摘要:
Thermoplastic molding masses made of thermoplastic polymers obtained by mixed graft polymerization and having a glass transition temperature above 20 C., and of special rubber-elastic block copolymers, are characterized by a balanced spectrum of properties.
摘要:
Thermoplastic molding materials contain A) polycarbonates B) elastomeric graft copolymers, C+D) two different, thermoplastic copolymers based on styrene or &agr;-methylstyrene, E) copolymers based on alkyl(meth)acrylate and F) polymeric, OH-containing compounds.
摘要:
Thermoplastic molding compositions comprising A) a graft polymer comprising 1) an elastomeric graft core, obtainable by copolymerization of one or more C1-C10-alkyl acrylates, and a monomer with crosslinking effect, and 2) a graft shell comprising a styrene compound or a C1-C8-alkyl acrylate or methacrylate, or a mixture of the styrene compound and the C1-C8-alkyl acrylate or methacrylate, and B) a thermoplastic polymer comprising C) an elastomeric block copolymer in which all or virtually all of the olefinic double bonds have been hydrogenated, comprising at least one block A, which forms a hard phase and contains, in its polymer chain, units of a vinylaromatic monomer, and/or a block B, which forms a first elastomeric (soft) phase and contains diene monomers, and at least one elastomeric block B/A, which forms a soft phase, and contains, randomly in its polymer chain, units of both a vinylaromatic monomer and a diene, where the glass transition temperature Tg of the block A is above 25° C. and that of the block B/A is below 25° C. and the phase-volume ratio of block A to block B/A is chosen so that the proportion of the hard phase in the entire block copolymer is from 1 to 40% by volume and the proportion by weight of the diene is less than 50% by weight.
摘要:
The invention relates to thermoplastic molding compositions comprisingA) from 30 to 98% by weight of a graft copolymer comprisinga.sub.K) from 30 to 90% by weight of an elastomeric graft core,a.sub.S) from 10 to 70% by weight of a graft shell comprisinga.sub.S /1) from 50 to 100% by weight of a styrene compound or a C.sub.1 -C.sub.8 -alkyl acrylate or methacrylate, or a mixture thereof, anda.sub.S /2) from 0 to 50% by weight of one or more other monomers,B) from 1 to 50% by weight of a thermoplastic polymer andC) from 1 to 70% by weight of an elastomeric block copolymer prepared by anionic polymerization of the monomers with addition of a potassium compound soluble in non-polar solvents (Step 1) followed by hydrogenation of all or virtually all the olefinic double bonds of the polymer obtained in Step 1, as described in greater detail herein.
摘要:
Graft copolymers are prepared by anionic polymerization which comprises reacting polymers (A) having at least one anionic chain end with polymers (B) which contain at least one nitrile group, in the presence of a solvent.
摘要:
Thermoplastic molding materials of A) from 30 to 98% by weight of a graft polymer of a.sub.c) from 30 to 90% by weight of an elastomeric graft core and a.sub.s) from 10 to 70% by weight of a graft shell, B) from 1 to 50% by weight of a thermoplastic polymer, C) from 1 to 70% by weight of an elastomeric block copolymer, and D) from 0 to 30% by weight of a polymer having a star-like structure.
摘要:
The present invention relates to a method for producing fiber-reinforced composite materials, in which a multiplicity of continuous filaments or woven fabric is impregnated optionally together with reinforcing materials, comprising caprolactam and other starting materials for polyamide 6 or other starting materials for copolymers of caprolactam, passed through at temperatures of 70 to 100° C., and anionically polymerized at temperatures of 100 to 190° C., and optionally repolymerized at temperatures of 90 to 170° C.
摘要:
The thermoplastic molding composition comprises, based on the thermoplastic molding composition, a) at least one polyamide, copolyamide or a polyamide-comprising polymer blend as component A, b) from 0.1 to 10% by weight of carbon nanotubes, graphenes or mixtures thereof as component B, c) from 0.1 to 3% by weight of ionic liquids as component C, wherein the thermoplastic molding composition does not comprise any polyamide-12 units.
摘要:
The invention relates to a process for the preparation of a hollow filament (F) based on one or several molten or dissolved hyperbranched polymers (P) and potentially one or several further polymers (FP), characterized in that the molten or dissolved hyperbranched polymer (P) or the mixture of the hyperbranched polymer (P) with the further polymer (FP) is passed through one or several spinnerets (S), wherein the ratio between the spinneret die-length (L) and the die-channel (Delta-D) is between 0.1 and 9.5. The process can be applied for the preparation of hyperbranched polyethersulfone (HPES) hollow filaments.
摘要:
The present invention relates to a process for the production of low-halogen-content polybiphenyl sulfone polymers, to the resultant polybiphenyl sulfone polymers, to polybiphenyl sulfone polymers having less than 400 ppm content of polymer-bonded halogen, to thermoplastic molding compositions comprising these polybiphenyl sulfone polymers, and to their use for the production of moldings, of fibers, of films, of membranes, or of foams.