Process for producing a strengthened fiber assembly
    43.
    发明授权
    Process for producing a strengthened fiber assembly 有权
    加强纤维集合体的制造方法

    公开(公告)号:US6042890A

    公开(公告)日:2000-03-28

    申请号:US173822

    申请日:1998-10-16

    摘要: The invention relates to a process for producing a strengthened fiber assembly containing cellulosic fibers with the cellulose being present in the crystalline structure of cellulose II, by contacting the fiber assembly with an aqueous solution of N-methylmorpholine-N-oxide (NMMO) at elevated temperature and subsequently washing the fiber assembly, characterized in that contacting is effected in a manner that from the relation-947+0.30.times.log.sub.(10) t+0.046.times.T-3.53.times.C +645.times.log.sub.(10) Cwherein t indicates the time in minutes during which the fiber assembly is contacted with the aqueous NMMO solution, T indicates the temperature of the aqueous NMMO solution in .degree.C. and C is the concentration of NMMO in % by mass, based on the aqueous NMMO solution, a number in the range of 0.30 to 1.70 results with the proviso that the temperature T is smaller than 130.degree. C. and the concentration C ranges between 70 and 84 % by mass.

    摘要翻译: 本发明涉及一种生产包含纤维素纤维的增强纤维组合物的方法,纤维素存在于纤维素II的晶体结构中,通过使纤维组合物与升高的N-甲基吗啉-N-氧化物(NMMO)的水溶液接触 温度并随后洗涤纤维组件,其特征在于,以从947 + 0.30xlog(10)t + 0.046xT-3.53xC + 645xlog(10)C的关系式来进行接触,其中t表示以分钟为单位的时间 纤维组合物与NMMO水溶液接触,T表示NMMO水溶液的温度为DEG,C为NMMO浓度,以NMMO水溶液为基准,其数量范围为0.30 至1.70的结果,条件是温度T小于130℃,浓度C在70和84质量%之间。

    Concentrated aqueous dispersions of tetrafluoroethylene polymers, and
process for their preparation
    44.
    发明授权
    Concentrated aqueous dispersions of tetrafluoroethylene polymers, and process for their preparation 失效
    四氢氟乙烯聚合物浓缩水分散体及其制备方法

    公开(公告)号:US5219910A

    公开(公告)日:1993-06-15

    申请号:US916202

    申请日:1992-07-17

    摘要: Concentrated, aqueous, colloidal dispersions of tetrafluoroethylene polymers having a polymer solids content of 25 to 70% by weight, which comprise, as the dispersion stabilizer, an amine oxide of the formula ##STR1## in which R.sup.1 is an alkyl radical having 6 to 22 carbon atoms or a mixture of such alkyl radicals and R.sup.2 is an alkyl radical having 1 to 22 carbon atoms or a mixture of such alkyl radicals, and in which R.sup.1 and R.sup.2 are identical or different and 50 to 0% by weight of the alkyl radicals R.sup.1 and R.sup.2 can be replaced by alkenyl radicals having 6 to 22 carbon atoms and having 1 to 3 C.dbd.C double bonds, are obtained by concentration with addition of these dispersion stabilizers. The dispersions are used for impregnating yarns and textile sheet-like structures.