Abstract:
A method for making low emissivity panels, including control the composition of a barrier layer formed on a thin conductive silver layer. The barrier structure can include an alloy of a first element having high oxygen affinity with a second element having low oxygen affinity. The first element can include Ta, Nb, Zr, Hf, Mn, Y, Si, and Ti, and the second element can include Ru, Ni, Co, Mo, and W, which can have low oxygen affinity property. The alloy barrier layer can reduce optical absorption in the visible range, can provide color-neutral product, and can improve adhesion to the silver layer.
Abstract:
Embodiments provided herein describe low-e panels and methods for forming low-e panels. A transparent substrate is provided. A low-e stack is formed above the transparent substrate. Each of the layers of the low-e stack are formed to have a specific thickness to tune the performance characteristics of the low-e panel.
Abstract:
Coated articles are disclosed. The coated articles include a doped or alloyed silver layer sandwiched between two layers of transparent conductive oxide such as indium tin oxide (ITO). The doped silver or silver alloy layer can be thin, such as between 1. 5 to 20 nm and thus can be transparent. The doped silver or silver alloy can provide improved ductility property, allowing the conductive stack to be bendable. The transparent conductive oxide layers can also be thin, allowing the conductive stack can have improved ductility property.
Abstract:
Methods for making conducting stacks includes forming a doped or alloyed silver layer sandwiched between two layers of transparent conductive oxide such as indium tin oxide (ITO). The doped silver or silver alloy layer can be thin, such as between 1.5 to 20 nm and thus can be transparent. The doped silver or silver alloy can provide improved ductility property, allowing the conductive stack to be bendable. The transparent conductive oxide layers can also be thin, allowing the conductive stack can have improved ductility property.
Abstract:
Disclosed herein are systems, methods, and apparatus for forming adjustable windows may include a substrate and a first conducting oxide layer formed over the substrate. The adjustable windows may further include a spectral tuning layer formed over the first conducting oxide layer and an ion conductor layer formed over the spectral tuning layer. The adjustable windows may also include an ion storage layer formed over the ion conductor layer and a second conducting oxide layer formed over the ion storage layer. In some embodiments, the spectral tuning layer may be configured to change an infrared transmissivity of the adjustable window. Furthermore, the spectral tuning layer may be configured to toggle a solar heat gain ratio coefficient of the adjustable window between two or more solar heat gain ratio coefficients.
Abstract:
Methods to improve the reflection of light emitting devices are disclosed. A method consistent with the present disclosure includes forming a light generating layer over a site-isolated region of a substrate. Next, forming a first transparent conductive layer over the light generating layer. Forming a low refractive index material over the first transparent conductive layer, and in time, forming a second transparent conductive layer over the low refractive index material. Subsequently, forming a reflective material layer thereon. Accordingly, methods consistent with the present disclosure may form a plurality of light emitting devices in various site-isolated regions on a substrate.
Abstract:
Disclosed herein are systems, methods, and apparatus for forming a low emissivity panel. In various embodiments, a partially fabricated panel may be provided. The partially fabricated panel may include a substrate, a reflective layer formed over the substrate, and a top dielectric layer formed over the reflective layer such that the reflective layer is formed between the substrate and the top dielectric layer. The top dielectric layer may include tin having an oxidation state of +4. An interface layer may be formed over the top dielectric layer. A top diffusion layer may be formed over the interface layer. The top diffusion layer may be formed in a nitrogen plasma environment. The interface layer may substantially prevent nitrogen from the nitrogen plasma environment from reaching the top dielectric layer and changing the oxidation state of tin included in the top dielectric layer.
Abstract:
Provided is High Productivity Combinatorial (HPC) testing methodology of semiconductor substrates, each including multiple site isolated regions. The site isolated regions are used for testing different compositions and/or structures of barrier layers disposed over silver reflectors. The tested barrier layers may include all or at least two of nickel, chromium, titanium, and aluminum. In some embodiments, the barrier layers include oxygen. This combination allows using relative thin barrier layers (e.g., 5-30 Angstroms thick) that have high transparency yet provide sufficient protection to the silver reflector. The amount of nickel in a barrier layer may be 5-10% by weight, chromium—25-30%, titanium and aluminum—30%-35% each. The barrier layer may be co-sputtered in a reactive or inert-environment using one or more targets that include all four metals. An article may include multiple silver reflectors, each having its own barrier layer.
Abstract:
Embodiments provided herein describe low-e panels and methods for forming low-e panels. A transparent substrate is provided. A reflective layer is formed above the transparent substrate. A barrier layer is formed above the reflective layer. A nitride-containing layer is formed above the barrier layer. The nitride-containing layer has a thickness that is 1 nm or less. A over-coating layer is formed above the nitride-containing layer. The over-coating layer includes a different material than that of the nitride-containing layer.
Abstract:
Disclosed herein are systems, methods, and apparatus for forming low emissivity panels that may include a first substrate. The first substrate may have a first side and a second side. The low emissivity panels may also include a magnetic fluid layer deposited over the first side of the first substrate and a reflective layer deposited over the second side of the first substrate. The magnetic fluid layer may include magnetic particles. The reflective layer may include a conductive material configured to conduct an electrical current and generate a magnetic field. The magnetic field may be configured to change an orientation of the magnetic particles in the magnetic fluid layer and a transmissivity of the magnetic fluid layer within a visible spectrum. The low emissivity panels may also include a first bus and a second bus deposited along opposite edges of the reflective layer and electrically connected to the reflective layer.