    摘要: A process for production of hydrocarbons including a) reforming a divided hydrocarbon feedstock stream, mixing the first stream with steam, passing the mixture over a catalyst disposed in heated heat exchange reformer tubes to form a primary reformed gas, forming a secondary reformer feed stream including the primary reformed gas and the second hydrocarbon stream, partially combusting the secondary reformer feed stream and bringing the partially combusted gas towards equilibrium over a secondary catalyst, and producing a partially cooled reformed gas, b) further cooling the partially cooled reformed gas below the dew point of steam therein to condense water and separating condensed water to give a de-watered synthesis gas, c) synthesising hydrocarbons from the de-watered synthesis gas by the Fischer-Tropsch reaction and separating some of the synthesised hydrocarbons into a tail gas, and d) incorporating part of the tail gas into the secondary reformer feed stream before partial combustion thereof.

    摘要翻译: 一种生产烃的方法,包括:a)重整分离的烃原料流,将第一料流与蒸汽混合,使混合物通过设置在加热的热交换重整器管中的催化剂,形成初级重整气体,形成二级重整器进料流,包括 主要重整气体和第二烃流,部分地燃烧二次重整器进料流并使部分燃烧的气体在二次催化剂上达到平衡,并产生部分冷却的重整气体,b)进一步冷却低于露点的部分冷却的重整气体 蒸汽点冷凝水,分离冷凝水,得到脱水合成气; c)通过费 - 托反应合成来自脱水的合成气的碳氢化合物,并将一些合成的烃分离成尾气;以及 d)将部分尾气混入二次重整器进料流中 其中。

    Metal Passivation
    5.
    发明申请
    Metal Passivation 有权
    金属钝化

    公开(公告)号:US20080313962A1

    公开(公告)日:2008-12-25

    申请号:US12091258

    申请日:2006-10-10

    IPC分类号: C10J3/00 C23F11/02

    摘要: A method for passivating low-alloy steel surfaces in apparatus operating in the temperature range 350 to 580° C. and exposed to a carbon monoxide containing gas mixture comprises adding a passivating compound containing at least one phosphorus (P) atom to the gas mixture. The gas mixture is preferably a reformed gas and also described is a process for producing a synthesis gas wherein, prior to cooling a reformed gas mixture to a temperature between 350 and 580° C. in apparatus having low-alloy steel surfaces downstream of one or more reforming steps, a passivating compound containing at least one phosphorus (P) atom is combined with the gas mixture.

    摘要翻译: 在350至580℃的温度范围内操作并暴露于含一氧化碳的气体混合物的设备中钝化低合金钢表面的方法包括向气体混合物中加入含有至少一个磷(P)原子的钝化化合物。 气体混合物优选是重整气体,并且还描述了一种生产合成气的方法,其中在将重整气体混合物冷却至350-580℃之间的温度之前,在具有低合金钢表面的装置中, 更多的重整步骤,含有至少一个磷(P)原子的钝化化合物与气体混合物组合。

    Catalysts
    6.
    发明授权
    Catalysts 失效
    催化剂

    公开(公告)号:US5263998A

    公开(公告)日:1993-11-23

    申请号:US899326

    申请日:1992-06-16

    摘要: Compositions suitable for use as oxidation catalysts essentially free from elements, or compounds thereof, of Group VIII of the Periodic Table, comprise an intimate mixture of oxides of at least three elements selected from Groups IIIa and IVa of the Periodic Table, including, of the total number of Group IIIa and IVa element atoms present, a) a total of at least 60% of atoms of at least one element X selected from cerium, zirconium, and hafnium, b) a total of at least 5% of atoms of at least one other element Y different from element X and selected from the variable valency elements titanium, cerium, praseodymium, and terbium; and c) a total of at least 5% of atoms of at least one element Z differing from X and Y and selected from Group IIIa elements. Such composition, and similar two component compositions wherein X and Y are both cerium, have, after heating for 8 hours at 1200.degree. C., a BET surface area of at least 1 m.sup.2 .multidot.g.sup.-1 and are particularly useful for the oxidation of a feedstock with an oxygen-containing gas, e.g. catalytic combustion, especially under conditions such that the catalyst attains a temperature of at least 1000.degree. C.

