摘要:
An device for Raman spectroscopy such as surface enhanced Raman spectroscopy (SERS) is disclosed herein. Various embodiments may be utilized to prepare a SERS substrate using several deposition techniques such as pulsed laser deposition. Some embodiments optimize coverage, volume, or elements of SERS active metals. The method is a single step inexpensive method for preparing a SERS active substrate. In some embodiments a coating layer underneath the SERS active metals is utilized for additional enhancements.
摘要:
In the present invention, a method of producing stable bare colloidal gold nanoparticles is disclosed. The nanoparticles can subsequently be subjected to partial or full surface modification. The method comprises preparation of colloidal gold nanoparticles in a liquid by employing a top-down nanofabrication method using bulk gold as a source material. The surface modification of these nanoparticles is carried out by adding one or multiple types of ligands each containing functional groups which exhibit affinity for gold nanoparticle surfaces to produce the conjugates. Because of the high efficiency and excellent stability of the nanoparticles produced by this method, the fabricated gold nanoparticle conjugates can have surface coverage with functional ligands which can be tuned to be any percent value between 0 and 100%.
摘要:
In the present invention, a method of producing stable bare colloidal gold nanoparticles is disclosed. The nanoparticles can subsequently be subjected to partial or full surface modification. The method comprises preparation of colloidal gold nanoparticles in a liquid by employing a top-down nanofabrication method using bulk gold as a source material. The surface modification of these nanoparticles is carried out by adding one or multiple types of ligands each containing functional groups which exhibit affinity for gold nanoparticle surfaces to produce the conjugates. Because of the high efficiency and excellent stability of the nanoparticles produced by this method, the fabricated gold nanoparticle conjugates can have surface coverage with functional ligands which can be tuned to be any percent value between 0 and 100%.
摘要:
A method of forming patterns on transparent substrates using a pulsed laser is disclosed. Various embodiments include an ultrashort pulsed laser, a substrate that is transparent to the laser wavelength, and a target plate. The laser beam is guided through the transparent substrate and focused on the target surface. The target material is ablated by the laser and is deposited on the opposite substrate surface. A pattern, for example a gray scale image, is formed by scanning the laser beam relative to the target. Variations of the laser beam scan speed and scan line density control the material deposition and change the optical properties of the deposited patterns, creating a visual effect of gray scale. In some embodiments patterns may be formed on a portion of a microelectronic device during a fabrication process. In some embodiments high repetition rate picoseconds and nanosecond sources are configured to produce the patterns.
摘要:
Various embodiments include a method of producing chemically pure and stably dispersed metal and metal-alloy nanoparticle colloids with ultrafast pulsed laser ablation. A method comprises irradiating a metal or metal alloy target submerged in a liquid with ultrashort laser pulses at a high repetition rate, cooling a portion of the liquid that includes an irradiated region, and collecting nanoparticles produced with the laser irradiation and liquid cooling. The method may be implemented with a high repetition rate ultrafast pulsed laser source, an optical system for focusing and moving the pulsed laser beams, a metal or metal alloy target submerged in a liquid, and a liquid circulating system to cool the laser focal volume and collect the nanoparticle products. By controlling various laser parameters, and with optional liquid flow movement, the method provides stable colloids of dispersed metal and metal-alloy nanoparticles. In various embodiments additional stabilizing chemical agents are not required.
摘要:
Various embodiments include a method of producing chemically pure and stably dispersed metal and metal-alloy nanoparticle colloids with ultrafast pulsed laser ablation. A method comprises irradiating a metal or metal alloy target submerged in a liquid with ultrashort laser pulses at a high repetition rate, cooling a portion of the liquid that includes an irradiated region, and collecting nanoparticles produced with the laser irradiation and liquid cooling. The method may be implemented with a high repetition rate ultrafast pulsed laser source, an optical system for focusing and moving the pulsed laser beams, a metal or metal alloy target submerged in a liquid, and a liquid circulating system to cool the laser focal volume and collect the nanoparticle products. By controlling various laser parameters, and with optional liquid flow movement, the method provides stable colloids of dispersed metal and metal-alloy nanoparticles. In various embodiments additional stabilizing chemical agents are not required.
摘要:
A method of pulsed laser deposition (PLD) capable of continuously tuning formed-film morphology from that of a nanoparticle aggregate to a smooth thin film free of particles and droplets. The materials that can be synthesized using various embodiments of the invention include, but are not limited to, metals, alloys, metal oxides, and semiconductors. In various embodiments a ‘burst’ mode of ultrashort pulsed laser ablation and deposition is provided. Tuning of the film morphology is achieved by controlling the burst-mode parameters such as the number of pulses and the time-spacing between the pulses within each burst, the burst repetition rate, and the laser fluence. The system includes an ultrashort pulsed laser, an optical system for delivering a focused onto the target surface with an appropriate energy density, and a vacuum chamber in which the target and the substrate are installed and background gases and their pressures are appropriately adjusted.
摘要:
A method for generating nanoparticles in a liquid comprises generating groups of ultrafast laser pulses, each pulse in a group having a pulse duration of from 10 femtoseconds to 200 picoseconds, and each group containing a plurality of pulses with a pulse separation of 1 to 100 nanoseconds and directing the groups of pulses at a target material in a liquid to ablate it. The multiple pulse group ablation produces nanoparticles with a reduced average size, a narrow size distribution, and improved production efficiency compared to prior pulsed ablation systems.
摘要:
A method of ultrashort pulsed laser deposition (PLD) capable of continuously tuning formed-film morphology from that of a nanoparticle aggregate to a smooth thin film completely free of particles and droplets. The materials that can be synthesized using various embodiments of the invention include, but are not limited to, metals, alloys, metal oxides, and semiconductors. A ‘burst’ mode of ultrashort pulsed laser ablation and deposition is provided, where each ‘burst’ contains a train of laser pulses. Tuning of the film morphology is achieved by controlling the burst-mode parameters such as the number of pulses and the time-spacing between the pulses within each burst, the burst repetition rate, and the laser fluence. The system includes an ultrashort pulsed laser, an optical setup for delivering the laser beam such that the beam is focused onto the target surface with an appropriate average energy density (fluence), and a vacuum chamber in which the target and the substrate are installed and background gases and their pressures are appropriately adjusted.
摘要:
A method of forming patterns on transparent substrates using a pulsed laser is disclosed. Various embodiments include an ultrashort pulsed laser, a substrate that is transparent to the laser wavelength, and a target plate. The laser beam is guided through the transparent substrate and focused on the target surface. The target material is ablated by the laser and is deposited on the opposite substrate surface. A pattern, for example a gray scale image, is formed by scanning the laser beam relative to the target. Variations of the laser beam scan speed and scan line density control the material deposition and change the optical properties of the deposited patterns, creating a visual effect of gray scale. In some embodiments patterns may be formed on a portion of a microelectronic device during a fabrication process. In some embodiments high repetition rate picoseconds and nanosecond sources are configured to produce the patterns.