Method for producing a pellet from a fiber-filled resin composition and injection-molded products thereof
    1.
    发明授权
    Method for producing a pellet from a fiber-filled resin composition and injection-molded products thereof 失效
    从纤维填充树脂组合物及其注射成型体制造颗粒的方法

    公开(公告)号:US07641833B2

    公开(公告)日:2010-01-05

    申请号:US10594679

    申请日:2005-04-12

    IPC分类号: B29C47/60 B29B7/24

    摘要: An object of the present invention is to economically produce a resin composition pellet with the degradation of resin suppressed, by using an ordinary extruder, the resin composition pellet being filled with a desired filling amount of a uniformly compounded fibrous filler, and having a required weight average fiber length, in particular, to produce a resin composition pellet used for a socket of a planar socket pin in which the pitch interval of a lattice area of a semiconductor device is 2.0 mm or less, the thickness of the lattice area is 0.5 mm or less, and the height of the socket is 5.0 mm or less. To achieve the object, in supplying 80 to 55% by weight of resin and 20 to 45% by weight of the fibrous filler with a weight average fiber length of 1 mm or more to an extruder to produce a resin composition pellet in which a weight average fiber length of a fibrous filler is 180 to 360 μm, a part of an amount (x) of the resin is supplied through a main feed port of the extruder, and the fibrous filler and a remaining amount (1−x) of the resin are supplied through a side-feed port so that x/(1−x) becomes 50/50 to 10/90% by weight.

    摘要翻译: 本发明的目的是通过使用普通的挤出机经济地生产树脂降解降解的树脂组合物颗粒,所述树脂组合物颗粒填充有所需的填充量的均匀复合的纤维填料并具有所需的重量 平均纤维长度,特别是为了制造用于平面插座销的插座的树脂组合物颗粒,其中半导体器件的晶格面积的间距间隔为2.0mm或更小,晶格面积的厚度为0.5mm 以下,插座的高度为5.0mm以下。 为了达到上述目的,向挤出机中供给80〜55重量%的树脂和20〜45重量%的重均纤维长度为1mm以上的纤维填料,制成树脂组合物颗粒,其中重量 纤维填料的平均纤维长度为180〜360μm,树脂的量(x)的一部分通过挤出机的主供料口供给,纤维填料的剩余量(1-x) 树脂通过侧进料口供给,使得x /(1-x)成为50/50至10/90重量%。

    Method for producing resin composition pellet with lengh of fibrous filler controlled
    2.
    发明申请
    Method for producing resin composition pellet with lengh of fibrous filler controlled 失效
    生产具有纤维填料长度的树脂组合物颗粒的方法

    公开(公告)号:US20070194478A1

    公开(公告)日:2007-08-23

    申请号:US10594679

    申请日:2005-04-12

    IPC分类号: B29C45/00

    摘要: An object of the present invention is to economically produce a resin composition pellet with the degradation of resin suppressed, by using an ordinary extruder, the resin composition pellet being filled with a desired filling amount of a uniformly compounded fibrous filler, and having a required weight average fiber length, in particular, to produce a resin composition pellet used for a socket of a planar socket pin in which the pitch interval of a lattice area of a semiconductor device is 2.0 mm or less, the thickness of the lattice area is 0.5 mm or less, and the height of the socket is 5.0 mm or less. To achieve the object, in supplying 80 to 55% by weight of resin and 20 to 45% by weight of the fibrous filler with a weight average fiber length of 1 mm or more to an extruder to produce a resin composition pellet in which a weight average fiber length of a fibrous filler is 180 to 360 μm, a part of an amount (x) of the resin is supplied through a main feed port of the extruder, and the fibrous filler and a remaining amount (1−x) of the resin are supplied through a side-feed port so that x/(1−x) becomes 50/50 to 10/90% by weight.

