Copolymers of alpha-methyl styrene and acrylonitrile
    1.
    发明授权
    Copolymers of alpha-methyl styrene and acrylonitrile 失效
    α-甲基苯乙烯和丙烯腈的共聚物

    公开(公告)号:US4755576A

    公开(公告)日:1988-07-05

    申请号:US765601

    申请日:1985-08-14

    CPC分类号: C08F212/12

    摘要: Copolymers of from 65 to 75%, by weight, of .alpha.-methyl styrene and from 35 to 25%, by weight, of .alpha.-methyl styrene and from 35 to 25%, by weight, of acrylonitrile, obtainable by radical emulsion polymerization, the monomers being metered in during the course of the polymerization, wherein the molar ratio: ##EQU1## of the unreacted monomers in the reaction mixture is maintained during the metering phase between 0.7 and 1.25.

    摘要翻译: 65至75重量%的α-甲基苯乙烯和35至25重量%的α-甲基苯乙烯和35至25重量%的丙烯腈的共聚物,可通过自由基乳液聚合获得, 在聚合过程中计量单体,其中反应混合物中未反应单体的摩尔比:在计量阶段期间维持在0.7和1.25之间。

    Thermoplastic molding materials based on special graft rubber components
    4.
    发明授权
    Thermoplastic molding materials based on special graft rubber components 失效
    基于特殊接枝橡胶成分的热塑性成型材料

    公开(公告)号:US06828380B2

    公开(公告)日:2004-12-07

    申请号:US10220707

    申请日:2002-11-21

    IPC分类号: C08L5502

    摘要: A molding composition having good surface gloss, high elongation at break and good thermoplastic processability is disclosed. The composition contains (A) a graft polymer that is obtained by free-radical polymerization of resin-forming vinyl monomers in the presence of rubber in latex form, (B) a copolymer of styrene and acrylonitrile and an optional (C) a resin selected from the group consisting of polycarbonates, polyester-carbonates, polyesters and polyamides. The preparation of the graft polymer is characterized in that (i) before the start of the grafting polymerization reaction the rubber latex is brought to a pH of 9 to 11, (ii) the redox initiator components are employed in amounts of 0.1 to 2.5 wt. % (based on the monomers metered in) and (iii) during the entire grafting polymerization reaction the pH remains constant±0.5 and in the range of 11.0 to 8.8, and (iv) the temperature difference between the start and end of the reaction is at least 10° C.

    摘要翻译: 公开了具有良好的表面光泽度,高断裂伸长率和良好的热塑性加工性能的成型组合物。 该组合物含有(A)通过在胶乳形式的橡胶存在下形成树脂的乙烯基单体的自由基聚合获得的接枝聚合物,(B)苯乙烯和丙烯腈的共聚物和任选的(C)树脂选择 由聚碳酸酯,聚酯 - 碳酸酯,聚酯和聚酰胺组成。 接枝聚合物的制备的特征在于:(i)在接枝聚合反应开始之前,使橡胶胶乳的pH值达到9至11,(ii)氧化还原引发剂组分的用量为0.1至2.5重量% 。 %(基于计量的单体)和(iii)在整个接枝聚合反应期间,pH保持恒定±0.5且在11.0至8.8的范围内,和(iv)反应开始和结束之间的温度差为 至少10℃

    Emulsifier composition
    10.
    发明授权
    Emulsifier composition 失效
    乳化剂组成

    公开(公告)号:US4360452A

    公开(公告)日:1982-11-23

    申请号:US170257

    申请日:1980-07-18

    摘要: An emulsifier composition comprising (a) a non-ionic emulsifier having an HLB-value of about 10 to 20 and (b) a polyoxyalkylene-polyester of which about 5 to 50% by weight comprises polyoxyalkylene radicals. It may be used in admixture with phosphoric acid esters, serving to reduce foaming and prevent settling of aqueous suspensions such as cement and calcium sulfate slurries.

    摘要翻译: 一种乳化剂组合物,其包含(a)HLB值为约10至20的非离子乳化剂和(b)约5至50重量%的聚氧化烯 - 聚酯包含聚氧化烯基团。 它可以与磷酸酯混合使用,用于减少起泡和防止水性悬浮液如水泥和硫酸钙浆液的沉降。