CPC分类号: C04B35/6365 , C04B26/285 , C04B35/185 , C04B35/63 , C04B35/64 , C04B38/0006 , C04B38/0022 , C04B2111/00793 , C04B2111/0081 , C04B2235/3217 , C04B2235/3218 , C04B2235/3418 , C04B2235/3463 , C04B2235/349 , C04B2235/36 , C04B2235/445 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/78 , C04B2235/788 , C04B2235/79 , C04B2235/80 , C04B2235/96 , C04B35/195 , C04B14/047 , C04B14/06 , C04B14/10 , C04B14/303 , C04B38/00 , C04B40/0268 , C04B38/0074
摘要: A method of forming a porous mullite composition of acicular mullite grains having improved properties is described, where the mullite is formed at some time in the presence of a fluorine containing gas. For example, it has been discovered that improved properties may result from heating the mullite to a high temperature in an atmosphere selected from the group consisting of water vapor, oxygen, an inert gas or mixtures thereof or forming the mullite composition from precursors having an Al/Si ratio of at most 2.95.
摘要翻译: 描述了一种形成具有改善性能的针状莫来石晶粒的多孔莫来石组合物的方法,其中在含氟气体存在下在某个时间形成莫来石。 例如,已经发现,在选自水蒸汽,氧气,惰性气体或其混合物的气氛中,将莫来石加热到高温可以产生改进的性能,或者由具有Al的前体形成莫来石组合物 / Si比至多为2.95。
-
公开(公告)号:US07485594B2
公开(公告)日:2009-02-03
申请号:US11799413
申请日:2007-05-01
申请人: Chandan Saha , Sharon Allen , Chan Han , Robert T. Nilsson , Arthur R. Prunier, Jr. , Aleksander J. Pyzik , Sten A. Wallin , Robin Ziebarth , Timothy J. Gallagher
发明人: Chandan Saha , Sharon Allen , Chan Han , Robert T. Nilsson , Arthur R. Prunier, Jr. , Aleksander J. Pyzik , Sten A. Wallin , Robin Ziebarth , Timothy J. Gallagher
IPC分类号: C04B35/00
CPC分类号: B01J23/10 , B01D39/2093 , B01J23/63 , B01J35/04 , B01J37/0215 , C04B35/185 , C04B35/6365 , C04B2235/3206 , C04B2235/3208 , C04B2235/322 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3409 , C04B2235/349 , C04B2235/449 , C04B2235/604 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/96 , C04B2235/9607 , F01N2330/06 , F01N2510/06 , F01N2510/0682
摘要: A porous mullite composition is made by forming a mixture of one or more precursor compounds having the elements present in mullite (e.g., clay, alumina, silica) and a property enhancing compound. The property enhancing compound is a compound having an element selected from the group consisting of Mg, Ca, Fe, Na, K, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, B, Y, Sc, La and combination thereof. The mixture is shaped and to form a porous green shape which is heated under an atmosphere having a fluorine containing gas to a temperature sufficient to form a mullite composition comprised substantially of acicular mullite grains that are essentially chemically bound.
摘要翻译: 通过形成具有莫来石(例如粘土,氧化铝,二氧化硅)和性能增强化合物中存在的元素的一种或多种前体化合物的混合物来制备多孔莫来石组合物。 性质增强化合物是具有选自Mg,Ca,Fe,Na,K,Ce,Pr,Nd,Sm,Eu,Gd,Tb,Dy,Ho,Er,Tm,Yb, Lu,B,Y,Sc,La及其组合。 混合物成型并形成多孔绿色形状,其在具有含氟气体的气氛下加热到足以形成基本上化学结合的基本上由针状莫来石颗粒组成的莫来石组合物的温度。
-
公开(公告)号:US20060197265A1
公开(公告)日:2006-09-07
申请号:US10551728
申请日:2004-04-23
申请人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
发明人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
CPC分类号: B01D53/885 , B01D53/944 , B01D71/02 , B01J21/12 , B01J21/16 , B01J23/002 , B01J23/02 , B01J23/10 , B01J23/63 , B01J23/78 , B01J35/002 , B01J35/1033 , B01J37/0018 , B01J37/0027 , B01J37/08 , B01J37/26 , B01J2523/00 , C04B35/185 , C04B35/64 , C04B38/00 , C04B2111/00793 , C04B2111/0081 , C04B2235/3201 , C04B2235/3206 , C04B2235/3208 , C04B2235/3217 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3272 , C04B2235/3409 , C04B2235/3418 , C04B2235/3445 , C04B2235/349 , C04B2235/449 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/78 , C04B2235/85 , C04B2235/96 , C04B2235/9607 , F01N3/022 , F01N3/0222 , F01N3/035 , F01N2330/06 , F01N2370/02 , C04B38/0022 , C04B38/0074 , C04B38/0645 , B01J2523/22 , B01J2523/31 , B01J2523/41 , B01J2523/842 , B01J2523/3725
摘要: A porous mullite composition is made by Forming a mixture of one or more precursor compounds having the elements present in mullite (e.g., clay, alumina, silica) and a property enhancing compound. The property enhancing compound is a compound having an element selected from the group consisting of Mg, Ca, Fe, Na, K, Ce, Pr, Nd, Sm, Eu, Gd, Th, Dy, Ho, Er, Tm, Yb, Lu, B, Y, Sc, La and combination thereof. The mixture is shaped and to form a porous green shape which is heated under an atmosphere having a fluorine containing gas to a temperature sufficient to form a mullite composition comprised substantially of acicular mullite grains that are essentially chemically bound.
