摘要:
Non-free flowable, non-dusting molding powders with a bulk density of more than 450 g/l are obtained when a suspension polymer of tetrafluoroethylene with a content of 0.01 to 1% by weight of units of at least one perfluoro(alkyl-vinyl) ether is ground to a particle diameter of 10 to 50 .mu.m and agglomerated in water.
摘要:
The invention relates to solutions of fluoropolymers which preferably contain carbonate groups, in solvents of the general formula (I) ##STR1## These solutions are suitable, in particular, for the production of membranes for liquid permeation processes, such as electrolysis.
摘要:
Fluorine-containing emulsifiers can be removed from fluoropolymer dispersions by adding to the dispersion a non ionic emulsifier, removing the fluorine-containing emulsifier by contact with an anion exchanger and separating the dispersion from the anion exchanger. The resulting dispersions can be concentrated and used for coating applications.
摘要:
Solutions of copolymers of the tetrafluoroethylene/ethylene typeCopolymer solutions comprising tetrafluoroethylene, ethylene and, as appropriate, further .alpha.-olefinic monomers in low-molecular-weight polymers of chlorotrifluoroethylene are described. They can be used for coatings, impregnations, cast films and for the production of fibers and filaments by gel spinning.
摘要:
The present invention provides a process of reducing the amount of fluorinated emulsifier in an aqueous fluoropolymer dispersion by contacting the aqueous fluoropolymer dispersion with an anion exchange resin in a non-fixed resin bed, the process comprising: (a) mixing the aqueous fluoropolymer dispersion with an effective amount of a surfactant so as to stabilize the fluoropolymer dispersion while being contacted with the anion exchange resin; (b) contacting the aqueous fluoropolymer dispersion with an anion exchange resin by agitating the aqueous fluoropolymer dispersion with an effective amount of anion exchange resin for a time of less than 4 hours to reduce the amount of fluorinated emulsifier in the aqueous fluoropolymer dispersion to a desired level; and (c) separating the anion exchange resin from the aqueous fluoropolymer dispersion.
摘要:
Polymerizing tetrafluoroethylene with modifying amounts of a perfluoro(alkyl vinyl ether) at temperatures below 60.degree. C. using permanganate or similar initiators by the suspension process and milling the raw polymer to an average particle size of from 10 to 50 .mu.m gives molding powders which are suitable for the preform free-sintering technique.
摘要:
The present invention provides a method of recovering a fluorinated acid surfactant or salt thereof from adsorbent particles to which said fluorinated acid surfactant has been adsorbed. The method comprises mixing adsorbent particles having adsorbed fluorinated acid surfactant or salt thereof with an alcohol and optionally an acid. The mixture is generally heated to cause esterification of the fluorinated acid surfactant or salt thereof with the alcohol so as to form an ester derivative of the fluorinated acid surfactant, distilling the mixture to form a distillate comprising the ester derivative, separating the ester derivative from the distillate and optionally feeding the remainder of the distillate back into the mixture.
摘要:
Labile end groups in fluorinated thermoplastics, in particular carboxyl and acid fluoride groups, are converted into carboxamide groups when the polymer is treated with an aqueous, ammonia-containing solution. The after-treated products have a pale color, do not cause corrosion during processing and can easily be taken from the molds in transfer molding.
摘要:
The present invention provides an aqueous fluoropolymer dispersion comprising a melt processible fluoropolymer in an amount of at least 25% by weight based on the weight of the aqueous fluoropolymer dispersion and a fluorinated surfactant having a molecular weight of not more than 1000 g/mol in an amount of not more than 100 ppm, preferably less than 50 ppm, more preferably less than 25 ppm and most preferably less than 10 ppm based on the weight of fluoropolymer solids or being free of said fluorinated surfactant. The aqueous fluoropolymer dispersion has a conductivity of at least 200 μS/cm, preferably at least 500 μS/cm and more preferably at least 1000 μS/cm.