    摘要翻译: 本发明的目的是通过使用普通的挤出机经济地生产树脂降解降解的树脂组合物颗粒,所述树脂组合物颗粒填充有所需的填充量的均匀复合的纤维填料并具有所需的重量 平均纤维长度,特别是为了制造用于平面插座销的插座的树脂组合物颗粒,其中半导体器件的晶格面积的间距间隔为2.0mm或更小,晶格面积的厚度为0.5mm 以下,插座的高度为5.0mm以下。 为了达到上述目的,向挤出机中供给80〜55重量%的树脂和20〜45重量%的重均纤维长度为1mm以上的纤维填料,制成树脂组合物颗粒,其中重量 纤维填料的平均纤维长度为180〜360μm,树脂的量(x)的一部分通过挤出机的主供料口供给,纤维填料的剩余量(1-x) 树脂通过侧进料口供给,使得x /(1-x)成为50/50至10/90重量%。

    Method for manufacturing liquid crystalline resin composition of reduced density
    3.
    发明授权
    Method for manufacturing liquid crystalline resin composition of reduced density 有权
    制造密度降低的液晶树脂组合物的方法

    公开(公告)号:US07897083B2

    公开(公告)日:2011-03-01

    申请号:US11177284

    申请日:2005-07-11

    IPC分类号: B29C47/38

    摘要: The object is to provide a method for manufacturing liquid crystalline resin composition having a hollow filler and a fibrous filler using a common melting-kneading extruder to maintain well-balanced relation between the residual percentages of hollow filler and the fiber length, which balance could not be attained in the prior art. A liquid crystalline resin composition having 5 to 30% by weight of hollow filler and 5 to 30% by weight of fibrous filler is manufactured using a melting-kneading extruder provided with a screw. (1) The liquid crystalline resin is fed from a main feed port located at upstream side in the extruding direction, while a hollow filler and a fibrous filler are fed from a side feed port located at downstream side in the extruding direction. The manufacture is conducted under the specific conditions between (2) L1 as the ratio L/D in which D is the screw diameter and L is the distance between the position of the side feed port and the position where the internal pressure of the extruder reaches 0.1 MPa; (3) L2 as the ratio L/D in which D is the screw diameter and L is the length of maintaining the internal pressure of the extruder at or above 0.1 MPa after feeding the hollow filler and the fibrous filler; and(4) La as the ratio L/D in which D is the screw diameter and L is the length of the resin plasticizing zone.

    摘要翻译: 本发明的目的是提供一种使用普通熔融捏合挤出机制造具有中空填料和纤维填料的液晶树脂组合物的方法,以保持中空填料的剩余百分比与纤维长度之间的平衡关系,其平衡不能 在现有技术中可以实现。 使用具有螺杆的熔融捏合挤出机制造具有5至30重量%的中空填料和5至30重量%的纤维填料的液晶树脂组合物。 (1)从位于挤压方向上游侧的主供给口供给液晶树脂,同时从位于挤出方向下游侧的侧供料口供给中空填料和纤维填料。 制造在(2)L1之间的特定条件下进行,其中D是螺杆直径的比率L / D,L是侧进料口的位置与挤出机的内部压力达到的位置之间的距离 0.1 MPa; (3)L2作为D =螺杆直径的比率L / L,L是在供给中空填料和纤维填料后保持挤出机的内压等于或大于0.1MPa的长度; 和(4)La的比例L / D,其中D是螺杆直径,L是树脂增塑区的长度。

    Method for manufacturing liquid crystalline resin composition
    4.
    发明申请
    Method for manufacturing liquid crystalline resin composition 有权
    液晶树脂组合物的制造方法

    公开(公告)号:US20060022378A1

    公开(公告)日:2006-02-02

    申请号:US11177284

    申请日:2005-07-11

    IPC分类号: B29C47/00 B29C47/38

    摘要: The object is to provide a method for manufacturing liquid crystalline resin composition having a hollow filler and a fibrous filler using a common melting-kneading extruder to maintain well-balanced relation between the residual percentages of hollow filler and the fiber length, which balance could not be attained in the prior art. A liquid crystalline resin composition having 5 to 30% by weight of hollow filler and 5 to 30% by weight of fibrous filler is manufactured using a melting-kneading extruder provided with a screw. (1) The liquid crystalline resin is fed from a main feed port located at upstream side in the extruding direction, while a hollow filler and a fibrous filler are fed from a side feed port located at downstream side in the extruding direction. The manufacture is conducted under the specific conditions between (2) L1 as the ratio L/D in which D is the screw diameter and L is the distance between the position of the side feed port and the position where the internal pressure of the extruder reaches 0.1 MPa; (3) L2 as the ratio L/D in which D is the screw diameter and L is the length of maintaining the internal pressure of the extruder at or above 0.1 MPa after feeding the hollow filler and the fibrous filler; and (4) La as the ratio L/D in which D is the screw diameter and L is the length of the resin plasticizing zone.

