Electronic component and method of manufacturing same
    1.
    发明授权
    Electronic component and method of manufacturing same 失效
    电子元件及其制造方法

    公开(公告)号:US5995359A

    公开(公告)日:1999-11-30

    申请号:US859796

    申请日:1997-05-19

    摘要: An electronic component has a substrate, electrode layers for the bottom electrode, top electrode and, optionally, one or more intermediate electrodes, and has intermediate functional layers, these electrode layers include an electroconductive oxidic compound, at least one electrode layer is composed of EuO.sub.x, wherein 1.ltoreq.x.ltoreq.2, LiTi.sub.2 O.sub.4, LiV.sub.2 O.sub.4, SrVO.sub.3, Eu.sub.x NbO.sub.3, Na.sub.x WO.sub.3, A.sub.2 P.sub.8 W.sub.32 O.sub.112, wherein A=K, Rb,RTl, Na.sub.x Ta.sub.y W.sub.1-y O.sub.3, Na.sub.1-x Sr.sub.x NbO.sub.3, LaTiO.sub.3 CeTiO.sub.3, CaVO.sub.3, La.sub.1-x Sr.sub.x VO.sub.3, SrCoO.sub.3, CaRuO.sub.3, SrRuO.sub.3, BaRuO.sub.3, BaPbO.sub.3, SrMoO.sub.3, Sr.sub.0.5 La.sub.0.5 O.sub.3, La.sub.4 BaCu.sub.5 O.sub.13-x, La.sub.2-x Sr.sub.x CuO.sub.4-.delta., YBa.sub.2 Cu.sub.3 O.sub.7-.delta., Bi.sub.2 Sr.sub.2 CaCu.sub.2 O.sub.8.sub.+d, Bi.sub.2 Sr.sub.2 CuO.sub.6+d, Bi.sub.2 Sr.sub.2 Ca.sub.2 Cu.sub.3 O.sub.10+d, Tl.sub.2 Ba.sub.2 CaCu.sub.2 O.sub.8, TlBa.sub.2 CuO.sub.6+d, Tl.sub.2 Ba.sub.2 Ca.sub.2 Cu.sub.3 O.sub.10+d, La.sub.4 BaCu.sub.6 O.sub.15, Gd.sub.1-x Sr.sub.x VO.sub.3, CaCrO.sub.3, SrFeO.sub.3, EuNbO.sub.3, SrIrO.sub.3, CaMoO.sub.3, BaMoO.sub.3, Bi.sub.3 Ru.sub.3 O.sub.11, VO.sub.2, CrO.sub.2, MoO.sub.2, WO.sub.2, PtO.sub.2, RuO.sub.x, wherein 1.5.ltoreq.x.ltoreq.2, IrO.sub.x, SnO.sub.2-x, La.sub.3 Ni.sub.2 O.sub.7, La.sub.3 Ni.sub.3 O.sub.10, M.sub.2 V.sub.2 O.sub.7-x, wherein M=Tm, Lu, M.sub.2 Mo.sub.2 O.sub.7, wherein M=Nd,Sm,Gd, Lu.sub.2 Ru.sub.2 O.sub.7, Pb.sub.2 Ru.sub.2 O.sub.7, Bi.sub.2 Ru.sub.2 O.sub.7, Pb.sub.2 Os.sub.2 O.sub.7, Tl.sub.2 Os.sub.2 O.sub.7, Pb.sub.2 Ir.sub.2 O.sub.2, Tl.sub.2 Rh.sub.2 O.sub.7-x, K.sub.0.3 MoO.sub.3, Rb.sub.0.3 MoO.sub.3, Tl.sub.0.3 MoO.sub.3 M.sub.x V.sub.2 O.sub.5, wherein M=Cu,Na, Mo,.sub.17 O.sub.47 or Tl.sub.2 O.sub.3-x, or of physical mixtures and/or solid solutions of the oxidic compound or physical mixtures and/or solid solutions of the oxidic compounds to which is a 50% by weight of further compounds or metals is added. This electrode layer exhibits an improved adhesion and it does not passivate itself.

