Resin composition, prepreg and laminate using the composition
    2.
    发明授权
    Resin composition, prepreg and laminate using the composition 失效
    树脂组合物,预浸料和使用该组合物的层压材料

    公开(公告)号:US07470471B2

    公开(公告)日:2008-12-30

    申请号:US10978379

    申请日:2004-11-02

    IPC分类号: B32B27/04

    摘要: The present invention is to provide a resin composition having sufficient rigidity and superior in the workability as well even if the thickness is as thin as 0.2 mm or less, and a prepreg and a laminate obtained from the resin composition. The resin composition comprises resin component containing a (A) compound having a maleimide group and (B) calcinated talc, wherein the calcinated talc is contained not less than 30 weight parts and not more than 250 weight parts to 100 weight parts of the total amount of the resin component containing a (A) compound having a maleimide group.

    摘要翻译: 本发明提供一种树脂组合物,即使厚度薄至0.2mm以下也能够得到刚性好,加工性优异的树脂组合物,以及由树脂组合物得到的预浸料和层叠体。 树脂组合物包含含有具有马来酰亚胺基团的(A)化合物和(B)煅烧滑石的树脂组分,其中煅烧滑石含有不少于30重量份且不超过250重量份至100重量份的总量 的树脂组分含有具有马来酰亚胺基团的(A)化合物。

    Resin composition, prepreg and laminate using the composition
    3.
    发明申请
    Resin composition, prepreg and laminate using the composition 审中-公开
    树脂组合物,预浸料和使用该组合物的层压材料

    公开(公告)号:US20050095434A1

    公开(公告)日:2005-05-05

    申请号:US10978403

    申请日:2004-11-02

    摘要: The present invention is to provide a laminate which is halogen-free, has sufficient flame retardancy even when a thickness is not more than 0.2 mm, and has sufficient humidity resistance and hygroscopic solder heat resistance. A resin composition comprising: (A) a compound having at least two or more maleimide groups; (B) a phenolic resin; and (C) an epoxy resin; wherein at least one of said (B) or (C) has a naphthalene ring; the total weight of the naphthalene ring when calculated using the OH equivalent and epoxy equivalent of (B) and (C) respectively is not less than 20 weight % to the total weight of (A), (B) and (C) components; and the total sum of the content ratio of the (A) component and that of the naphthalene ring is not less than 65 weight % to the total weight of the (A), (B) and (C) components, and a prepreg and laminate obtained from the same.

    摘要翻译: 本发明提供一种无卤素的层压体,即使厚度不大于0.2mm也具有足够的阻燃性,并且具有足够的耐湿性和吸湿性的耐热性。 一种树脂组合物,其包含:(A)具有至少两个或更多个马来酰亚胺基团的化合物; (B)酚醛树脂; 和(C)环氧树脂; 其中所述(B)或(C)中的至少一个具有萘环; 当使用(B)和(C)的OH当量和环氧当量计算时,萘环的总重量不小于(A),(B)和(C)组分的总重量的20重量% (A)成分和萘环的含有比例的总和相对于(A),(B)和(C)成分的总重量为65重量%以上,预浸料坯 从它们获得的层压板。

    Waterproof material and method for applying it
    4.
    发明授权
    Waterproof material and method for applying it 失效
    防水材料及其应用方法

    公开(公告)号:US5935683A

    公开(公告)日:1999-08-10

    申请号:US838261

    申请日:1997-04-17

    摘要: A waterproof material is disclosed herein which is obtainable by laminating many sheets of a photo-setting type fiber reinforced thermosetting resin composition comprising a resin composition containing a thermosetting resin, a photopolymerization initiator and a thickener, and a fiber reinforced material, or by laminating plural sheets of a synthetic polymer, and a waterproof application method using the waterproof material is also disclosed herein. According to the present invention, the waterproof layer can be formed on the surface of a civil engineering works or a building in a short time of about 30 minutes by a few steps without polluting a working environment. Furthermore, the waterproof layer, needless to say, has water resistance, weathering resistance, anticorrosion and substrate adhesion. In addition, it is further excellent in follow-up properties to cracks of the substrate, and walking on the waterproof layer is possible.