METHOD FOR PREPARING DENDRIMER-MODIFIED, MAGNETIC FINE PARTICLES
    2.
    发明申请
    METHOD FOR PREPARING DENDRIMER-MODIFIED, MAGNETIC FINE PARTICLES 审中-公开
    制备改性改性的磁性颗粒的方法

    公开(公告)号:US20110057145A1

    公开(公告)日:2011-03-10

    申请号:US12876562

    申请日:2010-09-07

    IPC分类号: H01F1/00

    CPC分类号: H01F1/42

    摘要: There is provided a method for preparing dendrimer-modified magnetic fine particles wherein such particles can be made within a shorter time and more inexpensively than in the above-stated prior art processes and lot-to-lot variations in properties are lessened. The method for preparing dendrimer-fixed magnetic fine particles comprises the steps of providing magnetic particles having a functional group at a surface thereof, providing a dendrimer having a functional group at a base end portion thereof and synthesized to a desired generation and binding the functional group of the magnetic particles and the functional group of the dendrimer directly or indirectly through a crosslinking agent.

    摘要翻译: 提供了一种制备树枝状聚合物改性的磁性细颗粒的方法,其中这种颗粒可以在比上述现有技术方法更短的时间和更廉价的情况下制备,并且批次间的性质变化减少。 制备树枝状大分子固定磁性微粒的方法包括以下步骤:在其表面提供具有官能团的磁性颗粒,提供在其基端部分具有官能团的树枝状聚合物,并合成所需的一代并结合官能团 的磁性颗粒和树枝状聚合物的官能团直接或间接地通过交联剂。

    Circuit inspection method, method of manufacturing liquid-crystal display, and circuit inspection apparatus
    3.
    发明授权
    Circuit inspection method, method of manufacturing liquid-crystal display, and circuit inspection apparatus 有权
    电路检查方法,液晶显示器的制造方法以及电路检查装置

    公开(公告)号:US07209843B2

    公开(公告)日:2007-04-24

    申请号:US11120942

    申请日:2005-05-04

    IPC分类号: G06F19/00 G01R19/00 G01R31/00

    CPC分类号: G09G3/006 G09G3/3648

    摘要: A circuit inspection method includes supplying electric charges to a first, second, and third electric charge holding electrodes in an electric circuit; outputting the electric charges held in the first electric charge holding electrode after a predetermined period of time from supplying of the electric charges; changing voltages of the first and second scan lines to a drive voltage to output the electric charges held in the second electric charge holding electrode; and determining whether an electric charge writing function and an electric charge holding function of the second electric charge holding electrode are good or not based on a quantity of the supplied electric charges and a quantity of the electric charges output from the second electric charge holding electrode.

    摘要翻译: 电路检查方法包括向电路中的第一,第二和第三电荷保持电极提供电荷; 在从所述电荷供给经过预定时间之后,输出保持在所述第一电荷保持电极中的电荷; 将第一和第二扫描线的电压改变为驱动电压,以输出保持在第二电荷保持电极中的电荷; 以及基于所提供的电荷的量和从第二电荷保持电极输出的电荷的量来确定第二电荷保持电极的电荷写入功能和电荷保持功能是否良好。

    Method and device for testing array substrate
    4.
    发明申请
    Method and device for testing array substrate 有权
    阵列基板测试方法及装置

    公开(公告)号:US20050204219A1

    公开(公告)日:2005-09-15

    申请号:US11063748

    申请日:2005-02-24

    摘要: A method and a device for testing an array substrate for a liquid crystal display that allow time for testing to be reduced are provided. An array substrate is divided into two test blocks, and two scanning signal lines in total, one from each of the test blocks, are selected and tested at a time, so that the addresses of possible defective pixels are specified. Then, the array substrate is divided into three test blocks, and three scanning signal lines in total, one from each of the test blocks, are selected and re-tested at a time, so that the addresses of possible defective pixels are specified. Then, the address of a pixel common between the first testing and re-testing is specified as a defective address.

