摘要:
Provided is a polyester film containing a lubricant having an average particle diameter of 0.001 to 2.5 .mu.m in an amount of 0.01 to 5.0% by weight and suited for the lamination onto the surface that comes in contact with the contents of an easy-open can cap. The polyester film has a plane orientation coefficient of 0.115 to 0.140, two or more endothermic peaks in DSC curve in the range of 170 to 270.degree. C., a peak temperature of 60 to 120.degree. C. of a complex elastic modulus (E") in water and an intrinsic viscosity of 0.50 to 0.64 dl/g. Having these features, the polyester film laminated onto a metal sheet is excellent in can-capping processability and in corrosion resistance even after holding at high temperature.
摘要:
A laminate polyester film to be laminated onto metal plate and molded comprises the first layer made from copoly(ethylene-terephthalate/isophthalate) having a melting point of 205 to 250.degree. C. and a second layer made from a polyester (i) comprising ester units of an aromatic dicarboxylic acid component, an aliphatic dicarboxylic acid component and aliphatic diol components, (ii) containing a titanium compound soluble in the polyester in an amount of 30 to 200 ppm in terms of elemental titanium and (iii) having one or two melting point(s) in the range of 170 to 245.degree. C., and has the maximum peak temperature of loss elastic modulus of higher than 47.degree. C. and 85.degree. C. or lower. This laminate polyester film is suitably used for application such as metal cans for juice and other refreshing drinks that are handled in a cooled state.
摘要:
The invented film comprises a layer A composed of a copolyester A, a layer B composed of a copolyester B, and a layer C composed of copolyester C. Layer A is laminated to one side of the layer B. Layer C is laminated to the other side of Layer B. Copolyester A contains 0-15 wt % of rutile titanium oxide (average particle diameter 0.1-0.5 &mgr;m). Copolyester B contains 10-50 wt % of the rutile titanium oxide. Copolyester C contains 0-15 wt % of the rutile titanium oxide. Each of Copolyester A, B, and C has a melting point of 210-245° C. The intrinsic viscosity (&eegr;A) of the polymer part of copolyester A, the intrinsic viscosity (&eegr;B) of the polymer part of copolyester B, and the intrinsic viscosity (&eegr;C) of the polymer part of copolyester C satisfy the following relationship. 0.46≦&eegr;B≦0.66, |&eegr;A-&eegr;B|
摘要:
A biaxially oriented film to be laminated on a metal, which is a laminate film comprising (A) a first layer of a polyester comprising ethylene terephthalate as a main recurring unit; and (B) a second layer formed from a composition of a polycarbonate and polyesters, the polycarbonate and the polyesters being each contained in amounts of 20 to 50% by weight and 50 to 80% by weight based on the total thereof; the polyesters consisting essentially of a first polyester comprising ethylene terephthalate as a main recurring unit and having a terminal carboxyl group concentration of more than 5 eq./10.sup.6 g and a second polyester comprising butylene terephthalate as a main recurring unit and having a terminal carboxyl group concentration of less than 20 eq./10.sup.6 g; and the first and second polyesters being each contained in an amount of 10 to 90% by weight based on the total thereof; and in which (C) the plane orientation coefficients of the first layer and second layer are both in the range of 0.05 to 0.10.
摘要:
A film to be laminated onto a metal plate and molded, which includes a first copolyester including ethylene-2,6-naphthalene dicarboxylate as a main recurring unit or a blend of the first copolyester and a second copolyester including terephthalate as a main recurring unit. Both the first copolyester and the blend contain diethylene glycol in an amount of 0.05 to 8 mol %. This film has a water extraction of 0.5 mg/inch.sup.2 or less and a center line surface roughness (Ra) of 4 to 30 nm.
