Liquefaction of sub-bituminous coal
    47.
    发明授权
    Liquefaction of sub-bituminous coal 失效
    次烟煤液化

    公开(公告)号:US4596650A

    公开(公告)日:1986-06-24

    申请号:US590175

    申请日:1984-03-16

    IPC分类号: C10G1/06 C10G1/00

    CPC分类号: C10G1/006

    摘要: Sub-bituminous coal is directly liquefied in two stages by use of a liquefaction solvent containing insoluble material as well as 850.degree. F.+ material and 850.degree. F.- material derived from the second stage, and controlled temperature and conversion in the second stage. The process is in hydrogen balance.

    摘要翻译: 次烟煤通过使用含有不溶性物质的液化溶剂以及衍生自第二阶段的850°F +材料和850°F的物质直接液化,在第二阶段中控制温度和转化率 。 该过程处于氢平衡。

    Preparation of reactive beta-dicalcium silicate
    48.
    发明授权
    Preparation of reactive beta-dicalcium silicate 失效
    反应性β-二硅酸钙的制备

    公开(公告)号:US4314980A

    公开(公告)日:1982-02-09

    申请号:US125406

    申请日:1980-02-28

    IPC分类号: C01B33/24

    CPC分类号: C01B33/24

    摘要: This invention relates to the preparation of fine particles of reactive beta-dicalcium silicate by means of a solid state process which comprises firing a mixture of calcium sulfate, silica and a reducing additive selected from the group consisting of calcium sulfide, carbon, carbon monoxide, methane and hydrogen, at a temperature of about 850.degree.-1000.degree. C. A carrier gas such as nitrogen or carbon dioxide may also be added, if desired. A high concentration of sulfur dioxide is a by-product of this process.

    摘要翻译: 本发明涉及通过固态方法制备反应性β-二硅酸二钙细颗粒,其包括硫酸钙,二氧化硅和还原添加剂的混合物的烧制,所述还原添加剂选自硫化钙,碳,一氧化碳, 甲烷和氢气,在约850℃-1000℃的温度下。如果需要,也可以加入载气如氮气或二氧化碳。 高浓度的二氧化硫是这个过程的副产品。