AQUEOUS COATING COMPOSITION WITH SOFT TOUCH UPON DRYING

    公开(公告)号:US20210087427A1

    公开(公告)日:2021-03-25

    申请号:US17109128

    申请日:2020-12-01

    Abstract: Aqueous coating compositions include dispersed polyurethane-vinyl polymer hybrid particles obtained by free-radical polymerization of at least one vinyl monomer in the presence of a polyurethane. The polyurethane and the vinyl polymer in the hybrid particles are present in a weight ratio of polyurethane to vinyl polymer ranging from 1:1 to 20:1, and the polyurethane is the reaction product of at least the following components: (a) from 5 to 40 wt. % of at least one organic difunctional isocyanate, (b) from 0.5 to 4 wt. % of an isocyanate-reactive compound containing ionic or potentially ionic water-dispersing groups having a molecular weight of from 100 to 500 g/mol, (c) from 40 to 80 wt. % of at least one diol having a molecular weight from 500 to 5000, (d) from 0 to 10 wt. % of at least one active-hydrogen chain extending compound with a functionality of at least 2 other than water, (e) from 0 to 10 wt. % of at least one diol having a molecular weight below 500 g/mol. The isocyanate and hydroxy groups on the components used are present in a respective mole ratio (NCO to OH) in the range of from 0.8:1 to 5:1.

    WATERBORNE DISPERSIONS
    12.
    发明申请

    公开(公告)号:US20210079209A1

    公开(公告)日:2021-03-18

    申请号:US16772994

    申请日:2018-12-18

    Abstract: The present invention relates to a waterborne dispersion comprising (A) amphiphilic block copolymer obtained with a controlled radical polymerization process and comprising at least blocks [A] and [B], whereby block [A] comprises ethylenically unsaturated monomer(s) bearing water-soluble and/or water-dispersible functional groups (monomer(s) (i)), and block [B] comprises ethylenically unsaturated monomer(s) different from monomer(s) (i) (monomer(s) (ii)); and (B) polymer P comprising ethylenically unsaturated monomer(s) different from (i) (monomer(s) (ii)), characterized in that the amount of block copolymer is higher than 1 and lower than 30 wt. %, based on the total weight of monomers used to prepare the block copolymer and polymer P; the acid value of the composition consisting of block copolymer and polymer P is higher than 1 and at most 35 mg KOH per g of the block copolymer-polymer P composition; the block copolymer has a calculated glass transition temperature of higher than 10° C. and lower than 250° C.; and polymer P comprises at least 20 wt. % (relative to the total monomer composition to prepare the polymer P) of a polymer fraction with calculated glass transition temperature higher than 10° C. and lower than 100° C.

    AQUEOUS COATING COMPOSITION
    13.
    发明申请

    公开(公告)号:US20200095460A1

    公开(公告)日:2020-03-26

    申请号:US16483823

    申请日:2018-02-07

    Abstract: The present invention relates to an aqueous coating composition comprising polyurethane A and vinyl polymer, wherein the polyurethane A comprising as building blocks at least: (a) a polyisocyanate(s) containing at least one cyclic group, (b) a non-cyclic aliphatic diisocyanate(s) whereby the non-cyclic aliphatic group connecting the two isocyanate groups has 5 carbon atoms, and (c) a component(s) containing an isocyanate-reactive group(s), whereby the summed amount of (a) and (b) is 10 to 60 wt. %, relative to the total weight amount of components used to prepare the polyurethane A; and whereby the weight ratio between (a) and (b) is in the range from 50:50 to 99:1.

    AQUEOUS POLYMER EMULSION
    15.
    发明申请

    公开(公告)号:US20180030186A1

    公开(公告)日:2018-02-01

    申请号:US15550565

    申请日:2016-02-12

    Abstract: The present invention relates to an aqueous polymer emulsion comprising at least 30 wt. % of a vinyl copolymer (A), said vinyl copolymer comprising: (I) from 10 to 90 wt. % of 2-octyl acrylate monomer; (II) from 10 to 90 wt. % of at least one itaconate ester monomer according to formula (1) in which A and B may be different or the same and A and B are independently an alkyl group or an aryl group; and (III) from 0 to 80 wt. % of ethylenically unsaturated monomer other than (I) and (II); whereby the summed amount of (I), (II) and (III) is 100 wt. % and whereby the amount of vinyl copolymer (A) is given relative to the total weight amount of the polymers present in the emulsion.