摘要:
A biaxially oriented polyester film to be laminated onto a metal plate and molded, (A) which comprises a copolyester comprising (a) terephthalic acid in an amount of 82 to 100 mol % and 2,6-naphthalenedicarboxylic acid or a combination of 2,6-naphthalenedicarboxylic acid and other dicarboxylic acid in an amount of 0 to 18 mol % of the total of all dicarboxylic acid components and (b) ethylene glycol in an amount of 82 to 100 mol % and cyclohexanedimethanol or a combination of cyclohexanedimethanol and other diol in an amount of 0 to 18 mol % of the total of all diol components, having (c) a glass transition temperature of 78° C. or more and (d) a melting point of 210 to 250° C., and containing (e) porous silica particles with a pore volume of 0.5 to 2.0 ml/g which are agglomerates of primary particles having an average particle diameter of 0.001 to 0.1 &mgr;m; and (B) which has the following relationship between the highest peak temperature (Te, °C.) of loss elastic modulus and the glass transition temperature (Tg, °C.): Te−Tg≦30. This film has improved taste-and-flavor retainabilities, particularly taste and flavor retainabilities after a retort treatment, without losing the excellent moldability, heat resistance, impact resistance and retort resistance of a copolyester film.
摘要:
A biaxially oriented polyester film to be laminated onto a metal plate and molded, which comprises a copolyester, said copolyester comprising (a) terephthalic acid in an amount of 82 to 100 mol % and 2,6-naphthalenedicarboxylic acid or a combination of 2,6-naphthalenedicarboxylic acid and other dicarboxylic acids in an amount of 0 to 18 mol % of the total of all dicarboxylic acid components and (b) ethylene glycol in an amount of 82 to 100 mol % and cyclohexanedimethanol or a combination of cyclohexanedimethanol and other diols in an amount of 0 to 18 mol % of the total of all diol components, and having (c) a glass transition temperature of 78.degree. C. or higher and (d) a melting point of 210 to 250.degree. C. The said film has the following relationship between the highest peak temperature (Te, .degree. C.) of loss elastic modulus and the glass transition temperature (Tg, .degree. C.): Te-Tg.ltoreq.30, or its content of a free dicarboxylic acid diol ester is 50 ppm or less. The said film has improved flavor retention properties for its contents taste, particularly taste and flavor retention properties after a retort treatment, while retaining excellent moldability, heat resistance, impact resistance.
摘要:
A laminated film comprising a porous semiconductor layer, a transparent conductive layer and a transparent plastic film, wherein the porous semiconductor layer comprises crystalline titanium oxide fibers and crystalline titanium oxide fine particles, the crystalline titanium oxide fibers and the crystalline titanium oxide fine particles are substantially composed of an anatase phase and a rutile phase, the anatase phase content ratio calculated from the integral intensity ratio of X-ray diffraction is between 1.00 and 0.32, and the laminated film is used in an electrode for dye-sensitized solar cells, and the electrode and a dye-sensitized solar cell comprising the same.
摘要:
An antistatic film having an antistatic coating film on at least one surface of a polyester film, the antistatic coating film comprising a polymer having a polymerized unit represented by the following formula (1): wherein R1 and R2 each independently represent a hydrogen atom or a methyl group, R3 represents an alkylene group having 2 to 10 carbon atoms, R4 and R5 each independently represent an alkyl group having 1 to 5 carbon atoms, R6 represents a hydrogen atom, an alkyl group having 1 to 5 carbon atoms or a hydroxyalkyl group having 2 to 10 carbon atoms, and Y− represents a halogen ion, a halogenated alkyl ion, a nitrate ion, a sulfate ion, an alkyl sulfate ion, a sulfonate ion or an alkyl sulfonate ion. The film is used in such applications requiring an antistatic property such as a protective film for a liquid crystal polarizing plate.
摘要:
There is provided a laminated polyester film which is improved in lubricity, transparency, dimensional stability, shock resistance and adhesion, and which comprises a polyester base film comprising polyester and to at least one direction, and a coating layer provided on at least one surface of the base film, wherein said coating layer contains polymer binder and inert particles, the refractive index of the inert particles being substantially same as that of the polymer binder, and wherein the laminated polyester film has a haze of 1.5% or less, a total light transmittance of 85% or more, 50% destructing energy per 100 μm film thickness of 0.3 J or more, and a thermal shrinkage at 230° C. for 30 minutes of 4% or less.