High-pressure tank and method for fabricating the same
    2.
    发明授权
    High-pressure tank and method for fabricating the same 失效
    高压罐及其制造方法

    公开(公告)号:US06908006B2

    公开(公告)日:2005-06-21

    申请号:US10307495

    申请日:2002-12-02

    IPC分类号: B23P11/02 F17C5/00 F17C1/02

    摘要: An annular fitting recess is formed circumferentially in the exterior of a tank body in the vicinity of the boundary between a dome section and a cylindrical gas discharge section of the tank body. A cylindrical reinforcing collar is fitted onto the cylindrical gas discharge section of the tank body to fit an annular boss of the reinforcing collar in the fitting recess of the tank body and then engaged integrally on the exterior of the tank body between the cylindrical gas discharge section and the dome section by shrinkage. This provides easily and inexpensively a high-pressure tank capable of withstanding high pressures of 35 to 75 MPa while keeping its lightness in weight.

    摘要翻译: 在罐体的外部附近,在圆筒部分和罐体的圆柱形气体排出部分之间的边界附近形成环形装配凹部。 圆柱形加强套环安装在罐体的圆柱形气体排放部分上,以将加强套环的环形凸起装配在罐体的装配凹槽中,然后一体地接合在罐体的外部在圆柱形气体排出部分 和圆顶部分通过收缩。 这提供了容易且廉价的能够承受35至75MPa的高压的高压罐,同时保持其重量轻。

    Method for fabricating fuser roller
    4.
    发明授权
    Method for fabricating fuser roller 有权
    定影辊的制造方法

    公开(公告)号:US06729170B1

    公开(公告)日:2004-05-04

    申请号:US10308222

    申请日:2002-12-03

    IPC分类号: B21B2706

    摘要: A fuser roller is obtained by heating a blank over predetermined regions starting from both the opening ends, and then necking the heated regions of the blank by moving a forming roller with rotation on the heated regions through the external pressing of the forming roller against the heated regions of the blank being rotated on its axis to draw form sidewalls integrally at both ends of a cylindrical body of the blank, respectively, and draw form cylindrical shafts integrally with the sidewalls, respectively. In this manner, the fuser roller can be fabricated using a single processing machine with respect to a single pipe member, which reduces equipment cost, further enhances production efficiency and implements low-cost production of fuser rollers.

    摘要翻译: 通过从两个开口端开始在预定区域上加热坯料,然后通过将加热区域上的成形辊通过成形辊的外部压制抵靠加热的 空白区域在其轴线上旋转以分别在坯件的圆柱体的两端处一体地形成侧壁,并分别与侧壁一体地形成圆柱形轴。 以这种方式,可以使用单个加工机器相对于单个管件来制造定影辊,这降低了设备成本,进一步提高了生产效率并实现了定影辊的低成本生产。

    Negative electrode for nonaqueous secondary battery
    7.
    发明授权
    Negative electrode for nonaqueous secondary battery 失效
    非水二次电池用负极

    公开(公告)号:US07838154B2

    公开(公告)日:2010-11-23

    申请号:US11174645

    申请日:2005-07-06

    IPC分类号: H01M4/80

    摘要: A negative electrode 10 for a nonaqueous secondary battery, has an active material layer 2 containing active material particles 2a. The active material layer 2 has a metallic material 4 deposited among the particles by electroplating. The negative electrode 10 has a large number of holes 5 open on at least one side thereof and extending through the thickness of the active material layer. The negative electrode 10 further has a pair of current collecting layers 3a and 3b adapted to be brought into contact with an electrolyte. The active material layer 2 is between the current collecting layers 3a and 3b. The holes 5 open on the negative electrode 10 preferably have an opening area ratio of 0.3% to 30%. At least one of the pair of the current collecting layers 3a and 3b preferably has a thickness of 0.3 to 10 μm.

    摘要翻译: 非水系二次电池用负极10具有含有活性物质粒子2a的活性物质层2。 活性物质层2具有通过电镀沉积在颗粒之间的金属材料4。 负极10具有在其至少一个侧面上开口并且延伸穿过活性材料层的厚度的大量孔5。 负极10还具有适于与电解液接触的一对集流层3a和3b。 活性物质层2位于集流层3a和3b之间。 在负极10上打开的孔5的开口面积比优选为0.3%〜30%。 一对集电层3a和3b中的至少一个优选具有0.3至10μm的厚度。

    NONAQUEOUS SECONDARY BATTERY AND METHOD OF PRODUCING THE SAME
    8.
    发明申请
    NONAQUEOUS SECONDARY BATTERY AND METHOD OF PRODUCING THE SAME 审中-公开
    非等级二次电池及其制造方法

    公开(公告)号:US20100136437A1

    公开(公告)日:2010-06-03

    申请号:US12593563

    申请日:2007-10-11

    IPC分类号: H01M6/16 H01M6/04 H01M6/00

    摘要: A nonaqueous secondary battery having a negative electrode containing a silicon active material and a nonaqueous solvent containing a fluorine-containing solvent. The active material layer has a fluorine content of 5 to 30 wt % based on the silicon content after at least 100 charge/discharge cycles at a rate of 50% or more of the battery's capacity. The battery is suitably produced by a method including applying a slurry containing silicon active material particles to a current collector, electroplating the resulting coating layer using a plating bath at a pH higher than 7 to coat at least part of the surface of the particles with copper, acid washing the coating layer to make a negative electrode, assembling the negative electrode together with a positive electrode, a separator, and a nonaqueous electrolyte containing a fluorine-containing solvent into a nonaqueous secondary battery, and subjecting the battery to a first charge operation at a low rate of 0.005 to 0.03 C.