Abstract:
Numerous embodiments of methods and apparatus for marking articles are disclosed. In one embodiment, a method of marking an article includes providing an article having a preliminary visual appearance; modifying a region of the article; and directing a plurality of optical pulses into the modified region of the article. The plurality of optical pulses can be configured to produce a visible mark on the article. Generally, the mark can be characterized as having a modified visual appearance different from the preliminary visual appearance.
Abstract:
An internal feature can be laser machined in strengthened glass sheets or panels by first laser machining a first scribe in a first surface proximate to the internal feature to be laser machined. The internal feature can be then laser machined by positioning a beam waist of a laser beam proximate to an opposite second surface by focusing the laser beam through the strengthened glass panel from the first surface. The internal feature is laser machined by repositioning the beam waist from the second surface to the first surface while removing material from a kerf surrounding the internal feature. When the laser beam waist is finally positioned proximate to the first surface material, the internal shape formed by the laser machining is easily and cleanly removed from the surrounding glass.
Abstract:
An internal feature can be laser machined in strengthened glass sheets or panels by first laser machining a first scribe in a first surface proximate to the internal feature to be laser machined. The internal feature can be then laser machined by positioning a beam waist of a laser beam proximate to an opposite second surface by focusing the laser beam through the strengthened glass panel from the first surface. The internal feature is laser machined by repositioning the beam waist from the second surface to the first surface while removing material from a kerf surrounding the internal feature. When the laser beam waist is finally positioned proximate to the first surface material, the internal shape formed by the laser machining is easily and cleanly removed from the surrounding glass.
Abstract:
The present invention is a method for separating a workpiece from a common substrate. It includes the steps of providing the workpiece, generating, within a beam source, a beam of laser pulses configured to modify a portion of the workpiece, determining a depth for creating a modified region based upon a characteristic of the workpiece and modifying a plurality of regions within the workpiece to form a plurality of modified regions. Modifying the plurality of regions includes directing the beam of laser pulses from an output of the beam source onto the workpiece, causing relative motion between the workpiece and the output of the beam source while directing the beam of laser pulses onto workpiece, and modifying a characteristic of the pulses of the beam upon generating a number of pulses which generally correspond to creating the modified regions to the determined depth.
Abstract:
The present invention is a method for separating a workpiece from a common substrate. It includes the steps of providing the workpiece, generating, within a beam source, a beam of laser pulses configured to modify a portion of the workpiece, determining a depth for creating a modified region based upon a characteristic of the workpiece and modifying a plurality of regions within the workpiece to form a plurality of modified regions. Modifying the plurality of regions includes directing the beam of laser pulses from an output of the beam source onto the workpiece, causing relative motion between the workpiece and the output of the beam source while directing the beam of laser pulses onto workpiece, and modifying a characteristic of the pulses of the beam upon generating a number of pulses which generally correspond to creating the modified regions to the determined depth.
Abstract:
A method for laser processing provides a coating material (130) applied to a rough surface (42) of a substrate (44) to mitigate adverse optical effects that would be caused by roughness of the surface (42). Laser pulses (52) of the laser output of suitable parameters can be directed and focused to internally mark the substrate (44) material without damaging the rough surface (42) after passing through the coating material (130).