摘要:
The present disclosure relates to a reforming catalyst and a process for preparing the same. The acidic functionality of the catalyst is suppressed by using a chloride free alumina and coating the chloride free alumina with Group V B metal oxide in the catalyst, which helps in minimizing the cracking reactions and achieving higher selectivity for liquid hydrocarbons and aromatic hydrocarbons.
摘要:
The present disclosure relates to a reforming catalyst and a process for preparing the same. The acidic functionality of the catalyst is suppressed by using a chloride free alumina and coating the chloride free alumina with Group V B metal oxide in the catalyst, which helps in minimizing the cracking reactions and achieving higher selectivity for liquid hydrocarbons and aromatic hydrocarbons.
摘要:
The present disclosure relates to a naphtha reforming process for obtaining reformed naphtha comprising contacting naphtha with a catalyst, the catalyst comprising a chloride free zeolite coated alumina support impregnated with 0.01 wt % to 0.5 wt % active metal and 0.01 wt % to 0.5 wt % promoter metal, wherein the thickness of the zeolite coating on the alumina support ranges from 100 μm to 200 μm, which results in formation of reformed products of naphtha and ethylbenzene formed in-situ.
摘要:
The present disclosure relates to a process for preparing a catalyst. The process comprises coating zeolite gel over the alumina support to obtain a chloride free zeolite gel coated alumina support, crystallizing the chloride free zeolite gel coated alumina support, washing, drying and calcining the crystallized zeolite coated alumina support to obtain a calcined crystallized chloride free zeolite coated alumina support, treating the calcined crystallized chloride free zeolite coated alumina support with ammonium nitrate to obtain sodium free support, washing, drying, and calcining the support to obtain a calcined chloride free zeolite coated alumina support, immersing the calcined chloride free zeolite coated alumina support in an active metal and a promoter metal solution mixture followed by stirring to obtain a metal coated chloride free zeolite coated alumina support, and drying and calcining the metal coated chloride free zeolite coated alumina support to obtain the catalyst.
摘要:
The present disclosure relates to a naphtha reforming process for obtaining reformed naphtha comprising contacting naphtha with a catalyst, the catalyst comprising a chloride free zeolite coated alumina support impregnated with 0.01 wt % to 0.5 wt % active metal and 0.01 wt % to 0.5 wt % promoter metal, wherein the thickness of the zeolite coating on the alumina support ranges from 100 μm to 200 μm, which results in formation of reformed products of naphtha and ethylbenzene formed in-situ.
摘要:
The present disclosure relates to a dehydrogenation catalyst composite comprising at least one alumina support impregnated with at least one layer of at least one alkaline earth metal element and at least one layer comprising at least one catalytic metal element, at least one group VIA element and optionally, at least one halogen element. The present disclosure also relates to a process for preparation of the dehydrogenation catalyst composite.
摘要:
The present disclosure relates to a reforming catalyst composition comprising a spherical gamma AI2O3 support; at least one Group VB metal oxide sheet coated on to the AI2O3 support; and at least one active metal and at least one promoter metal impregnated on the AI2O3 coated support. The reforming catalyst composition of the present disclosure has improved activity, better selectivity for total aromatics during naphtha reforming and results in less coke formation. The reforming catalyst composition has improved catalyst performance with simultaneous modification of acidic sites as well as metallic sites through metal support interaction. The acid site cracking activity of the catalyst is inhibited because of the use of chloride free alumina support modified with solid acid such as Group VB metal oxide and impregnated with active metals. The present disclosure provides a process for naphtha reforming in the presence of the reforming catalyst composition of the present disclosure to obtain reformates of naphtha.
摘要:
The present disclosure relates to a process for preparing a catalyst. The process comprises coating zeolite gel over the alumina support to obtain a chloride free zeolite gel coated alumina support, crystallizing the chloride free zeolite gel coated alumina support, washing, drying and calcining the crystallized zeolite coated alumina support to obtain a calcined crystallized chloride free zeolite coated alumina support, treating the calcined crystallized chloride free zeolite coated alumina support with ammonium nitrate to obtain sodium free support, washing, drying, and calcining the support to obtain a calcined chloride free zeolite coated alumina support, immersing the calcined chloride free zeolite coated alumina support in an active metal and a promoter metal solution mixture followed by stirring to obtain a metal coated chloride free zeolite coated alumina support, and drying and calcining the metal coated chloride free zeolite coated alumina support to obtain the catalyst.
摘要:
The present disclosure relates to a reforming catalyst composition comprising a spherical gamma AI2O3 support; at least one Group VB metal oxide sheet coated on to the AI2O3 support; and at least one active metal and at least one promoter metal impregnated on the AI2O3 coated support. The reforming catalyst composition of the present disclosure has improved activity, better selectivity for total aromatics during naphtha reforming and results in less coke formation. The reforming catalyst composition has improved catalyst performance with simultaneous modification of acidic sites as well as metallic sites through metal support interaction. The acid site cracking activity of the catalyst is inhibited because of the use of chloride free alumina support modified with solid acid such as Group VB metal oxide and impregnated with active metals. The present disclosure provides a process for naphtha reforming in the presence of the reforming catalyst composition of the present disclosure to obtain reformates of naphtha.
摘要:
The present disclosure relates to a catalyst for a naphtha reforming process. The catalyst comprises a chloride free zeolite coated alumina support impregnated with 0.01 wt % to 0.5 wt % active metal and 0.01 wt % to 0.5 wt % promoter metal, characterized in that the thickness of the zeolite coating on the alumina support ranges from 100 μm to 200 μm.