    摘要翻译: 电子部件具有基板,用于底部电极的电极层,顶部电极和任选的一个或多个中间电极,并且具有中间功能层,这些电极层包括导电氧化物,至少一个电极层由EuO x 其中A = K,Rb,RT1,NaxTayW1-yO3,Na1-xSrxNbO3,LaTiO3 CeTiO3,CaVO3,La1-xSrxVO3,La2-xSrxVO3,Ca2O4,Sr2O4, SrCoO3,CaRuO3,SrRuO3,BaRuO3,BaPbO3,SrMoO3,Sr0.5La0.5O3,La4BaCu5O13-x,La2-xSrxCuO4-δ,YBa2Cu3O7-δ,Bi2Sr2CaCu2O8 + d,Bi2Sr2CuO6 + d,Bi2Sr2Ca2Cu3O10 + d,T12Ba2CaCu2O8,TlBa2CuO6 + Tl2Ba2Ca2Cu3O10 + d,La4BaCu6O15,Gd1-xSrxVO3,CaCrO3,SrFeO3,EuNbO3,SrIrO3,CaMoO3,BaMoO3,Bi3Ru3O11,VO2,CrO2,MoO2,WO2,PtO2,RuOx,其中1.5≤x≤2,IrOx,SnO2 -x,La3Ni2O7,La3Ni3O10,M2V2O7-x,其中M = Tm,Lu,M2Mo2O7,其中M = Nd,Sm,Gd,Lu2Ru2O7,Pb2Ru2O7,Bi2Ru2O7,Pb2Os2O7,Tl2Os2O7,Pb2Ir2O2,T12Rh2O7-x,K0.3MoO3,Rb0 其中M = Cu,Na,Mo,17O47或Tl2O3-x,或氧化化合物的物理混合物和/或固体溶液或氧化化合物的物理混合物和/或固体溶液,其中M = 是50重量%的其它化合物或金属。 该电极层表现出改善的粘附性,并且不会使其自身钝化。

    Method of manufacturing powdered barium titanate
    2.
    发明授权
    Method of manufacturing powdered barium titanate 失效
    粉状钛酸钡的制造方法

    公开(公告)号:US4859448A

    公开(公告)日:1989-08-22

    申请号:US209450

    申请日:1988-06-20

    IPC分类号: C01G23/00

    摘要: A method of manufacturing powdered barium titanate, in which titanium dioxide is made to react with barium hydroxide, excluding CO.sub.2 at a temperature in the range from 60.degree. to 95.degree. C., amorphous titanium dioxide having a water content of .apprxeq.0.5 mol. being made to react with excess barium hydroxide in water, and being dried after removing the excess barium ions.

    摘要翻译: 制造粉末状钛酸钡的方法,其中二氧化钛与氢氧化钡反应,不包括CO 2在60℃至95℃的温度范围内,含水量为约0.1摩尔的无定形二氧化钛。 使其与过量的氢氧化钡在水中反应,并在除去过量的钡离子之后干燥。

    Multiple-component unit
    3.
    发明授权
    Multiple-component unit 有权
    多组件单元

    公开(公告)号:US06507498B1

    公开(公告)日:2003-01-14

    申请号:US09491626

    申请日:2000-01-26

    IPC分类号: H03H102

    CPC分类号: H03H1/00

    摘要: The invention relates to a multiple-component unit in which at least two passive components have been realized one above the other. A multiple-component unit thus comprises at least one resistor and at least one capacitor, or at least two capacitors. This space-saving construction allows for a miniaturization of circuits. A further miniaturization can be achieved in that the multiple-component units are not manufactured as discrete components, but are integrated into ICs.

    摘要翻译: 本发明涉及一种多组件单元,其中至少两个无源部件已经彼此上下实现。 因此,多组分单元包括至少一个电阻器和至少一个电容器,或至少两个电容器。 这种节省空间的结构允许电路的小型化。 可以实现进一步的小型化,因为多组分单元不是作为分立组件制造的,而是集成到IC中。

    Method of manufacturing mono-layer capacitors
    7.
    发明授权
    Method of manufacturing mono-layer capacitors 失效
    制造单层电容器的方法