    摘要翻译: 提供了一种用于测试液晶显示器用阵列基板的方法和装置,其允许测试时间减少。 阵列基板被分成两个测试块,并且每次测试块中选择和测试总共两个扫描信号线,每个测试块中的一个,从而指定可能的缺陷像素的地址。 然后,将阵列基板分割为三个测试块,总共选择三个扫描信号线,每个测试块中的一条,一次重新测试,从而指定可能的缺陷像素的地址。 然后,将第一测试和重新测试之间共同的像素的地址指定为缺陷地址。

    Glass composition for magnetic disk substrates and magnetic disk
substrate
    5.
    发明授权
    Glass composition for magnetic disk substrates and magnetic disk substrate 失效
    用于磁盘基板和磁盘基板的玻璃组合物

    公开(公告)号:US5691256A

    公开(公告)日:1997-11-25

    申请号:US773260

    申请日:1996-12-23

    摘要: A glass composition for magnetic disk substrates comprising as oxides: from 66 to 80% by weight of SiO.sub.2, from 5 to 15% by weight of Al.sub.2 O.sub.3, from 3 to 8.5% by weight of Li.sub.2 O, from 0 to 3% by weight of Na.sub.2 O, from 0 to 3% by weight of K.sub.2 O, from 0.5 to 8% by weight of TiO.sub.2, from 3.5 to 8% by weight of ZrO.sub.2, from 0.5 to 3% by weight of P.sub.2 O.sub.5, from 0 to 2% by weight of Sb.sub.2 O.sub.3, and from 0 to 2% by weight of As.sub.2 O.sub.3, and having a theoretical optical basicity of 0.548 or less; a magnetic disk substrate which is prepared by forming and polishing the above glass composition, followed by chemically strengthening the polished substrate by ion exchange or by forming, heat treating, and polishing the above composition and contains Li.sub.2 O.multidot.2SiO.sub.2 and/or spodumene as the main crystalline phase. The glass composition for magnetic disk substrates can easily be formed, can easily be polished after crystallization of the glass by heat treatment or chemically strengthened by ion exchange of the glass after forming and polishing, and is used for preparing magnetic disk substrates which has excellent chemical durability, mechanical strength, heat resistance, surface flatness, and surface smoothness, and shows little degradation of magnetic film characteristics by alkali migration.

    摘要翻译: 一种用于磁盘衬底的玻璃组合物,其包含氧化物:66至80重量%的SiO 2,5至15重量%的Al 2 O 3,3至8.5重量%的Li 2 O,0至3重量%的Na 2 O ,0〜3重量%的K 2 O,0.5〜8重量%的TiO 2,3.5〜8重量%的ZrO 2,0.5〜3重量%的P 2 O 5,0〜2重量%的Sb 2 O 3 ,0〜2重量%的As2O3,理论光学碱度为0.548以下; 通过形成和研磨上述玻璃组合物制备的磁盘基片,然后通过离子交换或通过成形,热处理和抛光上述组合物化学强化抛光的基片,并含有Li 2 O x 2 SiO 2和/或锂辉石作为主晶相 。 用于磁盘基板的玻璃组合物可以容易地形成,可以通过热处理在玻璃结晶后容易地进行抛光或者在成形和抛光后通过离子交换玻璃进行化学强化,并用于制备具有优异化学性质的磁盘基片 耐久性,机械强度,耐热性,表面平坦性和表面平滑性,并且通过碱迁移显示出很小的磁性膜特性劣化。

    Composition for producing low temperature co-fired substrate
    6.
    发明授权
    Composition for producing low temperature co-fired substrate 失效
    用于生产低温共烧基材的组合物

    公开(公告)号:US5468694A

    公开(公告)日:1995-11-21

    申请号:US156059

    申请日:1993-11-22

    摘要: A novel crystallizable glass composition for producing a novel low temperature co-fired glass-ceramic substrate having patterns of a low electrical-resistance conductor such as Ag, Ag-Pd, Au, and/or Cu is obtained. Being subjected to a firing process, the novel crystallizable glass can precipitate mullite as main crystalline phase, and at least one subordinate crystalline phase among forsterite, spinel, sapphirine, and similar crystalline phases. And also, the novel crystallizable glass powder composition with a inorganic filler as external additive having a minimum of 1.4 m.sup.2 /g. of mean specific surface area can precipitate both mullite phase and cordierite phase. The mixing weight ratio of the filler to the crystallizable glass powder is from 0.1/99.9 to 20/80. The crystallizable glass composition comprises following oxide components expressed in terms of percent by weight on the oxide basis; 45-58% of Al.sub.2 O.sub.3, 20-35% of SiO.sub.2, 5-15% of B.sub.2 O.sub.3, 5-20% of MgO, and 0-4% of alkali metal oxide. The substrates produced from the above compositions have high flexural strength, low dielectric constant, low loss factor, and controllable thermal expansion coefficient of ranging from about 30 to about 70.times.10.sup.- 7 /.degree.C. As for the substrate containing both mullite phase and cordierite phase, as the substrate has a low thermal expansion coefficient, it can be combined with AlN to produce a composite structure package.

