A CIS solar cell having flexibility and high conversion efficiency may be produced, using, as a substrate, a polyimide film which is prepared from an aromatic tetracarboxylic acid component comprising 3,3′,4,4′-biphenyltetracarboxylic dianhydride as the main component and an aromatic diamine component comprising p-phenylenediamine as the main component, and has a maximum dimensional change in the temperature-increasing step of from 25° C. to 500° C. within a range of from +0.6% to +0.9%, excluding +0.6%, based on the dimension at 25° C. before heat treatment.
摘要:
Disclosed is a polyimide film prepared from an aromatic tetracarboxylic acid component and an aromatic diamine component, which has a dimensional change from 25° C. to 500° C. within a range of from −0.3% to +0.6% based on the initial dimension at 25° C. The polyimide film may be used as a substrate for a CIS solar cell.
摘要:
A polyimide-metal laminate comprising a polyimide film and a metal layer for use as an electrode, which is formed on the side (Side B) of the polyimide film which was in contact with a support when producing a self-supporting film in the production of the polyimide film, is used to produce a CIS solar cell.
摘要:
Disclosed is a polyimide film prepared from an aromatic tetracarboxylic acid component and an aromatic diamine component, which has a dimensional change from 25° C. to 500° C. within a range of from −0.3% to +0.6% based on the initial dimension at 25° C. The polyimide film may be used as a substrate for a CIS solar cell.
摘要:
A polyimide-metal laminate comprising a polyimide film and a metal layer for use as an electrode, which is formed on the side (Side B) of the polyimide film which was in contact with a support when producing a self-supporting film in the production of the polyimide film, is used to produce a CIS solar cell.
摘要:
A composite tank that can suppress electrification, corrosion and strength degradation, a wing comprising the composite tank, and a method for manufacturing the composite tank. The composite tank comprises: a tank body inside which a combustible material is stored, having a first resin portion (11, 12) formed from a fiber reinforced resin and a metal portion formed from a metal material, a second resin portion (22) formed from a fiber reinforced resin, which covers at least those regions on the inner surface of the tank body where the first resin portion (11, 12) adjoins the metal portion, and a plurality of conductive portions (23) that enable charge transfer through the second resin portion (22), from the surface that contacts the combustible material to the first resin portion (11, 12), wherein the fiber in the second resin portion (22) has a higher electrical resistivity than fiber in the first resin portion (11, 12), and the second resin portion (22) forms a layer that isolates the first resin portion (11, 12) from the metal portion.
摘要:
Provided is a coating material that can prevent galvanic corrosion and is resistant to electrostatic charging. An antistatic coating comprising a primer containing either an inorganic fiber comprising Si, Ti or Zr, C, and O, or an Ag filler. Further, a structure made of a composite material which is resistant to galvanic corrosion and electrostatic charging is obtained by applying the antistatic coating containing either an inorganic fiber comprising Si, Ti or Zr, C, and O, or an Ag filler to the surface of the structure made of a composite material to form a layers.
摘要:
The polyimide film of the present invention is to be used for the production of a wiring board having a metal wiring, which is formed by forming a metal layer on one side (Side B) of the polyimide film, and etching the metal layer; the polyimide film is curled toward the side (Side A) opposite Side B; and the curling of the polyimide film is controlled so as to reduce the drooping of the wiring board having a metal wiring formed thereon. The handling characteristics and productivity in IC chip mounting may be improved by the use of the polyimide film.
摘要:
A thermosetting solution composition composed of a biphenyltetracarboxylic acid compound containing a partial lower aliphatic alkyl ester of 2,3,3′,4′-biphenyltetracarboxylic acid and/or a partial lower aliphatic alkyl ester of 2,2′,3,3′-biphenyltetracarboxylic acid, an aromatic diamine compound in a molar amount larger than a molar amount of the biphenyltetracarboxylic acid compound, a partial lower aliphatic alkyl ester of 4-(2-phenylethynyl)phthalic acid compound in a molar amount as much as 1.8-2.2 times a molar amount corresponding to a difference between the molar amount of the aromatic diamine compound and the molar amount of the biphenyltetracarboxylic acid compound, and an organic solvent composed of a lower aliphatic alcohol is of value for manufacture of a prepreg.
摘要:
A polyimide obtained by reacting a tetracarboxylic acid component with a diamine component containing a diamine compound represented by the following general formula (1): wherein, A represents a biphenylene group which may be substituted with an alkyl group having up to 4 carbon atoms.