    摘要翻译: 本发明的目的是提供一种使用普通熔融捏合挤出机制造具有中空填料和纤维填料的液晶树脂组合物的方法,以保持中空填料的剩余百分比与纤维长度之间的平衡关系,其平衡不能 在现有技术中可以实现。 使用具有螺杆的熔融捏合挤出机制造具有5至30重量%的中空填料和5至30重量%的纤维填料的液晶树脂组合物。 (1)从位于挤压方向上游侧的主供给口供给液晶树脂,同时从位于挤出方向下游侧的侧供料口供给中空填料和纤维填料。 制造在(2)L1之间的特定条件下进行,其中D是螺杆直径的比率L / D,L是侧进料口的位置与挤出机的内部压力达到的位置之间的距离 0.1 MPa; (3)L2作为D =螺杆直径的比率L / L,L是在供给中空填料和纤维填料后保持挤出机的内压等于或大于0.1MPa的长度; 和(4)La的比例L / D,其中D是螺杆直径,L是树脂增塑区的长度。

    Search device, search method, search program, and computer-readable memory medium for recording search program
    5.
    发明授权
    Search device, search method, search program, and computer-readable memory medium for recording search program 有权
    搜索装置,搜索方法,搜索程序和用于记录搜索程序的计算机可读存储介质

    公开(公告)号:US09058328B2

    公开(公告)日:2015-06-16

    申请号:US13989933

    申请日:2012-02-24

    IPC分类号: G06F17/30

    CPC分类号: G06F17/30011 G06F17/30699

    摘要: A search server includes an extracting unit that extracts a search target matching a search condition based on profile data, and a transmitting unit that transmits the search target to a user terminal. The search condition includes a first frequency of appearance for each of one or more specified topics specified by a user in a first specified period and a second frequency of appearance for each of the specified topics in a second specified period being later than the first specified period. The extracting unit extracts the search target where the frequency of appearance for each of the specified topics in a first search target period and a second search target period being later than the first search target period are identical or similar to the first frequency of appearance and the second frequency of appearance, respectively.

    摘要翻译: 搜索服务器包括:提取单元,其基于简档数据提取与搜索条件匹配的搜索目标;以及发送单元,其将搜索目标发送到用户终端。 搜索条件包括在第一指定时段内由用户指定的一个或多个指定主题中的每一个的第一出现频率和在第二指定周期中的每个指定主题的第二频率出现在第一指定周期之后 。 提取单元提取搜索目标,其中在第一搜索目标周期中的每个指定主题的出现频率和比第一搜索目标周期晚的第二搜索目标周期与第一出现频率相同或相似, 分别是外观的第二频率。

    Encoding system and encoding apparatus
    7.
    发明授权
    Encoding system and encoding apparatus 有权
    编码系统和编码装置

    公开(公告)号:US08660151B2

    公开(公告)日:2014-02-25

    申请号:US13497898

    申请日:2010-09-22

    IPC分类号: H04J3/06 H04J3/02

    摘要: An encoding apparatus 2 includes: an encoding unit 21 that encodes and multiplexes a video signal V2, an audio signal A2 and a data signal D2 to be given to the encoding apparatus 2; a timer 22 that outputs time information T2; a timer adjusting unit 23 that adjusts the timer 22 so that the time information T2 and time information T1 within a multiplexed stream S1 outputted from an encoding apparatus 1 are synchronized with each other; and a multiplexing unit 24 that multiplexes the multiplexed stream S1, an encoded stream S21 outputted from the encoding unit 21 and the time information T2, and outputs the resultant multiplexed stream and information as output of the encoding apparatus 2. Third and subsequent encoding apparatus are configured to have the same configuration as that of the encoding apparatus 2.

