摘要:
A spheroidal graphite cast iron having an excellent impact strength at low temperature and a method for producing the same are provided. The present disclosure relates to the spheroidal graphite cast iron comprising: C: 3.5 mass % to 4.2 mass %; Si: 2.0 mass % to 2.8 mass %; Mn: 0.2 mass % to 0.4 mass %; Cu: 0.1 mass % to 0.7 mass %; Mg: 0.02 mass % to 0.06 mass %; Cr: 0.01 mass % to 0.15 mass %; and the balance: Fe and inevitable impurities, wherein Mn+Cr+Cu is 0.431 mass % to 1.090 mass %, a graphite nodule count is 230/mm2 or less, and a pearlite fraction is 30% to 85%.
摘要:
A hard metal material and a method of manufacturing a component of the hard metal material are disclosed. The hard metal material comprises 5-50 volume % particles of a refractory material dispersed in a host metal. The method comprises forming a slurry of 5-50 volume % particles of the refractory material dispersed in a liquid host metal in an liquid atmosphere and pouring the slurry into a mould and forming a casting of the component.
摘要:
A casting of a white cast iron alloy and a method of producing the casting are disclosed. A white cast alloy is also disclosed. The casting has a solution treated microstructure that comprises a ferrous matrix of retained austenite and chromium carbides dispersed in the matrix, with the carbides comprising 15 to 60% volume fraction of the alloy. The matrix composition comprises: manganese: 8 to 20 wt %; carbon: 0.8 to 1.5 wt %; chromium: 5 to 15 wt %; and iron: balance (including incidental impurities).
摘要:
A spheroidal graphite cast iron comprising: C: 3.3 to 4.0 mass %, Si: 2.1 to 2.7 mass %, Mn: 0.20 to 0.50 mass %, S: 0.005 to 0.030 mass %, Cu: 0.20 to 0.50 mass %, Mg: 0.03 to 0.06 mass % and the balance: Fe and inevitable impurities, wherein a tensile strength is 550 MPa or more, and an elongation is 12% or more.
摘要:
A cast iron having high strength, hardness, and thermal conductivity for a cylinder liner of an internal combustion engine is provided. The cast iron includes 3.2 wt. % to 3.8 wt. % carbon, 2.2 wt. % to 3.2 wt. % silicon, 0.5 wt. % to 1.3 wt. % copper, and at least 75.0 wt. % iron, based on the total weight of the cast iron. The cast iron further includes 0.01 wt. % to 0.5 wt. % manganese, 0.01 wt. % to 0.2 wt. % chromium, up to 0.3 wt. % phosphorous, up to 0.05 wt. % sulfur, up to 0.2 wt. % tin, and up to 0.1 wt. % magnesium, based on the total weight of the cast iron. Preferably, the cast iron is free of molybdenum, nickel, and vanadium. The cast iron is also heat treated and solidifies to achieve fully spheroidal graphite.
摘要:
A roll outer layer material contains small-size carbides having a circle equivalent diameter of 3 to 30 μm in a number of 500 to 2500 pieces/mm2 and large-size carbides having a circle equivalent diameter of 50 μm or more in a number of 20 pieces/mm2 or less, preferably having a chemical composition containing, by mass %, C: 2.4% or more and 2.9% or less, Si: 0.2% or more and 1.0% or less, Mn: 0.2% or more and 1.0% or less, Cr: 4.0% or more and 7.5% or less, Mo: 4.0% or more and 6.5% or less, V: 5.3% or more and 7.0% or less, Nb: 0.5% or more and 3.0% or less, and the balance being Fe and inevitable impurities, in which the contents of Cr, Mo, and V satisfy the relationship 1.5≦(Cr+Mo)/V≦2.4.
摘要:
A thermal spray powder is provided for use in a thermal spray technique, such as flame spraying, plasma spraying, cold spraying, and high velocity oxygen fuel spraying (HVOF). The thermal spray powder is formed by water or gas atomization and comprises 3.0 to 7.0 wt. % carbon, 10.0 to 25.0 wt. % chromium, 1.0 to 5.0 wt. % tungsten, 3.5 to 7.0 wt. % vanadium, 1.0 to 5.0 wt. % molybdenum, not greater than 0.5 wt. % oxygen, and at least 40.0 wt. % iron, based on the total weight of the thermal spray powder. The thermal spray powder can be applied to a metal body, such as a piston or piston ring, to form a coating. The thermal spray powder can also provide a spray-formed part.
摘要:
Heat resistant spheroidal graphite cast iron having an improved high temperature tensile strength includes carbon (C) in a range of 3.2-3.4 wt %, silicon (Si) in a range of 4.3-4.8 wt %, manganese (Mn) in a range of 0.2-0.3 wt %, molybdenum (Mo) in a range of 0.8-1.0 wt %, vanadium (V) in a range of 0.4-0.6 wt %, chrome (Cr) in a range of 0.2-0.4 wt %, niobium (Nb) in a range of 0.2-0.4 wt %, inevitable impurities, and a remainder of iron (Fe) based on a total weight of the heat resistant spheroidal graphite cast iron. The heat resistant spheroidal graphite cast iron further includes barium (Ba) in a range of 0.0045-0.0075 wt %. A content ratio of chrome (Cr) and barium (Ba) (Cr/Ba) is in a range from about 26 to about 89.
摘要:
Disclosed are a hypereutectic white iron alloy and articles such as pump components made therefrom. Besides iron and unavoidable impurities the alloy comprises, in weight percent based on the total weight of the alloy, from 3 to 6 C, from 0.01 to 1.2 N, from 0.1 to 4 B, from 3 to 48 Cr, from 0.1 to 7.5 Ni and from 0.1 to 4 Si and, optionally, one or more of Mn, Co, Cu, Mo, W, V, Mg, Ca, rare earth elements, Nb, Ta, Ti, Zr, Hf, Al.
摘要翻译:公开了一种过共晶白色铁合金和诸如由其制成的泵组件的制品。 除了铁和不可避免的杂质之外,合金的重量百分比以合金的总重量为基准计,为3至6℃,0.01至1.2N,0.1至4 B,3至48 Cr,0.1至7.5 Ni Mn,Co,Cu,Mo,W,V,Mg,Ca,稀土元素,Nb,Ta,Ti,Zr,Hf,Al中的一种或多种。
摘要:
A powder metal steel alloy composition for high wear and temperature applications is made by water atomizing a molten steel alloy composition containing C in an amount of at least 3.0 wt %; at least one carbide-forming alloy element selected from the group consisting of: Cr, V, Mo or W; an O content less than about 0.5 wt %, and the balance comprising essentially Fe apart from incidental impurities. The high carbon content reduces the solubility of oxygen in the melt and thus lowers the oxygen content to a level below which would cause the carbide-forming element(s) to oxidixe during water atomization. The alloy elements are thus not tied up as oxides and are available to rapidly and readily form carbides in a subsequent sintering stage. The carbon, present in excess, is also available for diffusing into one or more other admixed powders that may be added to the prealloyed powder during sintering to control microstructure and properties of the final part.