-
公开(公告)号:US20070213207A1
公开(公告)日:2007-09-13
申请号:US11799413
申请日:2007-05-01
申请人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
发明人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
IPC分类号: C04B35/00 , C04B35/185 , B01J21/02
CPC分类号: B01J23/10 , B01D39/2093 , B01J23/63 , B01J35/04 , B01J37/0215 , C04B35/185 , C04B35/6365 , C04B2235/3206 , C04B2235/3208 , C04B2235/322 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3409 , C04B2235/349 , C04B2235/449 , C04B2235/604 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/96 , C04B2235/9607 , F01N2330/06 , F01N2510/06 , F01N2510/0682
摘要: A porous mullite composition is made by forming a mixture of one or more precursor compounds having the elements present in mullite (e.g., clay, alumina, silica) and a property enhancing compound. The property enhancing compound is a compound having an element selected from the group consisting of Mg, Ca, Fe, Na, K, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, B, Y, Sc, La and combination thereof. The mixture is shaped and to form a porous green shape which is heated under an atmosphere having a fluorine containing gas to a temperature sufficient to form a mullite composition comprised substantially of acicular mullite grains that are essentially chemically bound.
摘要翻译: 通过形成具有莫来石(例如粘土,氧化铝,二氧化硅)和性能增强化合物中存在的元素的一种或多种前体化合物的混合物来制备多孔莫来石组合物。 性质增强化合物是具有选自Mg,Ca,Fe,Na,K,Ce,Pr,Nd,Sm,Eu,Gd,Tb,Dy,Ho,Er,Tm,Yb, Lu,B,Y,Sc,La及其组合。 混合物成型并形成多孔绿色形状,其在具有含氟气体的气氛下加热到足以形成基本上化学结合的基本上由针状莫来石颗粒组成的莫来石组合物的温度。
-
公开(公告)号:US07528087B2
公开(公告)日:2009-05-05
申请号:US10551728
申请日:2004-04-23
申请人: Chandan Saha , Sharon Allen , Chan Han , Robert T. Nilsson , Arthur R. Prunier, Jr. , Aleksander J. Pyzik , Sten A. Wallin , Robin Ziebarth , Timothy J. Gallagher
发明人: Chandan Saha , Sharon Allen , Chan Han , Robert T. Nilsson , Arthur R. Prunier, Jr. , Aleksander J. Pyzik , Sten A. Wallin , Robin Ziebarth , Timothy J. Gallagher
IPC分类号: C04B35/00
CPC分类号: B01D53/885 , B01D53/944 , B01D71/02 , B01J21/12 , B01J21/16 , B01J23/002 , B01J23/02 , B01J23/10 , B01J23/63 , B01J23/78 , B01J35/002 , B01J35/1033 , B01J37/0018 , B01J37/0027 , B01J37/08 , B01J37/26 , B01J2523/00 , C04B35/185 , C04B35/64 , C04B38/00 , C04B2111/00793 , C04B2111/0081 , C04B2235/3201 , C04B2235/3206 , C04B2235/3208 , C04B2235/3217 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3272 , C04B2235/3409 , C04B2235/3418 , C04B2235/3445 , C04B2235/349 , C04B2235/449 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/78 , C04B2235/85 , C04B2235/96 , C04B2235/9607 , F01N3/022 , F01N3/0222 , F01N3/035 , F01N2330/06 , F01N2370/02 , C04B38/0022 , C04B38/0074 , C04B38/0645 , B01J2523/22 , B01J2523/31 , B01J2523/41 , B01J2523/842 , B01J2523/3725
摘要: A porous mullite composition is made by Forming a mixture of one or more precursor compounds having the elements present in mullite (e.g., clay, alumina, silica) and a property enhancing compound. The property enhancing compound is a compound having an element selected from the group consisting of Mg, Ca, Fe, Na, K, Ce, Pr, Nd, Sm, Eu, Gd, Th, Dy, Ho, Er, Tm, Yb, Lu, B, Y, Sc, La and combination thereof. The mixture is shaped and to form a porous green shape which is heated under an atmosphere having a fluorine containing gas to a temperature sufficient to form a mullite composition comprised substantially of acicular mullite grains that are essentially chemically bound.