    摘要翻译: 适合用作氧化催化剂的组合物基本上不含周期表第Ⅷ族元素或其化合物,包括选自元素周期表Ⅲa和Ⅳa族的至少三种元素的氧化物的紧密混合物,包括 存在IIIa族和IVa族元素原子的总数,a)选自铈,锆和铪中的至少一种元素X的至少60%的原子的总和,b)总共至少5%的原子 至少一个与元素X不同的元素Y,并且从可变价元素钛,铈,镨和铽中选择; 和c)至少一种元素Z至少5%的原子不同于X和Y并且选自IIIa族元素。 这种组合物和其中X和Y都是铈的类似的双组分组合物在1200℃下加热8小时之后,具有至少1m 2×g-1的BET表面积,并且特别可用于原料氧化 含氧气体,例如 催化燃烧,特别是在催化剂达到至少1000℃的温度的条件下。

    METAL PASSIVATION OF HEAT-EXCHANGER EXPOSED TO SYNTHESIS GAS
    7.
    发明申请
    METAL PASSIVATION OF HEAT-EXCHANGER EXPOSED TO SYNTHESIS GAS 失效
    接触合成气体的换热器的金属钝化

    公开(公告)号:US20130248770A1

    公开(公告)日:2013-09-26

    申请号:US13821882

    申请日:2011-08-19

    IPC分类号: C01B3/02

    摘要: A process for passivation of surfaces of heat exchange apparatus exposed to a synthesis gas containing carbon monoxide, includes the steps of: adding arsine to the synthesis gas to provide a total As concentration in the synthesis gas in range 0.001 to 10 ppmv, (ii) exposing the mixture of hot synthesis gas and arsine to the shell-side surfaces of said heat exchange apparatus to reduce the interaction between the carbon monoxide present in said gas and metals in said surfaces, (iii) recovering a cooled synthesis gas from the shell-side of said apparatus, and (iv) passing the cooled synthesis gas, optionally after further cooling, through a sorbent bed to remove arsenic compounds from the synthesis gas.

    摘要翻译: 一种暴露于含有一氧化碳的合成气体的热交换装置的表面的钝化方法包括以下步骤:向合成气中加入胂以提供合成气中的总As浓度范围为0.001至10ppmv,(ii) 将热合成气和胂的混合物暴露于所述热交换装置的壳侧表面,以减少所述气体中存在的一氧化碳和所述表面中的金属之间的相互作用,(iii)从壳层中回收冷却的合成气, (iv)任选地在进一步冷却之后将冷却的合成气通过吸附剂床以从合成气中除去砷化合物。

    Metal passivation
    8.
    发明授权
    Metal passivation 有权
    金属钝化

    公开(公告)号:US08470202B2

    公开(公告)日:2013-06-25

    申请号:US12091258

    申请日:2006-10-10

    IPC分类号: C01B3/26 C23C22/03

    摘要: A method for passivating low-alloy steel surfaces in apparatus operating in the temperature range 350 to 580° C. and exposed to a carbon monoxide containing gas mixture comprises adding a passivating compound containing at least one phosphorus (P) atom to the gas mixture. The gas mixture is preferably a reformed gas and also described is a process for producing a synthesis gas wherein, prior to cooling a reformed gas mixture to a temperature between 350 and 580° C. in apparatus having low-alloy steel surfaces downstream of one or more reforming steps, a passivating compound containing at least one phosphorus (P) atom is combined with the gas mixture.

    摘要翻译: 在350至580℃的温度范围内操作并暴露于含一氧化碳的气体混合物的设备中钝化低合金钢表面的方法包括向气体混合物中加入含有至少一个磷(P)原子的钝化化合物。 气体混合物优选是重整气体,并且还描述了一种生产合成气的方法,其中在将重整气体混合物冷却至350-580℃之间的温度之前,在具有低合金钢表面的装置中, 更多的重整步骤,含有至少一个磷(P)原子的钝化化合物与气体混合物组合。

    Oxidation catalysts
    10.
    发明授权
    Oxidation catalysts 失效
    氧化催化剂

    公开(公告)号:US5567667A

    公开(公告)日:1996-10-22

    申请号:US290831

    申请日:1994-10-21

    IPC分类号: B01J23/10

    CPC分类号: B01J23/10

    摘要: An oxidation catalyst composition comprises an intimate mixture of oxides of praseodymium, at least one nonvariable valency Group IIIa element, and, optionally zirconium, said composition containing a total of 5-50% of praseodymium atoms, 0-45% of zirconium atoms, and 20-95% of said non-variable valency Group IIIa element atoms, said percentages being based upon the total number of praseodymium, zirconium, and non-variable valency Group IIIa element atoms in said intimate mixture.