Occupant restraint device
    1.
    发明授权
    Occupant restraint device 失效
    乘员约束装置

    公开(公告)号:US06293581B1

    公开(公告)日:2001-09-25

    申请号:US09541689

    申请日:2000-04-03

    IPC分类号: B60R2122

    摘要: An air bag of an inflatable curtain device includes a first cell group and a second cell group whose internal spaces are independent from each other. A high-pressure gas discharged from opposite ends of a common inflater disposed between both of the first and second cell groups and is supplied to a high-pressure gas supply port in the first cell group and a high-pressure gas supply port in the second cell group. The first and second cell groups can be expanded simultaneously by the common inflater, whereby the entire air bag can be deployed promptly, but also even when one of the first and second cell groups and is damaged, the deployment of the other cell group can be achieved without hindrance.

    摘要翻译: 充气帘装置的气囊包括第一电池组和其内部空间彼此独立的第二电池组。 从设置在第一和第二电池组之间的公共充气器的相对端部排出的高压气体供给到第一电池组中的高压气体供给口和第二电池组中的高压气体供给口 细胞组。 第一和第二细胞群可以通过共同的充气器同时扩张,从而可以迅速地部署整个气囊,但是即使当第一和第二细胞组中的一个被损坏时,另一个细胞群的展开可以是 实现无障碍

    Method for producing quartz glass crucible
    2.
    发明授权
    Method for producing quartz glass crucible 有权
    生产石英玻璃坩埚的方法

    公开(公告)号:US08286447B2

    公开(公告)日:2012-10-16

    申请号:US12169838

    申请日:2008-07-09

    IPC分类号: C03B19/01 C03B19/06

    摘要: A method of producing a quartz glass crucible by arc melting a quartz powder molded product loaded on the inner side of a mold while performing vacuum suction, includes initiating the melting of quartz powder from the rim edge of a quartz powder molded product, subsequently lowering the arc electrode or raising the mold to heat and melt the sections on the downside of the rim edge. The method is preferably carried out such that the inner surface of the crucible is sealed within a time corresponding to 10% of the total arc time starting from the initiation of arc melting, and the seal thickness is 3 mm or less. The quartz glass crucible thus produced is useful for the pulling up of silicon single crystals and has a uniform glass layer with fewer internal bubbles.

    摘要翻译: 通过电弧熔融装载在模具内侧的石英粉末成形体同时进行真空抽吸来制造石英玻璃坩埚的方法包括从石英粉末成型品的边缘开始熔融石英粉末,随后将 电弧电极或提升模具以加热和熔化边缘边缘的下侧的部分。 该方法优选进行,使得坩埚的内表面在从电弧熔化开始起的总电弧时间的10%的时间内密封,并且密封厚度为3mm以下。 由此制造的石英玻璃坩埚可用于提升硅单晶,并且具有均匀的具有较少内部气泡的玻璃层。

    Silica glass crucible and method for pulling up silicon single crystal using the same
    3.
    发明授权
    Silica glass crucible and method for pulling up silicon single crystal using the same 有权
    二氧化硅玻璃坩埚和使用其同时提升硅单晶的方法

    公开(公告)号:US08163083B2

    公开(公告)日:2012-04-24

    申请号:US12169828

    申请日:2008-07-09

    摘要: A silica glass crucible causing fewer pinholes in silicon single crystals is provided by a method of preventing pinholes by performing the pulling up of a silicon single crystal while restraining the dissolution rate of the crucible inner surface to 20 μm/hr or less, using a silica glass crucible for the pulling up of silicon single crystals, wherein the area of crystalline silica formed by crystallization of amorphous silica is restricted to 10% or less of the crucible inner surface area, or the density of pits formed from open bubbles on the crucible inner surface is restricted to 0.01 to 0.2 counts/mm2.

