Honeycomb structure, method for producing the same, and exhaust emission purification apparatus
    81.
    发明授权
    Honeycomb structure, method for producing the same, and exhaust emission purification apparatus 有权
    蜂窝结构体及其制造方法以及排气净化装置

    公开(公告)号:US07833936B2

    公开(公告)日:2010-11-16

    申请号:US11712410

    申请日:2007-03-01

    IPC分类号: B01J23/00 B01J21/00 B01J20/00

    摘要: The present invention provides a method for producing a honeycomb structure which carries a catalyst component containing at least one element selected from the group consisting of alkali metals and alkaline earth metals and purifies exhaust emissions. The method of the invention includes: a starting material mixing step of mixing ceramic particles having a predetermined average particle size, fine particles being composed of the same material as the ceramic particles and having an average particle size smaller than the predetermined average particle size, and an erosion-resistant material or a precursor thereof which inhibits the catalyst component from eroding the ceramic particles more effectively than an oxide of the element contained in the ceramic particles, to prepare a puddle; a molding and firing step of molding the puddle into a molded body and firing the molded body to sinter the molded body and to allow a ceramic particle protection material composed of the erosion-resistant material or the precursor thereof to be present on the surface of the molded body; and a catalyst-carrying step of making the fired molded body to carry the catalyst component.

    摘要翻译: 本发明提供了一种蜂窝结构体的制造方法,该蜂窝结构体含有含有选自碱金属和碱土金属中的至少一种元素的催化剂成分,并净化废气排放物。 本发明的方法包括:将具有预定平均粒度的陶瓷颗粒混合的原料混合步骤,由与陶瓷颗粒相同的材料构成并具有小于预定平均粒度的平均粒径的细颗粒,以及 耐腐蚀材料或其前体,其抑制催化剂组分比陶瓷颗粒中所含元素的氧化物更有效地侵蚀陶瓷颗粒,以制备熔池; 模制和煅烧步骤,将熔池模制成型体,并烧制成型体以烧结成型体,并允许由抗侵蚀材料或其前体组成的陶瓷颗粒保护材料存在于 成型体; 以及使烧成的成型体携带催化剂成分的催化剂负载工序。

    IMAGE SENSOR AND METHOD FOR MANUFACTURING THE SAME
    83.
    发明申请
    IMAGE SENSOR AND METHOD FOR MANUFACTURING THE SAME 有权
    图像传感器及其制造方法

    公开(公告)号:US20090072122A1

    公开(公告)日:2009-03-19

    申请号:US12209000

    申请日:2008-09-11

    IPC分类号: H01L27/00

    CPC分类号: H01L27/14647

    摘要: An image sensor 1 has a substrate 2 and primary light-receiving pixels 4 arrayed in the direction of the surface of the substrate, and the primary light-receiving pixels are formed by laminating plural secondary light-receiving pixels 10, 20 and 30 which sense lights in different wavelength ranges, respectively, via at least sealing insulation layers 18 and 28 between adjacent secondary light-receiving pixels in the thickness direction. Each secondary light-receiving pixel includes a photoelectric conversion portion 14, 24, or 34 for photoelectrically converting the lights and a signal output portion 12, 22 or 32 for outputting signals from a thin film transistor 40 according to charges generated by the photoelectric conversion portion, and the active layer 48 of the thin film transistor is formed from an oxide semiconductor or organic semiconductor.

    摘要翻译: 图像传感器1具有在基板的表面方向排列的基板2和一次受光像素4,并且通过层叠感测的多个次级受光像素10,20和30来形成一次受光像素 通过至少在相邻的次级光接收像素之间的厚度方向上的密封绝缘层18和28分别在不同波长范围内的光。 每个次级光接收像素包括用于光电转换光的光电转换部分14,24或34以及用于根据由光电转换部分产生的电荷从薄膜晶体管40输出信号的信号输出部分12,22或32 并且薄膜晶体管的有源层48由氧化物半导体或有机半导体形成。

    Honeycomb structured body
    87.
    发明授权
    Honeycomb structured body 有权
    蜂窝结构体

    公开(公告)号:US07449427B2

    公开(公告)日:2008-11-11

    申请号:US11518998

    申请日:2006-09-12

    摘要: The honeycomb structured body of the present invention is a honeycomb structured body in which a plurality of porous ceramic members are combined with one another through an adhesive layer, each of the porous ceramic members having a plurality of cells which are allowed to penetrate in a longitudinal direction with a wall portion therebetween and either one end of which is sealed, with a catalyst supporting layer being adhered to the wall portion, wherein an average pore diameter of the porous ceramic member is larger than an average particle diameter of particles constituting the catalyst supporting layer, and when a pore diameter distribution of the porous ceramic member and a particle diameter distribution of particles constituting the catalyst supporting layer are drawn with the pore diameter and the particle diameter being on the same axis, a pore volume in an overlapped area of both the distributions is about 10% or less to the entire pore volume of the porous ceramic member.

