    摘要: A method of forming a low level carbon high-density tungsten carbide-containing material includes sintering a preform which contains tungsten carbide powder and has a composition such that the resulting sintered material has at most 6.05 weight percent tungsten-bound carbon based on the total weight of tungsten and tungsten-bound carbon. This low level of carbon may be achieved by, prior to the sintering step, oxidizing the tungsten carbide powder sufficiently to achieve the desired substoichiometric carbon level in the sintered product or by adding a carbon-lowering material selected from the group consisting of tungsten, ditungsten carbide, and tungsten oxide. Optionally, other materials can be present in the preform such as carbon-getter metals and compounds thereof. The carbon-getter metals are those metals of which the carbides thereof are more thermodynamically stable than monotungsten carbide.

    摘要翻译: 形成低碳碳高密度碳化钨的材料的方法包括烧结含有碳化钨粉末的预成型体,并且具有使得所得烧结材料基于总重量具有至多6.05重量%的钨结合碳的组成 的钨和钨结合的碳。 这种低水平的碳可以通过在烧结步骤之前充分氧化碳化钨粉末以达到烧结产品中所需的亚化学计量碳水平,或通过添加选自钨,二钨的碳的降低材料 碳化物和氧化钨。 任选地,其它材料可以存在于预成型体中,例如碳吸收剂金属及其化合物。 碳吸收剂金属是其碳化物比单碳化钨更具有热力学稳定性的金属。

    Cemented ceramic article made from ultrafine solid solution powders,
method of making same, and the material thereof
    4.
    发明授权
    Cemented ceramic article made from ultrafine solid solution powders, method of making same, and the material thereof 失效
    由超细固溶粉末制成的水泥陶瓷制品,其制造方法及其材料

    公开(公告)号:US5580666A

    公开(公告)日:1996-12-03

    申请号:US375759

    申请日:1995-01-20

    摘要: A multi-phase cemented ceramic article, method of making same, and the material thereof is disclosed which is useful for machining and forming of metals, including ferrous metals, titanium, aluminum and other metals. The article and its material preferably includes novel microstructures including platelets, a range of grain sizes which yields superior hardness and other characteristics, and a lower tungsten concentration within the binder phase than has been seen in the prior art. The preferred composition includes ultrafine WC, an ultrafine solid solution of (Ti, Ta, W)C, and a cobalt binder. Platelets are formed in-situ, eliminating the need to add them during manufacture for improving toughness.