Coated narrow band green phosphor

    公开(公告)号:US10584280B2

    公开(公告)日:2020-03-10

    申请号:US15775318

    申请日:2017-10-20

    Abstract: A coated phosphor may comprise: phosphor particles comprised of a phosphor with composition (M)(A)2S4: Eu, wherein: M is at least one of Mg, Ca, Sr and Ba; and A is at least one of Ga, Al, In, Y; a dense impermeable (pinhole-free) coating of an oxide material encapsulating individual ones of the phosphor particles. The coated phosphor is configured to satisfy one or more of the conditions: (1) under excitation by blue light, the reduction in photoluminescent intensity at the peak emission wavelength after 1,000 hours of aging at about 85° C. and about 85% relative humidity is no greater than about 30%; (2) the change in chromaticity coordinates CIE(y), ΔCIE y, after 1,000 hours of aging at about 85° C. and about 85% relative humidity is less than about 5×10−3; (3) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least two hours at 85° C.; (4) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least one day at 20° C.; and (5) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least 5 days at 20° C.

    Coatings for Photoluminescent Materials
    6.
    发明申请
    Coatings for Photoluminescent Materials 审中-公开
    光致发光材料涂料

    公开(公告)号:US20150284628A1

    公开(公告)日:2015-10-08

    申请号:US14682831

    申请日:2015-04-09

    Abstract: The teachings are generally directed to phosphors having combination coatings with multifunctional characteristics that increase the performance and/or reliability of the phosphor. The teachings include highly reliable phosphors having coatings that contain more than one inorganic component, more than one layer, more than one thicknesses, more than one combination of layers or thicknesses, a gradient-interface between components, a primer thickness or layer to inhibit or prevent leaching of phosphor components into the coatings, a sealant layer to inhibit or prevent entry of moisture or oxygen from the environment, a mixed composition layer as a sealant and multifunctional combination coatings.

    Abstract translation: 该教导通常涉及具有增加荧光体的性能和/或可靠性的具有多功能特性的组合涂层的荧光体。 该教导包括高度可靠的荧光体,其具有包含多于一种无机组分,多于一层,多于一个厚度,多于一层或多层组合的涂层,组分之间的梯度界面,底漆厚度或抑制层或 防止荧光体组分浸入涂层中,抑制或防止水分或氧从环境进入的密封剂层,作为密封剂的混合组合物层和多功能组合涂层。

    Coatings for photoluminescent materials
    8.
    发明授权
    Coatings for photoluminescent materials 有权
    光致发光材料涂料

    公开(公告)号:US09006966B2

    公开(公告)日:2015-04-14

    申请号:US13671501

    申请日:2012-11-07

    Abstract: The teachings are generally directed to phosphors having combination coatings with multifunctional characteristics that increase the performance and/or reliability of the phosphor. The teachings include highly reliable phosphors having coatings that contain more than one inorganic component, more than one layer, more than one thicknesses, more than one combination of layers or thicknesses, a gradient-interface between components, a primer thickness or layer to inhibit or prevent leaching of phosphor components into the coatings, a sealant layer to inhibit or prevent entry of moisture or oxygen from the environment, a mixed composition layer as a sealant and multifunctional combination coatings.

    Abstract translation: 该教导通常涉及具有增加荧光体的性能和/或可靠性的具有多功能特性的组合涂层的荧光体。 该教导包括高度可靠的荧光体,其具有包含多于一种无机组分,多于一层,多于一个厚度,多于一层或多层组合的涂层,组分之间的梯度界面,底漆厚度或抑制层或 防止荧光体组分浸入涂层中,抑制或防止水分或氧从环境进入的密封剂层,作为密封剂的混合组合物层和多功能组合涂层。

    Coated narrow band green phosphor

    公开(公告)号:US11015116B2

    公开(公告)日:2021-05-25

    申请号:US16814110

    申请日:2020-03-10

    Abstract: A coated phosphor may comprise: phosphor particles comprised of a phosphor with composition (M)(A)2S4:Eu, wherein: M is at least one of Mg, Ca, Sr and Ba; and A is at least one of Ga, Al, In, Y; a dense impermeable (pinhole-free) coating of an oxide material encapsulating individual ones of the phosphor particles. The coated phosphor is configured to satisfy one or more of the conditions: (1) under excitation by blue light, the reduction in photoluminescent intensity at the peak emission wavelength after 1,000 hours of aging at about 85° C. and about 85% relative humidity is no greater than about 30%; (2) the change in chromaticity coordinates CIE(y), ΔCIE y, after 1,000 hours of aging at about 85° C. and about 85 % relative humidity is less than about 5×10−3; (3) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least two hours at 85° C.; (4) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least one day at 20° C.; and (5) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least 5 days at 20° C.

    Coated Narrow Band Green Phosphor
    10.
    发明申请

    公开(公告)号:US20200208049A1

    公开(公告)日:2020-07-02

    申请号:US16814110

    申请日:2020-03-10

    Abstract: A coated phosphor may comprise: phosphor particles comprised of a phosphor with composition (M)(A)2S4:Eu, wherein: M is at least one of Mg, Ca, Sr and Ba; and A is at least one of Ga, Al, In, Y; a dense impermeable (pinhole-free) coating of an oxide material encapsulating individual ones of the phosphor particles. The coated phosphor is configured to satisfy one or more of the conditions: (1) under excitation by blue light, the reduction in photoluminescent intensity at the peak emission wavelength after 1,000 hours of aging at about 85° C. and about 85% relative humidity is no greater than about 30%; (2) the change in chromaticity coordinates CIE(y), ΔCIE y, after 1,000 hours of aging at about 85° C. and about 85 % relative humidity is less than about 5×10−3; (3) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least two hours at 85° C.; (4) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least one day at 20° C.; and (5) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least 5 days at 20° C.

Patent Agency Ranking