公开(公告)号:US10457837B2
公开(公告)日:2019-10-29
申请号:US15855268
申请日:2017-12-27
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Yuan-Chang Huang , Ya-I Hsu , Yi-Che Su , Wei-Cheng Tang , Shu-Yun Chien
IPC: C09D183/10 , C08G81/00 , C08G77/445
Abstract: The embodiments of the present disclosure provide a coating composition, including: polysilsesquioxane polymer modified organic resin represented by Formula (1): Wherein, R1 is C3-12 epoxy group, C3-12 acrylate group, C3-12 alkylacryloxy group, C3-12 aminoalkyl group, C3-12 isocyanate-alkyl group, C3-12 alkylcarboxylic acid group, C3-12 alkyl halide group, C3-12 mercaptoalkyl group, C3-12 alkyl group, or C3-12 alkenyl group; R2 is half oxygen(O1/2), hydroxyl group, C1-8 alkyl group, or C1-8 alkoxy group; R3 is halide group, C1-8 alkyl halide group, C1-8 alkoxy group, C1-12 alkyl group, or C5-20 aromatic ring; R4 is hydrogen or C1-8 alkyl group; R5 is modified or unmodified carbonyl compound moiety; n is a positive integer from 1 to 200; m is a positive integer from 10 to 500, and s is an integer from 0 to 250.
-
公开(公告)号:US20170158802A1
公开(公告)日:2017-06-08
申请号:US15273724
申请日:2016-09-23
Applicant: Industrial Technology Research Institute
Inventor: Wen-Pin Chuang , Yi-Che Su , Yun-Ya Huang , Yuung-Ching Sheen , Chao-Chieh Chiang
CPC classification number: C08G18/14 , C08G18/0871 , C08G18/165 , C08G18/4081 , C08G18/4825 , C08G18/6492 , C08G18/7664 , C08G2101/0083 , C08J9/0061 , C08J2205/044 , C08J2375/08 , C08J2497/00
Abstract: A bio-polyol composition and a bio-polyurethane foam are provided. The bio-polyol composition includes polyol, a surface-modified lignin, and a surfactant represented by formula 1. wherein R is represented by CnH2n+1, n is an integer of 0 to 3; x/y is between 5 and 13; a is an integer of 1 to 100; b is an integer of 1 to 100.
-
公开(公告)号:US10676645B2
公开(公告)日:2020-06-09
申请号:US16046423
申请日:2018-07-26
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Yuan-Chang Huang , Yi-Che Su , Shu-Yun Chien , Hong-Yuan Lian , Huai-Kuang Fu , Pang-Hung Liu
IPC: C09D183/06 , F16L59/00 , C09D5/00 , C09D7/65 , C09D183/04 , C09D7/45 , C08G77/20
Abstract: A method of forming a thermal insulation porous film includes mixing 100 parts by weight of polysilsesquioxane-containing polymer, 20 to 75 parts by weight of surfactant, and 20 to 2000 parts by weight of solvent to form a thermal insulation coating material, wherein the polysilsesquioxane-containing polymer in the thermal insulation coating material is tube-shaped or sheet-shaped. The thermal insulation coating material is coated on a substrate, and then dried and sintered to form a thermal insulation porous film.
-
公开(公告)号:US09695333B2
公开(公告)日:2017-07-04
申请号:US14807603
申请日:2015-07-23
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Wei-Cheng Tang , Su-Mei Chen Wei , Yi-Che Su , Ya-I Hsu , Yi-Tzu Peng
IPC: C08L63/00 , C08L67/00 , C09D163/00 , C08G59/32 , C08G59/42
CPC classification number: C09D163/00 , C08G59/32 , C08G59/4215 , C08G59/4276
Abstract: A resin composition formed by reacting a polyester-polyacid oligomer with a poly-epoxy oligomer is provided. The functionality of the resin composition is between 4 and 10. The weight average molecular weight of the resin composition is between 3,000 and 20,000 g/mol.
-
公开(公告)号:US10696867B2
公开(公告)日:2020-06-30
申请号:US16743228
申请日:2020-01-15
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Yuan-Chang Huang , Yi-Che Su , Shu-Yun Chien , Hong-Yuan Lian , Huai-Kuang Fu , Pang-Hung Liu
IPC: C09D183/06 , F16L59/00 , C09D5/00 , C09D7/65 , C09D183/04 , C09D7/45 , C08G77/20
Abstract: A method of forming a thermal insulation porous film includes mixing 100 parts by weight of polysilsesquioxane-containing polymer, 20 to 75 parts by weight of surfactant, and 20 to 2000 parts by weight of solvent to form a thermal insulation coating material, wherein the polysilsesquioxane-containing polymer in the thermal insulation coating material is tube-shaped or sheet-shaped. The thermal insulation coating material is coated on a substrate, and then dried and sintered to form a thermal insulation porous film.
