摘要:
Set of compositions for preparing system-in-package type semiconductor device. The composition set consists of underfill composition for preparing underfill part and encapsulation resin composition for preparing resin encapsulation part. 1) A cured product of the underfill composition has a glass transition temperature, Tg, ≧100° C. and is the same with or differs from a Tg of a cured product of the encapsulation resin composition by ≦20° C. 2) Total linear expansion coefficient of the cured product of the underfill composition at a temperature not higher than (Tg−30)° C. and a linear expansion coefficient of the cured product of the encapsulation resin composition at a temperature not higher than (Tg−30)° C. is ≦42 ppm/° C. 3) A ratio of the linear expansion coefficient of the cured product of the encapsulation resin composition to the linear expansion coefficient of the cured product of the underfill composition ranges from 0.3 to 1.0.
摘要:
A set of compositions for preparing a system-in-package type semiconductor device, characterized in that the set of compositions consists of an underfill composition for preparing the underfill part and an encapsulation resin composition for preparing the resin encapsulation part, wherein 1) a cured product of the underfill composition has a glass transition temperature, Tg, which is 100° C. or higher and is the same with or differs from a Tg of a cured product of the encapsulation resin composition by 20° C. or smaller, 2) a total of a linear expansion coefficient of the cured product of the underfill composition at a temperature not higher than (Tg-30)° C. and a linear expansion coefficient of the cured product of the encapsulation resin composition at a temperature not higher than (Tg-30)° C. is 42 ppm/° C. or smaller, and 3) a ratio of the linear expansion coefficient of the cured product of the encapsulation resin composition to the linear expansion coefficient of the cured product of the underfill composition ranges from 0.3 to 1.0.
摘要:
A liquid epoxy resin composition comprising (A) a liquid epoxy resin (B) an amine curing agent (C) a nitrogen compound selected from the group consisting of organic acids salts of tertiary amines, amino acids, imino acids, and monoamine compounds having an alcoholic hydroxyl group in an amount of from 0.1 to 20 parts by weight per total 100 parts by weight of the components (A) and (B), and (D) an inorganic filler in an amount of from 50 to 900 parts by weight per 100 parts by weight of the component (A).
摘要:
A composition comprising (A) an epoxy resin, (B) a curing agent, (C) an inorganic filler having an average particle size of 0.1-10 μm and a maximum particle size of up to 75 μm, and (D) a surface-silylated silica having an average particle size of 0.005 μm to less than 0.1 μm is suited as a dam composition for use with a underfill material in the fabrication of multilayer semiconductor packages.
摘要:
A liquid epoxy resin composition comprising (A) a liquid epoxy resin, (B) an amine curing agent, and (C) an inorganic filler in an amount of from 50 to 900 parts by weight per 100 parts by weight of the component (A), wherein the component (B) is contained in such an amount that a molar ratio of epoxy groups of the component (A) to amino groups of the component (B), ranges from 0.6 to less than 1.0, provided that, if the component (B) includes an amine curing agent which is solid in the composition at a temperature of from room temperature to 150° C., a content of such an amine is 30 mol % or less, based on the component (B).
摘要:
Set of compositions for preparing system-in-package type semiconductor device. The composition set consists of underfill composition for preparing underfill part and encapsulation resin composition for preparing resin encapsulation part. 1) A cured product of the underfill composition has a glass transition temperature, Tg, ≧100° C. and is the same with or differs from a Tg of a cured product of the encapsulation resin composition by ≦20° C. 2) Total linear expansion coefficient of the cured product of the underfill composition at a temperature not higher than (Tg−30)° C. and a linear expansion coefficient of the cured product of the encapsulation resin composition at a temperature not higher than (Tg−30)° C. is ≦42 ppm/° C. 3) A ratio of the linear expansion coefficient of the cured product of the encapsulation resin composition to the linear expansion coefficient of the cured product of the underfill composition ranges from 0.3 to 1.0.
摘要:
A liquid epoxy resin composition comprising (A) a liquid epoxy resin; (B) an amine curing agent; (C) a nitrogen compound selected from the group consisting of organic acids salts of tertiary amines, amino acids, imino acids, and monoamine compounds having an alcoholic hydroxyl group in an amount of from 0.1 to 20 parts by weight per total 100 parts by weight of the components (A) and (B); and (D) an inorganic filler in an amount of from 50 to 900 parts by weight per 100 parts by weight of the component (A).
摘要:
The invention relates to a process for producing a semiconductor device in which a circuit substrate and a semiconductor chip are connected through a plurality of solder bump electrodes, said process comprising applying a non-cleaning type flux to at least a portion of a bonding pad in the circuit substrate and a semiconductor chip; applying an under-fill material to the circuit substrate or the semiconductor chip; positioning the semiconductor chip and the circuit substrate; and bonding the semiconductor chip and the circuit substrate through a thermocompression bonding, and a semiconductor device produced by the process. By using the process, since it is not necessary to add a flux component deteriorating the reliability of an under-fill material as the sealant to the under-fill material, reliability of the semiconductor device is not deteriorated. Further, since the intrusion step of thin film is not used, mounting can be conducted in a relatively short time.
摘要:
A liquid epoxy resin composition comprising: (A) a liquid epoxy resin; (B) an amine type curing agent; (C) a sulfur-containing phenol compound in an amount of from 1 to 20 parts by weight per total 100 parts by weight of the components (A) and (B); and (D) an inorganic filler in an amount of from 50 to 900 parts by weight per 100 parts by weight of the component (A).
摘要:
A liquid epoxy resin composition comprising (A) a liquid epoxy resin, (B) an aromatic amine curing agent, and (C) an inorganic filler having an average particle size of more than 5 μm in an amount of from 300 parts by weight to 1,000 parts by weight per 100 parts by weight of components (A) and (B) combined, has a low viscosity and a low coefficient of linear expansion and is suited for the encapsulation of semiconductor devices.