摘要:
Provided is a method for producing regularly ordered narrow pores excellent in linearity, and a structure with such narrow pores. A method for producing a narrow pore comprises a step of radiating a particle beam onto a workpiece, and a step of carrying out anodic oxidation of the workpiece having been irradiated with the particle beam, to form a narrow pore in the workpiece.
摘要:
Disclosed herein is a process for producing a narrow titanium-containing wire, comprising steps of: (i) providing a structure comprising a substrate having a titanium-containing surface and a porous layer containing narrow pores extending towards the surface; and (ii) forming narrow titanium-containing wires in the respective narrow pores by heat treatment of the structure obtained in the step (i).
摘要:
A method of producing a structure having narrow pores includes a first step of bringing pore-guiding members into contact with upper and lower surfaces of a member comprising aluminum as a principal ingredient and a second step of anodizing the member comprising aluminum as the principal ingredient to form narrow pores. The pore-guiding members contain the same material as a principal ingredient. The second step includes preferably a step of transforming the member comprising aluminum as the principal ingredient into a porous body comprising alumina having narrow pores oriented substantially parallel to the interfaces between the pore-guiding members and the member comprising aluminum as the principal ingredient.
摘要:
A method for producing narrow wires including titanium oxide of high crystallinity and diameter of the order of nanometer, in particular whiskers of titanium oxide, and including a first step of preparing a base having a titanium-including surface, second step of discretely depositing a material other than titanium over the above surface, and third step of thermally treating the above surface, obtained by the second step, in a titanium-oxidizing atmosphere.
摘要:
A metal oxide is provided which is represented by the compositional formula:(Bi.sub.1-x A.sup.I.sub.x).sub.2 (Sr.sub.y Ca.sub.1-y-z A.sup.II.sub.z).sub.p (Cu.sub.1-r A.sup.III.sub.r).sub.q O.sub..delta.wherein 0.ltoreq.x.ltoreq.0.5, 0.3.ltoreq.y.ltoreq.0.7, 0.ltoreq.z.ltoreq.0.5, 0.ltoreq.r.ltoreq.0.1, 1>y+z, 2>p>11, 1.ltoreq.q.ltoreq.10 and 5.4.ltoreq..delta..ltoreq.24 with the exclusion of x=z=r=0, A.sup.I is at least one element selected from In, Sb, Pb and Sn; A.sup.II is at least one element selected from Na, K, Mg, Ba, and Sn and A.sup.III is at least one element selected from Ti, V, Cu, Ni, Zr, Nb, Ta, Fe and Ru. The metal oxide may further comprise an element selected from lanthanoids and yttrium. The metal oxide material shows superconductivity at a temperature not lower than the boiling point of liquid helium.
摘要翻译:提供了由组成式:(Bi1-xAl x)2(SryCa1-y-zAIIz)p(Cu1-rAIIIr)qOδ表示的金属氧化物,其中0≤x≤0.5,0.3≤y = 0.7,0 = z = 0.5,0 = r = 0.1,1> y + z,2> p> 11,1 = 10和5.4 < =ΔX= 24,排除x = z = r = 0,AI是选自In,Sb,Pb和Sn中的至少一种元素; AII是选自Na,K,Mg,Ba和Sn中的至少一种元素,AIII是选自Ti,V,Cu,Ni,Zr,Nb,Ta,Fe和Ru中的至少一种元素。 金属氧化物还可以包含选自镧系元素和钇的元素。 金属氧化物材料在不低于液氦的沸点的温度下显示出超导性。
摘要:
A light detecting device includes a signal input portion which generates a current upon input of a light signal, a signal detecting portion including a superconductor which detects the light signal with injection of the generated current, and electrodes through which the generated current is injected into the superconductor.
摘要:
An object of the present invention is to provide a new light-emitting device with the use of an amorphous oxide. The light-emitting device has a light-emitting layer existing between first and second electrodes and a field effect transistor, of which the active layer is an amorphous.
摘要:
A light-emitting device is provided that is excellent in light emission efficiency and stability. The light-emitting device has a first part of a first dielectric constant, a second part of a second dielectric constant and a third part of a third dielectric constant, and has a triple junction where they are in contact with one another. Moreover, a first and a second electrode are provided for applying a voltage for controlling an electric field at the triple junction and in the vicinity thereof. Further, at least one of the first, the second and the third parts is a constituted by light-emitting material, and the triple junction forms a closed line.
摘要:
A molding apparatus for patterning a workpiece includes a mold having a pattern to be transferred to the workpiece, with the pattern including recesses, a first support member for supporting the mold, and a second support member, arranged opposite to the first support member, for supporting the workpiece. A pressing mechanism brings the first and second support members close to each other and presses the mold and the workpiece together so as to transfer, to the workpiece, the pattern on the mold. Recessed portions are provided on at least one of a surface of the mold on the first support member side, a region of the first support member, and a region of the second support member. The recessed portions correspond to recesses in the pattern of the mold.
摘要:
A molding apparatus for patterning a workpiece includes a mold having a pattern to be transferred to the workpiece, with the pattern including recesses, a first support member for supporting the mold, and a second support member, arranged opposite to the first support member, for supporting the workpiece. A pressing mechanism brings the first and second support members close to each other and presses the mold and the workpiece together so as to transfer, to the workpiece, the pattern on the mold. Recessed portions are provided on at least one of a surface of the mold on the first support member side, a region of the first support member, and a region of the second support member. The recessed portions correspond to recesses in the pattern of the mold.