Process for profile extrusion of a polyester
    41.
    发明授权
    Process for profile extrusion of a polyester 失效
    聚酯型材挤出工艺

    公开(公告)号:US06632390B1

    公开(公告)日:2003-10-14

    申请号:US09560455

    申请日:2000-04-28

    IPC分类号: C08G6302

    摘要: In a process for producing a profile by profile extrusion, a melt of a polyester composition is extruded through a die to form a profile. The processability of the polyester composition is improved by the addition of a branching agent, which provides increased melt strength and increased high shear thinning. The polyester composition has an inherent viscosity of at least 0.65 dl/g. The diacid component of the polyester composition has from 100 to 98.0 mole percent of residues of a primary acid selected from terephthalic acid, naphthalenedicarboxylic acid, isophthalic acid and mixtures thereof. The glycol component of the polyester composition has from 100 to 98.0 mole percent of residues of a primary glycol selected from ethylene glycol, 1,4-cyclohexanedimethanol, diethylene glycol, neopentyl glycol, and mixtures thereof. The polyester composition has from 0.05 to 2.0 mole percent of residues of the branching agent selected from an acidic branching agent with a tri-functional or greater monomer, an alcoholic branching agent with a tri-functional or greater monomer, and mixtures thereof. The branching agent is present as part of either the diacid component or glycol component depending on whether the functionality is acidic or alcoholic, respectively.

    摘要翻译: 在通过型材挤出生产型材的方法中,通过模具挤出聚酯组合物的熔体以形成轮廓。 聚酯组合物的加工性通过加入支化剂得到改善,其提供增加的熔体强度和增加的高剪切变稀。 聚酯组合物的特性粘度至少为0.65dl / g。 聚酯组合物的二酸组分具有100至98.0摩尔%的选自对苯二甲酸,萘二甲酸,间苯二甲酸的伯酸残基及其混合物。 聚酯组合物的二醇组分具有100至98.0摩尔%的选自乙二醇,1,4-环己烷二甲醇,二甘醇,新戊二醇及其混合物的伯二醇残基。 所述聚酯组合物具有0.05至2.0摩尔%的选自具有三官能以上单体的酸性支化剂的支链剂残基,具有三官能以上单体的醇支化剂及其混合物。 分支剂分别作为二酸组分或二醇组分的一部分存在,这取决于官能度是分别是酸性还是醇类。