    公开(公告)号:US5160762A

    公开(公告)日:1992-11-03

    申请号:US706822

    申请日:1991-05-29

    CPC分类号: H01L28/55 H01G4/1227

    摘要: A method of manufacturing monolayer capacitors having a ferroelectric layer on the basis of titanium as a dielectric on a substrate, the ferroelectric layer being located between a first and a second noble metal electrode, in which the ferroelectric layer is formed as a barium titanate layer having a layer thickness in the range of from 0.2 to 0.6 .mu.m in that a stable solution of salts of carbonic acids, alkoxides and/or acetyl acetonates is applied and is thermally decomposed at temperatures in the range of from 500.degree. to 700.degree. C., the solution constituting the ferroelectric layer being adjusted so that after the thermal decomposition process an excess quantity of titanium oxide of about 1 mol. % is obtained, and this coating process being repeated until the desired layer thickness is attained, after which the second noble metal electrode is provided on the ferroelectric layer.

    摘要翻译: 一种制造单层电容器的方法,所述单层电容器具有基于钛作为电介质的铁电层,所述铁电层位于第一和第二贵金属电极之间,所述铁电层形成为钛酸钡层,所述钛酸钡层具有 层厚度在0.2至0.6μm的范围内,因为碳酸,醇盐和/或乙酰基丙酮酸盐的稳定溶液被施加并且在500-700℃的温度下被热分解。 ,调整构成铁电体层的溶液,使得在热分解处理后,过量的氧化钛为约1mol。 %,并重复该涂覆处理直到达到所需的层厚度,之后将第二贵金属电极设置在强电介质层上。

    Method of manufacturing titanium dioxide powder
    8.
    发明授权
    Method of manufacturing titanium dioxide powder 失效
    二氧化钛粉末的制造方法

    公开(公告)号:US4999181A

    公开(公告)日:1991-03-12

    申请号:US504731

    申请日:1990-04-02

    IPC分类号: C01G23/053

    摘要: A method of manufacturing titanium dioxide powder by hydrolysis of a titanium alcoholate, in which the titanium alcoholate is made to react with a 10M acetic acid aqueous solution and an aqueous ethanol solution under an N.sub.2 atmosphere, the precipitate consisting of titanium dioxide is separated from the liquid phase after a reaction time of 24 hours, the precipitate is rinsed with deionized water and subsequently with an aqueous ammoniacal solution having a pH value of 9, and the phases are separated.

    摘要翻译: 通过水解钛醇化物制备二氧化钛粉末的方法,其中使钛醇化物与10M乙酸水溶液和乙醇水溶液在N 2气氛下反应,将由二氧化钛组成的沉淀物从 在24小时的反应时间后,用去离子水冲洗沉淀物,随后用pH值为9的氨水溶液洗涤,分离各相。

    Thin-film capacitor
    10.
    发明授权
    Thin-film capacitor 失效
    薄膜电容器

    公开(公告)号:US06337790B1

    公开(公告)日:2002-01-08

    申请号:US09385279

    申请日:1999-08-30

    IPC分类号: H01G4228

    CPC分类号: H01G2/20 H01G2/14

    摘要: The present invention provides a new type of thin-film capacitor which is insensitive to breakdown voltages during its mounting on a printed circuit board. Said capacitor has an insulating substrate having at least two internal electrode layers which are mutually separated by means of a dielectric layer. The substrate also has two end contacts each of which are electroconductively connected to one of said internal electrode layers. According to the invention, the capacitor also has breakable electrically conductive means, preferably formed as a metal layer, which means are electrically connected to said end contacts. The presence of said breakable electrically conductive means between said end contacts prevents damage due to electrical storage which can arise during the mounting of the capacitor on a printed circuit board.

    摘要翻译: 本发明提供了一种新型薄膜电容器,其在其安装在印刷电路板上时对击穿电压不敏感。 所述电容器具有绝缘基板,该绝缘基板具有至少两个通过介电层相互分离的内部电极层。 基板还具有两个端部触头,每个触头都与所述内部电极层中的一个导电连接。 根据本发明,电容器还具有可破坏的导电装置,优选地形成为金属层,该装置电连接到所述端触点。 在所述端部触点之间存在所述可破坏的导电装置可以防止由于在将电容器安装在印刷电路板上时可能引起的电存储的损坏。