Shutdown, bilayer battery separator
    1.
    发明授权
    Shutdown, bilayer battery separator 失效
    关闭,双层电池分离器

    公开(公告)号:US5565281A

    公开(公告)日:1996-10-15

    申请号:US348630

    申请日:1994-12-02

    摘要: The present invention is directed to a shutdown, bilayer battery separator and a process for making the same. A first microporous membrane with shutdown capability and a second microporous membrane with strength capability are joined together in face-to-face contact. The face of the first membrane being adhered by calendaring, adhesives, or welding, to the face of the second membrane, and the separator having a thickness of less than 3 mils, and a puncture strength, as measured from the second microporous membrane, of greater than 1900 g-mm, and a peel strength of greater than 1 grams/centimeter.

    摘要翻译: 本发明涉及关闭双层电池隔板及其制造方法。 具有关闭能力的第一微孔膜和具有强度能力的第二微孔膜以面对面接触连接在一起。 第一膜的表面通过压延,粘合剂或焊接粘附到第二膜的表面,并且具有小于3密耳的厚度的隔膜和从第二微孔膜测量的穿刺强度为 大于1900g-mm,剥离强度大于1克/厘米。

    FOUNDATION PILE AND INSTALLING METHOD THEREOF
    2.
    发明申请
    FOUNDATION PILE AND INSTALLING METHOD THEREOF 审中-公开
    基础桩及其安装方法

    公开(公告)号:US20120301227A1

    公开(公告)日:2012-11-29

    申请号:US13270308

    申请日:2011-10-11

    IPC分类号: E02D5/34

    CPC分类号: E02D5/28

    摘要: A foundation pile includes a tubular wall, a top cap covering a top end of the tubular wall, a partition plate disposed transversely in the tubular wall below the top cap and dividing an inner space of the tubular wall into upper and lower spaces, two opposite fixing holes extending radially through the tubular wall and communicated with the upper space, and a plurality of pressure release holes extending radially through the tubular wall and communicated with the lower space. The partition plate prevents concrete slurry from flowing into the upper space. The pressure release holes allow the concrete to consolidate therein and to thereby increase transverse binding forces with the foundation pile. A method of installing the foundation pile is also disclosed.

    摘要翻译: 基础桩包括管状壁,覆盖管状壁的顶端的顶盖,横向设置在顶盖下方的管状壁中并将管状壁的内部空间分隔成上部和下部空间的隔板,两个相对的 固定孔径向延伸穿过管状壁并与上部空间连通,并且多个压力释放孔径向延伸穿过管状壁并与下部空间连通。 隔板防止混凝土浆料流入上部空间。 压力释放孔允许混凝土在其中固结,从而增加与基础桩的横向结合力。 还公开了一种安装地基桩的方法。

    Film capacitors comprising melt-stretched films as dielectrics
    6.
    发明申请
    Film capacitors comprising melt-stretched films as dielectrics 审中-公开
    薄膜电容器包括作为电介质的熔融拉伸薄膜

    公开(公告)号:US20120008251A1

    公开(公告)日:2012-01-12

    申请号:US12805104

    申请日:2010-07-12

    申请人: Wei-Ching Yu Jason Yu

    发明人: Wei-Ching Yu Jason Yu

    IPC分类号: H01G4/18 H01G4/06 H01G4/008

    CPC分类号: H01G4/18 H01G4/32

    摘要: A film capacitor comprising (1) of electric conduction electrodes and (2) of semi-crystalline polymeric dielectric film(s), the thickness of which ranges from 1 micron to 80 micron, made by a melt-stretching extrusion process through a die (circular die or flat die) with a drawdown ratio of 30 or higher (the ratio of die gap to the film thickness) at die temperatures higher than the melting point of said semi-crystalline polymer(s). The semi-crystalline polymeric dielectric films made by such melt-stretching extrusion process show a significantly low shrinkage at high temperatures until they are melted. The capacitor comprising such low shrinkage film dielectrics can be used at a much higher temperature than comprising conventional biaxially oriented film dielectrics made of the same plastic materials.

    摘要翻译: 一种薄膜电容器,其包括(1)导电电极和(2)半结晶聚合物电介质薄膜,其厚度范围为1微米至80微米,通过熔融拉伸挤出方法通过模头 圆模或平模),其在比所述半结晶聚合物的熔点高的模具温度下具有30或更高的压下比(模头间隙与膜厚度的比率)。 通过这种熔融拉伸挤出方法制备的半结晶聚合物介电膜在高温下显示出显着低的收缩率,直到它们熔融。 包括这种低收缩膜电介质的电容器可以在比包含由相同塑料材料制成的常规双轴取向薄膜电介质的温度高得多的温度下使用。

    Method of making a trilayer battery separator
    8.
    发明授权
    Method of making a trilayer battery separator 失效
    制造三层电池隔膜的方法

    公开(公告)号:US5952120A

    公开(公告)日:1999-09-14

    申请号:US839664

    申请日:1997-04-15

    摘要: A method of making a trilayer, shutdown battery separator has the following steps: extruding a polyethylene precursor; extruding a polypropylene precursor; forming a trilayer precursor, the trilayer precursor having the polyethylene precursor sandwiched between two polypropylene precursors; bonding the trilayer precursor; annealing the trilayer precursor; stretching the trilayer precursor; and forming thereby the battery separator.

    摘要翻译: 制造三层,关闭电池隔板的方法有以下步骤:挤出聚乙烯前体; 挤出聚丙烯前体; 形成三层前体,所述三层前体具有夹在两个聚丙烯前体之间的聚乙烯前体; 键合三层前体; 退火三层前体; 拉伸三层前体; 并由此形成电池隔板。

    PROCESS FOR CRYSTALLIZING AND SOLID STATE POLYMERIZING POLYMERS AND THE COATED POLYMER
    10.
    发明申请
    PROCESS FOR CRYSTALLIZING AND SOLID STATE POLYMERIZING POLYMERS AND THE COATED POLYMER 审中-公开
    用于结晶和固态聚合聚合物和涂覆的聚合物的方法

    公开(公告)号:US20090169782A1

    公开(公告)日:2009-07-02

    申请号:US11719231

    申请日:2004-11-22

    申请人: Wei-Ching Yu

    发明人: Wei-Ching Yu

    IPC分类号: B05D7/02 B32B5/16 B32B27/06

    摘要: This invention relates to a process for crystallizing and solid state polymerizing polymers, in the form of amorphous pellets by coating the pellets with a coating of 50 to 250 ppm of an anti-sticking agent to the amorphous pellets. The invention also relates to such a coated pellet. The coated pellet is then heated such that its surface is at least partially crystallized or essentially crystallized. Next it is solid state polymerize to a high molecular weight. The capacity of the crystallization and solid state polymerization process can be increased by using higher temperatures when the anti-sticking agent is present as compared to a normal process using the same polymer. The preferred anti-sticking agents are chosen to give high clarity to articles made from the high molecular weight pellet. The preferred anti-slicking agent is fumed silica, but other organic and inorganic coatings may be used.