    摘要翻译: 编码装置2包括:编码单元21,对编码装置2给出的视频信号V2,音频信号A2和数据信号D2进行编码和复用; 输出时间信息T2的定时器22; 定时器调整单元23,其调整定时器22,使得从编码装置1输出的复用流S1内的时间信息T2和时间信息T1彼此同步; 以及复用单元24,多路复用流S1,从编码单元21输出的编码流S21和时间信息T2,并输出所生成的多路复用流和信息作为编码装置2的输出。第三和随后的编码装置 被配置为具有与编码装置2相同的配置。

    Solid-state imaging device and electronic equipment
    8.
    发明授权
    Solid-state imaging device and electronic equipment 有权
    固态成像装置和电子设备

    公开(公告)号:US08492864B2

    公开(公告)日:2013-07-23

    申请号:US13252618

    申请日:2011-10-04

    申请人: Kazufumi Watanabe

    发明人: Kazufumi Watanabe

    IPC分类号: H01L27/146

    摘要: A solid-state imaging device includes: a substrate; a wiring layer formed on a front side of the substrate in which pixels are formed; a surface electrode pad section formed in the wiring layer; a light-shielding film formed on a rear side of the substrate; a pad section base layer formed in the same layer as the light-shielding film; an on-chip lens layer formed over the light-shielding film and the pad section base layer in a side opposite from the substrate side; a back electrode pad section formed above the on-chip lens layer; a through-hole formed to penetrate the on-chip lens layer, the pad section base layer, and the substrate so as to expose the surface electrode pad section; and a through-electrode layer which is formed in the through-hole and connects the surface electrode pad section and the back electrode pad section.

    摘要翻译: 固态成像装置包括:基板; 形成在其上形成有像素的基板的前侧的布线层; 形成在所述布线层中的表面电极焊盘部; 形成在所述基板的后侧的遮光膜; 形成在与所述遮光膜相同的层中的焊盘部分基底层; 在与所述基板侧相反的一侧的所述遮光膜和所述焊盘部分基底层上形成的片上透镜层; 形成在片上透镜层之上的背面电极焊盘部; 形成为贯穿片上透镜层的通孔,焊盘部分基底层和基板,以露出表面电极焊盘部分; 以及形成在所述通孔中并连接所述表面电极焊盘部和所述背面电极焊盘部的贯通电极层。

    Thermoplastic Resin Composition, and Liquid Crystal Display Component Thereof or Information Recording Media Component Thereof
    9.
    发明申请
    Thermoplastic Resin Composition, and Liquid Crystal Display Component Thereof or Information Recording Media Component Thereof 审中-公开
    热塑性树脂组合物及其液晶显示元件或信息记录媒体组件

    公开(公告)号:US20090027586A1

    公开(公告)日:2009-01-29

    申请号:US12223655

    申请日:2007-02-08

    IPC分类号: G02F1/1333 C08L69/00

    摘要: The present invention provides a thermoplastic resin composition having high flowability, has high dimensional stability like being free from deformation after molding, shows excellent rigidity, impact resistance, and heat resistance, and is suitable for thin-wall molded article. Specifically the thermoplastic resin composition is composed of: 100 parts by weight of a resin composition structured by (A) 91 to 99% by weight of a thermoplastic resin having a specified melt viscosity and (B) 1 to 9% by weight of a liquid crystalline polymer; and 0.001 to 2 parts by weight of (C) a specified phosphorus oxo acid monoester or diester, wherein the (B) liquid crystalline polymer is dispersed as particles, and the ratio of the melt viscosity of (A) component to (B) component is within a specified range. The present invention also provides a liquid crystal display component and an information recording media component.

    摘要翻译: 本发明提供流动性高的热塑性树脂组合物,具有成型后无变形的尺寸稳定性,显示优异的刚性,耐冲击性和耐热性,适用于薄壁成型体。 具体而言,热塑性树脂组合物由以下组成:100重量份由(A)91〜99重量%的具有规定的熔融粘度的热塑性树脂构成的树脂组合物和(B)1〜9重量%的液体 结晶聚合物; 和(C)特定的含磷酸单酯或二酯的0.001至2重量份,其中(B)液晶聚合物作为颗粒分散,并且(A)组分与(B)组分的熔体粘度之比 在指定的范围内。 本发明还提供一种液晶显示部件和信息记录介质部件。