-
公开(公告)号:US10428229B2
公开(公告)日:2019-10-01
申请号:US15856475
申请日:2017-12-28
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Yeu-Kuen Wei , Shu-Yun Chien , Su-Mei Chen Wei , Yi-Che Su
IPC: C09D7/65 , C09D5/00 , C08L83/12 , C08G77/388 , C08G77/50 , C09D7/63 , C09D7/20 , C09D133/08 , C09D169/00 , C09D175/04 , C09K3/18 , C08F283/12 , C08K5/00 , C08K5/06 , C08K5/17 , C07F7/08
Abstract: An aqueous coating material is provided. The aqueous coating material includes an aqueous resin and a surfactant. The surfactant having a hydrophilic segment of poly(alkylene glycol), a hydrophobic segment of siloxane, and a terminal hydrophilic group. The aqueous resin and the surfactant may have a weight ratio of 100:1 to 100:25.
-
公开(公告)号:US09758624B2
公开(公告)日:2017-09-12
申请号:US14305354
申请日:2014-06-16
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Wei-Cheng Tang , Yun-Shan Huang , Ya-Tin Yu , Yi-Che Su , Yuung-Ching Sheen , Yuan-Chang Huang
IPC: B05D3/00 , C08G77/395 , C09D183/04 , C09D183/06 , C09D183/08 , C08G77/30
CPC classification number: C08G77/395 , C08G77/30 , C09D183/04 , C09D183/06 , C09D183/08 , C08K5/5406
Abstract: A method for forming an inorganic passivation material is provided. The method includes mixing about 5 to 80 parts by weight of trialkoxysilane, about 10 to 80 parts by weight of tetraalkoxysilane, and about 1 to 30 parts by weight of catalyst to perform a reaction at pH of about 0.05 to 4 to form an inorganic resin material. The inorganic resin material is modified by phosphate ester to form an inorganic passivation material, wherein phosphate ester is about 0.1-10 parts by weight based on 100 parts by weight of the inorganic resin material. An inorganic passivation material and a passivation protective film produced therefrom are also provided.
-
公开(公告)号:US10787590B2
公开(公告)日:2020-09-29
申请号:US16232302
申请日:2018-12-26
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Kai-Wei Liao , Wei-Cheng Tang , Yi-Tzu Peng , Ya-Tin Yu , Yi-Che Su
IPC: C09D163/00 , C08L63/00
Abstract: A polymer is provided, which is formed by reacting a diol having hydrogenated bisphenol group with a bis-epoxy compound. The diol having hydrogenated bisphenol group may have a chemical structure of wherein each of R1 is independently H or methyl, and m and n are independently integers of 1 to 4. The bis-epoxy compound can be or a combination thereof, wherein each of R2 is independently H or methyl, and each of R3 is independently H or methyl.
-
公开(公告)号:US10087298B2
公开(公告)日:2018-10-02
申请号:US14583567
申请日:2014-12-26
Applicant: Industrial Technology Research Institute
Inventor: Wen-Pin Chuang , Yuung-Ching Sheen , Yun-Ya Huang , Yi-Che Su
IPC: C08J9/04 , C07G1/00 , C08G18/48 , C08H7/00 , C08G18/64 , C08G18/76 , C08G18/32 , C08L71/02 , C08L97/00 , C08J9/00 , C08G101/00
Abstract: A bio-polyol composition and a bio-polyurethane foam material are provided. By using the modifier and applying the dispersing and grinding process, the modified lignin is uniformly dispersed in the polyol solution and a bio-polyol composition is obtained. The obtained bio-polyol composition may be used to prepare the bio-polyurethane foam material with a high lignin content, a high compression strength and superior flame-resistance.
-
10.
公开(公告)号:US09856346B2
公开(公告)日:2018-01-02
申请号:US14879871
申请日:2015-10-09
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Yuung-Ching Sheen , Yi-Ting Wang , Su-Mei Chen Wei , Yi-Che Su , Wen-Pin Chuang
IPC: C08H7/00 , C08H8/00 , C08G59/16 , C08G59/42 , C08G59/02 , C08G59/40 , C08K3/00 , C08K5/00 , C08K9/04 , C08L97/00 , C08L63/00 , C09D163/00 , C09D197/00 , C08G59/06
CPC classification number: C08G59/1455 , C08G59/027 , C08G59/06 , C08G59/42 , C08H6/00 , C08H8/00 , C08K3/011 , C08K5/0025 , C08K9/04 , C08L97/005
Abstract: A method of forming a lignin-based biomass epoxy resin is provided, which includes: (a) mixing a lignin, an acid anhydride compound, and a solvent to react for forming a first intermediate product, (b) reacting the first intermediate compound with a first polyol to form a second intermediate compound, and (c) reacting the second intermediate compound with an epoxy compound to form a lignin-based biomass epoxy resin.
-
-
-
-
-
-
-
-
-