    摘要翻译: 本发明的蜂窝结构体是蜂窝结构体,其中多个多孔陶瓷构件通过粘合剂层彼此结合,每个多孔陶瓷构件具有多个细胞,其允许纵向穿透 方向,其间具有壁部,并且其一端被密封,催化剂支撑层粘附到壁部,其中多孔陶瓷构件的平均孔径大于构成催化剂载体的颗粒的平均粒径 层,并且当多孔陶瓷构件的孔径分布和构成催化剂负载层的颗粒的粒径分布以孔径和粒径在同一轴线上被拉伸时,两者的重叠区域中的孔体积 该分布对于多孔陶瓷构件的整个孔体积为大约10%或更小。

    Honeycomb structure, method for producing the same, and exhaust emission purification apparatus
    88.
    发明申请
    Honeycomb structure, method for producing the same, and exhaust emission purification apparatus 有权
    蜂窝结构体及其制造方法以及排气净化装置

    公开(公告)号:US20070154728A1

    公开(公告)日:2007-07-05

    申请号:US11712410

    申请日:2007-03-01

    IPC分类号: B32B3/12 C04B33/32

    摘要: The present invention provides a method for producing a honeycomb structure which carries a catalyst component containing at least one element selected from the group consisting of alkali metals and alkaline earth metals and purifies exhaust emissions. The method of the invention includes: a starting material mixing step of mixing ceramic particles having a predetermined average particle size, fine particles being composed of the same material as the ceramic particles and having an average particle size smaller than the predetermined average particle size, and an erosion-resistant material or a precursor thereof which inhibits the catalyst component from eroding the ceramic particles more effectively than an oxide of the element contained in the ceramic particles, to prepare a puddle; a molding and firing step of molding the puddle into a molded body and firing the molded body to sinter the molded body and to allow a ceramic particle protection material composed of the erosion-resistant material or the precursor thereof to be present on the surface of the molded body; and a catalyst-carrying step of making the fired molded body to carry the catalyst component.

    摘要翻译: 本发明提供了一种蜂窝结构体的制造方法,该蜂窝结构体含有含有选自碱金属和碱土金属中的至少一种元素的催化剂成分,并净化废气排放物。 本发明的方法包括:将具有预定平均粒度的陶瓷颗粒混合的原料混合步骤,由与陶瓷颗粒相同的材料构成并具有小于预定平均粒度的平均粒径的细颗粒,以及 耐腐蚀材料或其前体,其抑制催化剂组分比陶瓷颗粒中所含元素的氧化物更有效地侵蚀陶瓷颗粒,以制备熔池; 模制和煅烧步骤,将熔池模制成型体,并烧制成型体以烧结成型体,并允许由抗侵蚀材料或其前体组成的陶瓷颗粒保护材料存在于 成型体; 以及使烧成的成型体携带催化剂成分的催化剂负载工序。

    Honeycomb structured body
    90.
    发明申请
    Honeycomb structured body 有权
    蜂窝结构体

    公开(公告)号:US20070028575A1

    公开(公告)日:2007-02-08

    申请号:US11496431

    申请日:2006-08-01

    IPC分类号: B01D39/20

    摘要: A honeycomb structured body of the present invention is a honeycomb structured body in which a plurality of porous ceramic members are combined with one another through an adhesive layer, each of the porous ceramic members having a plurality of cells which are allowed to penetrate in a longitudinal direction with a wall portion therebetween and either one end of which is sealed, with a catalyst supporting layer being adhered to the wall portion, wherein, supposing that the rate of the pore volume of pores having a pore diameter of 10 μm or less to the entire pore volume of the porous ceramic member is X1 (%), the porosity is Y1 (%) and the weight of the catalyst supporting layer is Z1 (g/l), these X1, Y1 and Z1 are allowed to satisfy the following expressions (1) and (2): X1≦20−Z1/10  (1), and Y1≧35+7Z1/40  (2) (where about 20≦Z1≦about 150).

    摘要翻译: 本发明的蜂窝结构体是蜂窝结构体,其中多个多孔陶瓷构件通过粘合剂层彼此结合,每个多孔陶瓷构件具有多个细胞,其允许纵向穿透 方向,其间具有壁部分,并且其一端被密封,催化剂支撑层粘附到壁部分,其中,假设孔径为10μm或更小的孔的孔体积相对于 多孔陶瓷构件的整个孔体积为X 1(%),孔隙率为Y 1(%),催化剂负载层的重量为Z < 1(g / l),这些X 1,Y 1和Z 1被允许满足下列表达式(1 )和(2):<?in-line-formula description =“In-line Formulas”end =“lead”?> X <1> <= 20 -Z 1 / 10(1)和<?in-line-formula description =“联机表单 ulae“end =”tail“?> <?in-line-formula description =”In-line formula“end =”lead“?> Y <1> = 35 + 7Z < / SUB> / 40(2)<?in-line-formula description =“In-line Formulas”end =“tail”?>(其中约20 <= Z <1> <= 150) 。