Formulated resin component for use in spray-in-place foam system to produce a low density polyurethane foam
    111.
    发明申请
    Formulated resin component for use in spray-in-place foam system to produce a low density polyurethane foam 有权
    配制树脂组分,用于喷雾现场泡沫体系,以生产低密度聚氨酯泡沫

    公开(公告)号:US20050043423A1

    公开(公告)日:2005-02-24

    申请号:US10644450

    申请日:2003-08-20

    摘要: The subject invention provides an open-celled polyurethane foam formed from a polyurethane spray foam system that mixes a formulated resin component with an isocyanate component. The resultant open-celled polyurethane spray foam has a density of about ½ pound per cubic foot. The resin component includes water as a blowing agent, a first aliphatic, amine-initiated polyol having a number-average molecular weight of from 150 to 500 and having tetra-functionality, and a second polyol having terminal hydroxyl groups and having a number-average molecular weight of from 3500 to 8000. A curing component having at least one primary amine group and having a number-average molecular weight of from 150 to 5000 is also included in the resin component. The spray foam system reacts a) the resin component and b) the isocyanate component in a volumetric ratio of a) to b) of from 1:1.2 to 1:5 and having an isocyanate index of from 15 to 70.

    摘要翻译: 本发明提供由聚氨酯喷雾泡沫体系形成的开孔聚氨酯泡沫体,其将配制的树脂组分与异氰酸酯组分混合。 所得的开孔聚氨酯喷雾泡沫体的密度约为1/2磅/立方英尺。 树脂组分包括作为发泡剂的水,数均分子量为150-500的具有四官能度的第一种脂族胺引发的多元醇,和具有末端羟基并具有数均分子量的第二多元醇 分子量为3500至8000.树脂组分中还包括具有至少一个伯胺基且数均分子量为150至5000的固化组分。 喷雾泡沫体系a)树脂组分和b)异氰酸酯组分的体积比为a)至b)为1:1.2至1:5,异氰酸酯指数为15至70。

    Flame resistant rigid foams and formulations for the production thereof
    112.
    发明申请
    Flame resistant rigid foams and formulations for the production thereof 有权
    阻燃硬质泡沫塑料及其制备方法

    公开(公告)号:US20030225174A1

    公开(公告)日:2003-12-04

    申请号:US10384882

    申请日:2003-03-10

    IPC分类号: C08G018/00

    摘要: The invention relates to flame resistant rigid foams and formulations useful for the production thereof. The polyol formulation must include at least one substance which is inert with respect to isocyanates, does not deplete the ozone layer and has a boiling point below 55null C. and a reaction product of at least one compound with an aromatic ring, at least one aldehyde or ketone and at least one primary or secondary amine. This polyol formulation is reacted with an isocyanate, optionally with other commonly used additives, to produce rigid flame resistant foams.

    摘要翻译: 本发明涉及用于制备其的阻燃硬质泡沫和制剂。 多元醇制剂必须包括至少一种相对于异氰酸酯是惰性的物质,不会消耗臭氧层并且沸点低于55℃,并且至少一种化合物与芳环的反应产物,至少一种 醛或酮和至少一种伯胺或仲胺。 该多元醇配方与任选与其它常用添加剂的异氰酸酯反应以制备刚性阻燃泡沫体。

    Low-temperature, heat-activated adhesives with high heat resistance properties
    117.
    发明申请
    Low-temperature, heat-activated adhesives with high heat resistance properties 有权
    低温,热活化粘合剂具有高耐热性能

    公开(公告)号:US20020068792A1

    公开(公告)日:2002-06-06

    申请号:US09954943

    申请日:2001-09-18

    IPC分类号: C08K003/00

    摘要: The present invention is directed to a polymer component having controlled branching, formed from the reaction product of a prepolymer and a chain extender, which prepolymer is itself formed from the reaction product of a mixture of a non-self-associating isocyanate component, a diol component having a molecular weight from about 1500 to 6000 grams/mole and present in an amount greater than about 50% by weight based on the total weight of the prepolymer, and an ion-forming compound, where the chain extender includes an amine-containing compound and is present in an amount sufficient to react with at least about 99% of the isocyanate groups present after the prepolymer has been formed, wherein the controlled branching of the polymer includes at least one of: a hydroxy-functional component having hydroxyl functionality greater than 2.0 and a molecular weight from about 700 to 2000; or a low molecular weight component having more than two hydroxyl groups. Methods of making and using such dispersion compositions are also included.

    摘要翻译: 本发明涉及由预聚物和扩链剂的反应产物形成的受控支化的聚合物组分,该预聚物本身由非自缔合的异氰酸酯组分,二醇的混合物的反应产物形成 组分,其分子量为约1500至6000克/摩尔,并且以基于预聚物总重量的约50重量%的量存在,以及形成离子的化合物,其中扩链剂包含含胺 化合物,并且其存在量足以与形成预聚物之后存在的至少约99%的异氰酸酯基反应,其中聚合物的受控支化包括以下至少一种:具有羟基官能度的羟基官能组分 大于2.0,分子量约为700至2000; 或具有多于两个羟基的低分子量组分。 还包括制备和使用这种分散组合物的方法。