    POLYMER, PROCESS AND USE
    16.
    发明申请

    公开(公告)号:US20170240765A1

    公开(公告)日:2017-08-24

    申请号:US15519354

    申请日:2015-10-21

    Abstract: The current invention relates to a process for preparing an aqueous binder composition free of organic solvent, the process comprising at least the following steps: A) preparing a hydrophilic vinyl polymer (Polymer A) by polymerisation of a monomer composition A that contains: Ai) at least one carboxylic acid functional olefinically unsaturated monomer; and Aii) at least one olefinically unsaturated monomer different than Ai); and Aiii) optionally at least one wet adhesion promoting olefinically unsaturated monomer different than Ai and Aii); where Polymer A has an acid value (AV) from 32 to 98 mg KOH/g of solid Polymer A; B) preparing a hydrophobic vinyl polymer (Polymer B) by emulsion polymerization of a monomer composition B in the presence of Polymer A where the monomer composition B contains: Bi) at least one olefinically unsaturated monomer; Bii) optionally carboxylic acid functional olefinically unsaturated monomer different than Bi); and Biii) optionally wet adhesion promoting olefinically unsaturated monomer different than Bi); where Polymer B has an acid value (AV) of no more than 23.4 mg KOH/g of solid polymer B, wherein at least a part of the carboxylic acid groups that are present in Polymer A and Polymer B are neutralized during or following the steps A and/or B to form a (partially) neutralized polymer emulsion; where the weight average molecular weight (Mw) of Polymer A is lower than the weight average molecular weight (Mw) of polymer B; and wherein the process is further characterized by the presence of a further step C) reacting at least 10 mol % of the carboxylic acid and/or carboxylate salt groups of the (partially) neutralized polymer emulsion with an iminating agent to produce an iminated polymer C; wherein the total amount of surfactant applied in steps A, B and C is at most 0.5 wt. %, based on the total weight of monomers charged for the preparation of polymer A and polymer B

    ADHESION TO METAL SURFACES WITH BLOCK COPOLYMERS OBTAINED USING RAFT

    公开(公告)号:US20140170428A1

    公开(公告)日:2014-06-19

    申请号:US14188624

    申请日:2014-02-24

    Abstract: An aqueous, metal, coating composition (and process for obtaining it) comprising a block copolymer and a polymer P; wherein the block copolymer comprises at least blocks [A]x[B]y, where at least block [A] is obtained by a controlled radical polymerisation of at least one ethylenically unsaturated monomer via a reversible addition-fragmentation chain transfer (RAFT) mechanism in solution in the presence of a control agent and a source of free radicals; and where (a) block [A] comprises (i) 0 to 80 mol % of metal adhering ethylenically unsaturated monomers; (ii) 0 to 100 mol % of water dispersible ethylenically unsaturated monomers; (iii) 0 to 70 mol % of C1 to C30 hydrocarbo (meth)acrylate and/or styrenic monomers; (iv) 0 to 35 mol % of ethylenically unsaturated monomer different from i), ii)+iii); where the amount of at least one of i), ii), iii)+iv) is >0 mol %; block [A] has a Hansch parameter x); and (c) polymer P is obtained by an emulsion polymerisation process in the presence of the block copolymer [A][B] and comprises: i) 0 to 5 wt % of metal adhering ethylenically unsaturated monomers; ii) 0 to 15 wt % of water dispersible ethylenically unsaturated monomers; iii) 50 to 100 wt % C1 to C30 hydrocarbo (meth)acrylate and/or styrenic monomers; and iv) 0 to 35% by weight of ethylenically unsaturated monomers units different from those from i), ii)+iii).