    摘要翻译: 通过使用二氧化硅将硅坩埚内表面的溶解速度抑制为20μm/小时以下,通过进行硅单晶的拉拔来防止针孔的方法来提供硅单晶中的针孔少的石英玻璃坩埚 用于提取硅单晶的玻璃坩埚,其中由无定形二氧化硅结晶形成的结晶二氧化硅的面积限制在坩埚内表面积的10%以下,或坩埚内部由开放气泡形成的凹坑的密度 表面限制在0.01〜0.2个/ mm2。

    SILICA GLASS CRUCIBLE, METHOD OF MANUFACTURING THE SAME AND PULLING METHOD
    4.
    发明申请
    SILICA GLASS CRUCIBLE, METHOD OF MANUFACTURING THE SAME AND PULLING METHOD 审中-公开
    二氧化硅玻璃巧克力,制造方法和拉伸方法

    公开(公告)号:US20100319608A1

    公开(公告)日:2010-12-23

    申请号:US12303139

    申请日:2008-09-29

    申请人: Minoru Kanda

    发明人: Minoru Kanda

    IPC分类号: C30B15/10 C03C10/14 C30B15/00

    摘要: A silica glass crucible including an outer surface layer formed of a bubble-containing silica glass layer and an inner surface layer formed of a silica glass layer whose bubbles are invisible to the naked eye, so as to sufficiently disperse heat from the external radiation thereby preventing temperature irregularity in the silicon melt, and at the same time, exhibit excellent heat conductivity thereby giving a uniformly heated state over a wide range in the entire crucible without taking a long time for increasing the temperature to form a silicon melt, wherein an intermediate layer is interposed between the outer surface layer and the inner surface layer while in the intermediate layer, a bubble-containing silica glass layer (bubble-containing layer) including bubbles with a diameter of 100 μm or smaller by 0.1% or more in the volumetric bubble content and a silica glass layer (transparent glass layer) including the bubbles by 0.05% or less in the volumetric bubble content are laminated.

    摘要翻译: 一种二氧化硅玻璃坩埚,其包括由含气泡的石英玻璃层形成的外表面层和由石墨玻璃层形成的内表面层,所述内表面层的气泡对肉眼不可见,从而充分地分散来自外部辐射的热量,从而防止 硅熔体中的温度不均匀性,并且同时显示出优异的导热性,从而在整个坩埚中在宽范围内均匀地加热状态,而不需要较长时间来提高温度以形成硅熔体,其中中间层 介于外表面层和内表面层之间,而在中间层中,在体积气泡中包含直径为100μm或更小直径为0.1%或更大的气泡的含气泡石英玻璃层(含气泡层) 含量和包含气泡的二氧化硅玻璃层(透明玻璃层)的体积气泡含量为0.05%以下 ted。

    METHOD AND APPARATUS FOR MANUFACTURING VITREOUS SILICA CRUCIBLE
    5.
    发明申请
    METHOD AND APPARATUS FOR MANUFACTURING VITREOUS SILICA CRUCIBLE 有权
    用于制造维生素二氧化硅可溶性的方法和装置

    公开(公告)号:US20100229599A1

    公开(公告)日:2010-09-16

    申请号:US12303134

    申请日:2008-07-25

    IPC分类号: C03C1/00

    CPC分类号: C03B19/095 C30B15/10

    摘要: In order to provide method and apparatus for manufacturing a vitreous silica crucible with little mixing of foreign matter and stable arc during arc melting, the method and apparatus for manufacturing a vitreous silica crucible have a device which blows off air from the side of arc electrodes toward a melting space of a mold, and air discharge ports which discharge the air within the heating furnace, and perform forced supply of air into the melting space during melting to make the atmospheric pressure of the melting space higher than the surroundings, and preferably, form an air pressure difference of 100 Pa or more between the melting space and the surroundings, thereby performing melting.