摘要翻译: 通过形成具有莫来石(例如,粘土,氧化铝,二氧化硅)和性能增强化合物中存在的元素的一种或多种前体化合物的混合物制备多孔莫来石组合物。 特性增强化合物是具有选自Mg,Ca,Fe,Na,K,Ce,Pr,Nd,Sm,Eu,Gd,Th,Dy,Ho,Er,Tm,Yb, Lu,B,Y,Sc,La及其组合。 混合物成型并形成多孔绿色形状,其在具有含氟气体的气氛下加热到足以形成基本上化学结合的基本上由针状莫来石颗粒组成的莫来石组合物的温度。
-
公开(公告)号:US20070203315A1
公开(公告)日:2007-08-30
申请号:US11799414
申请日:2007-05-01
申请人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
发明人: Chandan Saha , Sharon Allen , Chan Han , Robert Nilsson , Arthur Prunier , Aleksander Pyzik , Sten Wallin , Robin Ziebarth , Timothy Gallagher
IPC分类号: C08G77/06
CPC分类号: B01D53/885 , B01D53/944 , B01D71/02 , B01J21/12 , B01J21/16 , B01J23/002 , B01J23/02 , B01J23/10 , B01J23/63 , B01J23/78 , B01J35/002 , B01J35/1033 , B01J37/0018 , B01J37/0027 , B01J37/08 , B01J37/26 , B01J2523/00 , C04B35/185 , C04B35/64 , C04B38/00 , C04B2111/00793 , C04B2111/0081 , C04B2235/3201 , C04B2235/3206 , C04B2235/3208 , C04B2235/3217 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3272 , C04B2235/3409 , C04B2235/3418 , C04B2235/3445 , C04B2235/349 , C04B2235/449 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/78 , C04B2235/85 , C04B2235/96 , C04B2235/9607 , F01N3/022 , F01N3/0222 , F01N3/035 , F01N2330/06 , F01N2370/02 , C04B38/0022 , C04B38/0074 , C04B38/0645 , B01J2523/22 , B01J2523/31 , B01J2523/41 , B01J2523/842 , B01J2523/3725
摘要: A porous mullite composition is made by forming a mixture of one or more precursor compounds having the elements present in mullite (e.g., clay, alumina, silica) and a property enhancing compound. The property enhancing compound is a compound having an element selected from the group consisting of Mg, Ca, Fe, Na, K, Ce, Pr, Nd, Sm, Eu, Gd, Th, Dy, Ho, Er, Tm, Yb, Lu, B, Y, Sc, La and combination thereof. The mixture is shaped and to form a porous green shape which is heated under an atmosphere having a fluorine containing gas to a temperature sufficient to form a mullite composition comprised substantially of acicular mullite grains that are essentially chemically bound.
摘要翻译: 通过形成具有莫来石(例如粘土,氧化铝,二氧化硅)和性能增强化合物中存在的元素的一种或多种前体化合物的混合物来制备多孔莫来石组合物。 特性增强化合物是具有选自Mg,Ca,Fe,Na,K,Ce,Pr,Nd,Sm,Eu,Gd,Th,Dy,Ho,Er,Tm,Yb, Lu,B,Y,Sc,La及其组合。 混合物成型并形成多孔绿色形状,其在具有含氟气体的气氛下加热到足以形成基本上化学结合的基本上由针状莫来石颗粒组成的莫来石组合物的温度。
-
公开(公告)号:US20050115214A1
公开(公告)日:2005-06-02
申请号:US10477833
申请日:2003-03-24
IPC分类号: F01N3/02 , B01D39/20 , B01D53/94 , B01J21/06 , C01B33/26 , C04B26/28 , C04B35/18 , C04B35/185 , C04B35/636 , C04B35/64 , C04B38/00 , F01N3/10 , F01N3/28
CPC分类号: C04B35/6365 , C04B26/285 , C04B35/185 , C04B35/63 , C04B35/64 , C04B38/0006 , C04B38/0022 , C04B2111/00793 , C04B2111/0081 , C04B2235/3217 , C04B2235/3218 , C04B2235/3418 , C04B2235/3463 , C04B2235/349 , C04B2235/36 , C04B2235/445 , C04B2235/658 , C04B2235/661 , C04B2235/72 , C04B2235/77 , C04B2235/78 , C04B2235/788 , C04B2235/79 , C04B2235/80 , C04B2235/96 , C04B35/195 , C04B14/047 , C04B14/06 , C04B14/10 , C04B14/303 , C04B38/00 , C04B40/0268 , C04B38/0074
摘要: A method of forming a porous mullite composition of acicular mullite grains having improved properties is described, where the mullite is formed at some time in the presence of a fluorine containing gas. For example, it has been discovered that improved properties may result from heating the mullite to a high temperature in an atmosphere selected from the group consisting of water vapor, oxygen, an inert gas or mixtures thereof or forming the mullite composition from precursors having an AL/Si ratio of at most 2.95.
摘要翻译: 描述了一种形成具有改进性能的针状莫来石晶粒的多孔莫来石组合物的方法,其中在含氟气体存在下在某个时间形成莫来石。 例如,已经发现,在由水蒸气,氧气,惰性气体或其混合物组成的组中选择的气氛中将莫来石加热到高温可以产生改进的性质,或者由具有AL的前体形成莫来石组合物 / Si比至多为2.95。
-
-
-
-
-
-