摘要:
A compound for metal powder injection molding includes secondary particles in which first metal particles are bound to one another, and a matrix region including a binder and second metal particles whose constituent material is different from that of the first metal particles. It is preferred that in the secondary particles, the first metal particles are bound to one another through the binder. It is also preferred that the average particle diameter of the second metal particles is smaller than that of the first metal particles.
摘要:
A titanium sintered body is composed of a material containing titanium, and has an oxygen content of 2500 ppm by mass or more and 5500 ppm by mass or less and a surface Vickers hardness of 250 or more and 500 or less. It is preferred that an α-phase and a β-phase are contained as crystal structures, and an area ratio occupied by the α-phase in a cross section is 70% or more and 99.8% or less. It is also preferred that in an X-ray diffraction spectrum obtained by X-ray diffractometry, the value of a peak reflection intensity by the plane orientation (110) of the β-phase is 5% or more and 60% or less of the value of a peak reflection intensity by the plane orientation (100) of the α-phase. It is also preferred that particles composed mainly of titanium oxide are included.
摘要:
A titanium sintered body contains an α-phase and a β-phase as crystal structures, wherein the average grain size of the α-phase in a cross section is 3 μm or more and 30 μm or less, and an area ratio occupied by the α-phase in a cross section is 70% or more and 99.8% or less. In the titanium sintered body, it is preferred that the average aspect ratio of the α-phase in a cross section is 1 or more and 3 or less. It is also preferred that the titanium sintered body contains titanium as a main component, and also contains an α-phase stabilizing element and a β-phase stabilizing element.
摘要:
A metal powder contains Fe as a principal component, Cr in a proportion of 10 to 30 mass %, C in a proportion of 0.15 to 1.5 mass %, Si in a proportion of 0.3 to 1 mass %, and Mn and Ni in a total proportion of 0.05 to 1.6 mass %, wherein when Ti, V, Y, Zr, Nb, Hf, and Ta is defined as a first element, and one element selected from the group and having a larger group number in the periodic table than that of the first element or having the same group number in the periodic table as that of the first element and a larger period number than that of the first element is defined as a second element, the first element is contained in a proportion of 0.01 to 0.5 mass %, and the second element is contained in a proportion of 0.01 to 0.5 mass %.
摘要:
A blank material to be cut for dentistry includes: Co as a main component; Cr at a ratio equal to or higher than 26 mass % and equal to or less than 35 mass %; Mo at a ratio equal to or higher than 5 mass % and equal to or less than 12 mass %; Si at a ratio equal to or higher than 0.3 mass % and equal to or less than 2.0 mass %; and N at a ratio equal to or higher than 0.09 mass % and equal to or less than 0.5 mass %. The blank material is formed of a sintered body of a metal powder.
摘要:
A method for producing a composition for injection molding which contains an inorganic powder composed of at least one of a metal material and a ceramic material and a binder containing a polyacetal-based resin and a glycidyl group-containing polymer. The method includes: cryogenically grinding a first resin containing the polyacetal-based resin as a main component; cryogenically grinding a second resin containing the glycidyl group-containing polymer as a main component; mixing a powder obtained by grinding the first resin, a powder obtained by grinding the second resin, and the inorganic powder, thereby obtaining a mixed powder; and kneading the mixed powder.
摘要:
A metal powder for powder metallurgy contains Co as a principal component, Cr in a proportion of 10 to 25 mass %, Ni in a proportion of 5 to 40 mass %, at least one of Mo and W in a proportion of 2 to 20 mass % in total, Si in a proportion of 0.3 to 1.5 mass %, and C in a proportion of 0.05 to 0.8 mass %, wherein one element selected from the group consisting of Ti, V, Y, Zr, Nb, Hf, and Ta is defined as a first element, that is contained in a proportion of 0.01 to 0.5 mass %.
摘要:
A metal powder for powder metallurgy according to the invention contains Fe as a principal component, Cr in a proportion of 6 mass % or more and 32 mass % or less, Si in a proportion of 0.3 mass % or more and 3 mass % or less, and C in a proportion of 0.005 mass % or more and 1.4 mass % or less, wherein when one element selected from the group consisting of Ti, V, Y, Zr, Nb, Hf, and Ta is defined as a first element, and one element selected from the group and having a larger group number in the periodic table than that of the first element or having the same group number in the periodic table as that of the first element and a larger period number than that of the first element is defined as a second element, the first element is contained in a proportion of 0.01 mass % or more and 2 mass % or less, and the second element is contained in a proportion of 0.01 mass % or more and 2 mass % or less.
摘要:
A package base includes a package base body and a bonding metal layer provided in a frame shape or a ring shape in plan view on the package base body, wherein the bonding metal layer contains a Ti—Ag—Cu-containing alloy and a metal belonging to Group 6 in the periodic table.
摘要:
A composition for injection molding includes: an inorganic powder composed of at least one of a metal material and a ceramic material; and a binder containing a polyacetal-based resin and an ethylene-glycidyl methacrylate-based copolymer. In the composition, the ethylene-glycidyl methacrylate-based copolymer is contained in an amount of 1% by mass or more and 30% by mass or less with respect to the amount of the polyacetal-based resin.