    摘要翻译: 获得了具有诸如Ag,Ag-Pd,Au和/或Cu等低电阻导体图形的新型低温共烧玻璃陶瓷基板的可结晶玻璃组合物。 经过焙烧处理后,新型可结晶玻璃可以将莫来石沉淀为主晶相,并在镁橄榄石,尖晶石,蓝宝石和类似结晶相中至少存在一个以下结晶相。 另外,作为外部添加剂的无机填料的新型可结晶玻璃粉末组合物的最小值为1.4m 2 / g。 的平均比表面积可以沉淀莫来石相和堇青石相。 填料与可结晶玻璃粉末的混合重量比为0.1 / 99.9〜20/80。 可结晶玻璃组合物包含以氧化物为基准的以重量百分比表示的以下氧化物组分; 45-58%的Al2O3,20-35%的SiO2,5-15%的B2O3,5-20%的MgO和0-4%的碱金属氧化物。 由上述组合物制备的基材具有约30至约70×10 -7 /℃范围内的高弯曲强度,低介电常数,低损耗因数和可控热膨胀系数。对于含有莫来石相和堇青石相的基材 由于基板具有低的热膨胀系数,因此可以与AlN组合以产生复合结构封装。

    MICROFLUIDIC DEVICE FOR TRAPPING SINGLE CELL
    7.
    发明申请
    MICROFLUIDIC DEVICE FOR TRAPPING SINGLE CELL 有权
    用于捕获单细胞的微流体装置

    公开(公告)号:US20100240041A1

    公开(公告)日:2010-09-23

    申请号:US12670990

    申请日:2008-07-31

    IPC分类号: C12Q1/68 C12M1/00 C12N5/00

    摘要: It is to provide a microfluidic device which separates and captures with high efficiency a large amount of cells in a sample at one-cell level without damaging the cells by utilizing a microfabrication technology. The device sequentially comprises: an upper substrate consisting of a plastic plate provided with a groove for forming a microchannel communicating a sample-supply opening and a sample-discharge opening; a plastic upper flat plate forming the microchannel by cooperating with the upper substrate, the plate being provided with an aperture for a micromesh; a holding plate holding a plastic micromesh having a plurality of micro through-pores for capturing cells; a plastic lower flat plate provided with an aperture for suctioning; and a lower substrate consisting of a plastic flat plate provided with a groove for forming a suction channel, wherein the micro through-pores for capturing cells of the micromesh have an inverted mortar-like shape or a cylindrical shape, and wherein the upper flat plate is constituted by a softer plastic as compared to the upper substrate.

    摘要翻译: 它提供了一种微流体装置,其以单细胞水平高效地分离和捕获样品中的大量细胞,而不通过利用微细加工技术损伤细胞。 所述装置依次包括:上基板,由具有沟槽的塑料板构成,所述槽用于形成连通供样开口的微通道和采样排出口; 通过与上基板配合形成微通道的塑料上平板,该板设置有微孔的孔; 保持板,其保持具有用于捕获细胞的多个微通孔的塑料微镜; 一个塑料下平板设有一个用于抽吸的孔; 以及由设置有用于形成吸引通道的槽的塑料平板构成的下基板,其中,用于捕获微胶粒的细胞的微通孔具有倒立的砂浆状或圆筒形状,并且其中上平板 由与上基板相比较软的塑料构成。

    Inspection method of array board and inspection equipment thereof
    9.
    发明授权
    Inspection method of array board and inspection equipment thereof 失效
    阵列板检查方法及其检测设备

    公开(公告)号:US07269051B2

    公开(公告)日:2007-09-11

    申请号:US11297305

    申请日:2005-12-08

    申请人: Tomoyuki Taguchi

    发明人: Tomoyuki Taguchi

    IPC分类号: G11C11/24

    摘要: The present invention provides an inspection method of an array board and an inspection equipment thereof, which can detect a disconnection failure of a gate line even if electric potentials are applied from both ends of the gate line.