Composite material for magnetooptic recording, comprising a thin layer deposited on a non-magnetic solid substrate. The said thin layer is a polycrystalline layer consisting of microcrystals having a structure of a vacant-site spinel ferrite, based on iron, cobalt and transition metals. By virtue of a particular process for producing the thin layers, enabling especially the size of the crystallites to be increased, it is possible to optimize the magnetic and magnetooptic properties and to obtain thin layers having, for example, a remanent Faraday rotation and a coercive field which are greater, respectively, than 1 degree per micron for the Faraday rotation and 1000 Oe for the coercive field.
摘要:
Composite material for magnetooptic recording, comprising a thin layer deposited on a non-magnetic solid substrate. The said thin layer is a polycrystalline layer consisting of microcrystals having a structure of a vacant-site spinel ferrite, based on iron, cobalt and transition metals. By virtue of a particular process for producing the thin layers, enabling especially the size of the crystallites to be increased, it is possible to optimize the magnetic and magnetooptic properties and to obtain thin layers having, for example, a remanent Faraday rotation and a coercive field which are greater, respectively, than 1 degree per micron for the Faraday rotation and 1000 Oe for the coercive field.
摘要:
The present invention relates to a method of recording data in digital form on a write-once read-many optical medium comprising a sensitive film based on a metal oxide of the oxidizable spinel type. Regions of the sensitive film are heated, locally and in succession, under conditions allowing oxidation of the oxidizable metal ions of the oxide. In the optical medium thus recorded, the virgin regions, which are not modified by the write operation, are oxidizable and change color after heat treatment in an oxidizing atmosphere.
摘要:
A magneto-optical recording medium has a recording layer and a reflective layer on a substrate. The recording layer has a layered structure in which at least one spinel ferrite (or rutile-type oxide or hematite) layer and at least one garnet ferrite layer are piled together. It is preferable that the layered structure is formed on tracks where data are recorded. A manufacturing method comprises the steps of heat treatment in the range of 500-700° C., preferably 600-630° C., after the formation of the recording layer. In the magneto-optical recording and playback device to record and play back data, the wavelength of light for recording data is different from that for reading data, which is preferable for a magneto-optical recording medium comprising a garnet ferrite layer.
摘要:
This invention relates to magneto-optical recording media such as magneto-optical disks and cards, manufacturing methods of the medium and a magneto-optical recording and playback device to record and play back data using the magneto-optical recording media. The magneto-optical recording medium of the present invention has a recording layer and a reflective layer on a substrate, and the recording layer has a layered structure in which at least one spinel ferrite (or rutile-type oxide or hematite) layer and at least one garnet ferrite layer are piled together. It is preferable that the layered structure is formed on tracks where data are recorded. The manufacturing method of the present invention comprises the steps of heat treatment in the range of 500-700° C., preferably 600-630° C., after the formation of the recording layer. In the magneto-optical recording and playback device to record and play back data of the present invention, the wavelength of light for recording data is different from that for reading data, which is preferable for a magneto-optical recording medium comprising a garnet ferrite layer.
摘要:
This invention relates to magneto-optical recording media such as magneto-optical disks and cards, manufacturing methods of the medium and a magneto-optical recording and playback device to record and play back data using the magneto-optical recording media. The magneto-optical recording medium of the present invention has a recording layer and a reflective layer on a substrate, and the recording layer has a layered structure in which at least one spinel ferrite (or rutile-type oxide or hematite) layer and at least one garnet ferrite layer are piled together. It is preferable that the layered structure is formed on tracks where data are recorded. The manufacturing method of the present invention comprises the steps of heat treatment in the range of 500-700° C., preferably 600-630° C., after the formation of the recording layer. In the magneto-optical recording and playback device to record and play back data of the present invention, the wavelength of light for recording data is different from that for reading data, which is preferable for a magneto-optical recording medium comprising a garnet ferrite layer.
摘要:
The invention relates to the use of a material having a spinel ferrite/iron monoxide structure as a sensitive material in the form of a thin film for the bolometric detection of infrared radiation, the chemical composition of said structure, excluding doping agents that may be present, having empirical formula (I): (Fe1−zMz)xO, where x is strictly less than 1 and strictly greater than 0.75. The invention also relates to a bolometric device for infrared radiation detection and infrared imaging, comprising at least one sensor provided with a sensitive element in the form of a thin film as defined above.
摘要:
The present invention relates to the use as a sensitive material in a thin layer for bolometric detection of infrared radiation, of a material having a spinel ferrite structure of chemical composition, ignoring doping agents if any are present, satisfying empirical formula I: Fe3-(x+y)MxAyO4+δ. The invention also provides a bolometric device for detecting infrared radiation or for infrared imaging, and including at least one sensor provided with a sensitive element in the form of a thin layer as defined above.
摘要翻译:本发明涉及在具有化学组成的尖晶石铁素体结构的材料的红外线辐射的测定用薄层的敏感材料中的用途,忽视掺杂剂,如果有的话,满足实验式I:Fe3-( x + y)MxAyO4 +δ。 本发明还提供一种用于检测红外辐射或用于红外成像的测温装置,并且包括至少一个传感器,其设置有如上所述的薄层形式的敏感元件。
摘要:
The present invention relates to the use as a sensitive material in a thin layer for bolometric detection of infrared radiation, of a material having a spinel ferrite structure of chemical composition, ignoring doping agents if any are present, satisfying empirical formula I: Fe3−(x+y)MxAyO4+δ (I) The invention also provides a bolometric device for detecting infrared radiation or for infrared imaging, and including at least one sensor provided with a sensitive element in the form of a thin layer as defined above.
摘要翻译:本发明涉及在具有化学成分的尖晶石铁素体结构的材料的红外线辐射的测定用薄层中作为敏感材料的用途,忽视掺杂剂,如果有的话,满足实验式I:<α -line-formula description =“In-line Formulas”end =“lead”?Fe 3-x(x + y)M x x A y (I)<?in-line-formula description =“In-line Formulas”end =“tail”?>本发明还提供了一种用于检测红外辐射的辐射测量装置或 用于红外成像,并且包括至少一个传感器,其设置有如上所述的薄层形式的敏感元件。
摘要:
The purpose of the invention is a process for making a solid part designed to form all or part of an anode for the production of aluminium by fused bath electrolysis, containing a cermet formed from at least one metallic oxide such as a mixed oxide with spinel structure, and at least one metallic phase, in which a mixed oxide is used containing a metal R in the form of a cation in its chemical structure, the said metal R being fully or partly reducible by a reduction operation during the manufacturing process, so as to form all or part of the said metallic phase. This process can provide a cermet with a uniform distribution of fine metallic particles.