    摘要翻译: 为了提供在电弧熔化期间少量异物混合和稳定电弧的制造石英玻璃坩埚的方法和装置,用于制造石英玻璃坩埚的方法和装置具有从电弧电极的侧面吹出空气的装置 模具的熔化空间和排出加热炉内的空气的排气口,并且在熔融期间强制地将空气送入熔融空间,使熔融空间的大气压力高于周围环境,优选形成 熔融空间与周围环境之间的空气压差为100Pa以上,进行熔融。

    Air bag device for passenger seat
    7.
    发明授权
    Air bag device for passenger seat 失效
    乘客座椅气囊装置

    公开(公告)号:US5429385A

    公开(公告)日:1995-07-04

    申请号:US115007

    申请日:1993-09-01

    摘要: An air bag device for use in front of a passenger seat of an automobile includes a casing disposed in the instrument panel of the automobile, a folded air bag housed in the casing and inflatable through the upper opening upon impact, and a lid openably joined to the casing in covering relationship to the upper opening. An air bag restraint guide or protective cloth is joined to the casing for preventing the air bag from directly contacting an edge of the upper opening when the air bag is inflated through the upper opening.

    摘要翻译: 用于汽车乘客座椅前方的气囊装置包括设置在汽车仪表板中的壳体,容纳在壳体中的折叠气囊,并且在撞击时可通过上开口充气,并且盖可开启地连接到 套管覆盖与上开口的关系。 气囊保护引导件或防护布被连接到壳体,用于当气囊通过上部开口膨胀时,防止气囊与上部开口的边缘直接接触。

    VITREOUS SILICA CRUCIBLE FOR PULLING SILICON SINGLE CRYSTAL AND METHOD OF MANUFACTURING THE SAME
    10.
    发明申请
    VITREOUS SILICA CRUCIBLE FOR PULLING SILICON SINGLE CRYSTAL AND METHOD OF MANUFACTURING THE SAME 有权
    用于拉丝硅单晶的耐火二氧化硅巧克力及其制造方法

    公开(公告)号:US20120160159A1

    公开(公告)日:2012-06-28

    申请号:US13394284

    申请日:2010-08-10

    IPC分类号: C30B15/10 C03B20/00

    摘要: The present invention provides a vitreous silica crucible which can suppress the sidewall lowering of the crucible under high temperature during pulling a silicon single crystal, and a method of manufacturing such a vitreous silica crucible. The vitreous silica crucible 10 includes an opaque vitreous silica layer 11 provided on the outer surface side of the crucible and containing numerous bubbles, and a transparent vitreous silica layer 12 provided on the inner surface side. The opaque vitreous silica layer 11 includes a first opaque vitreous silica portion 11a provided on the crucible upper portion, and a second opaque vitreous silica portion 11b provided on the crucible lower portion. The specific gravity of the second opaque vitreous silica portion 11b is 1.7 to 2.1, and the specific gravity of the first opaque vitreous silica portion 11a is 1.4 to 1.8, and smaller than that of the second opaque vitreous silica portion. The particle size distribution of the material silica powder for the first opaque vitreous silica portion 11a is wider than that of the second opaque vitreous silica portion 11b, and the material silica powder for the first opaque vitreous silica portion 11a includes more fine powder than that for the second opaque vitreous silica portion 11b.

    摘要翻译: 本发明提供一种可以在拉拔硅单晶时抑制坩埚在高温下的侧壁降低的石英玻璃坩埚,以及制造这种石英玻璃坩埚的方法。 玻璃状石英玻璃坩埚10包括设置在坩埚的外表面侧并且含有大量气泡的不透明玻璃状石英层11和设置在内表面侧的透明氧化硅玻璃层12。 不透明玻璃状石英层11包括设置在坩埚上部的第一不透明玻璃状石英部分11a和设置在坩埚下部的第二不透明玻璃状石英部分11b。 第二不透玻璃状二氧化硅部11b的比重为1.7〜2.1,第一不透明玻璃状石英部11a的比重为1.4〜1.8,小于第二不透明玻璃状二氧化硅部的比重。 用于第一不透明玻璃状石英部分11a的材料二氧化硅粉末的粒度分布比第二不透明玻璃状二氧化硅部分11b的粒度分布宽,并且用于第一不透明玻璃状石英部分11a的材料二氧化硅粉末包含比 第二不透明玻璃状石英部分11b。