Method for rolling and/or heat treating a metal strip

    公开(公告)号:US11319611B2

    公开(公告)日:2022-05-03

    申请号:US16084595

    申请日:2017-03-03

    Applicant: SMS Group GmbH

    Abstract: The invention relates to a method for rolling a metal product (1), wherein the metal product is subjected to a rolling operation at a first station (2), which rolling operation is controlled by a control device (3), wherein the product (1) is subject to a measurement at a second station (4), wherein the product (1) is subjected to a further processing operation at a third station (6), and wherein the product (1) is in a specified quality at a fourth station (7). In order to increase the quality of the produced strip, the invention provides that the method has the following steps: a) measuring the value of a material property (IW) that the second station (4); b) feeding the value measured at the second station (4) to the control device (3), comparing the measured value with a value (SW) stored in the control device (3), and adjusting a parameter (PPI) if the measured value deviates from the stored value (SW), e) measuring a value of a quality material property (Q) at the fourth station (7); d) comparing the measured value with a stored value, and initiating a measure to influence the quality material property (Q) if the measured value deviates from the stored value beyond a permissible tolerance.

    METHOD FOR ROLLING AND/OR HEAT TREATING A METAL STRIP

    公开(公告)号:US20190071750A1

    公开(公告)日:2019-03-07

    申请号:US16084595

    申请日:2017-03-03

    Applicant: SMS Group GmbH

    Abstract: The invention relates to a method for rolling a metal product (1), wherein the metal product is subjected to a rolling operation at a first station (2), which rolling operation is controlled by a control device (3), wherein the product (1) is subject to a measurement at a second station (4), wherein the product (1) is subjected to a further processing operation at a third station (6), and wherein the product (1) is in a specified quality at a fourth station (7). In order to increase the quality of the produced strip, the invention provides that the method has the following steps: a) measuring the value of a material property (IW) that the second station (4); b) feeding the value measured at the second station (4) to the control device (3), comparing the measured value with a value (SW) stored in the control device (3), and adjusting a parameter (PPI) if the measured value deviates from the stored value (SW), e) measuring a value of a quality material property (Q) at the fourth station (7); d) comparing the measured value with a stored value, and initiating a measure to influence the quality material property (Q) if the measured value deviates from the stored value beyond a permissible tolerance

    Process for producing grain-oriented electrical steel strip

    公开(公告)号:US11239012B2

    公开(公告)日:2022-02-01

    申请号:US14638338

    申请日:2015-03-04

    Applicant: SMS Group GmbH

    Abstract: A process for producing grain-oriented electrical steel strip by means of thin slab continuous casting and which includes continuously casting the smelt by thin slab continuous casting, subjecting the thin slabs to homogenization annealing at a maximum temperature of 1250° C. and heating to a temperature between 1350° C. and 1380° C., and continuously hot rolling the thin slabs to form a hot-rolled strip, with cooling and reeling the hot-rolled strip to form a coil and cold rolling the hot-rolled strip to a nominal thickness, with subjecting the cold-rolled strip to recrystallization, decarburization and nitridation annealing, which includes a decarburization annealing phase and a subsequent nitridation annealing phase, with an intermediate reduction annealing phase being interposed between the decarburization annealing phase and the nitridation annealing phase, whereby a cold-rolled strip is obtained, which primary recrystallized grains have a circle equivalent mean size (diameter) between 22 μm and 25 μm.