis adduct of boron trifluoride or of aluminium trichloride, or arylsulphonic acids or alkylsulphonic acids, or latent arylsulphonic acids or latent alkylsulphonic acids, in a stream B, and the epoxide in a stream C, the infeed of stream A being situated, as seen in extrusion direction, before the infeed of stream C, these reactants are mixed at a reaction temperature of 120 to 200° C. with a residence time in the extruder of 3 seconds to 15 minutes, and then the product discharge of the extruder is cooled to a temperature of less than 45° C. within from 30 to 60 seconds.
摘要:
The invention relates to heat-curing powder-lacquer compositions exhibiting a matte surface after curing of the coating, as well as to a simple method for production of the same.